Lightweight Honeycomb rGO/Ti3C2Tx MXene Aerogel without Magnetic Metals toward Efficient Electromagnetic Wave Absorption Performance AITranslate

Qingdao University of Technology; Qingdao University of Technology; Qingdao University of Technology; Qingdao University of Technology; Qingdao University of Technology; Qingdao University of Technology; Qingdao University of Technology;Postdoctoral Workstation, Guangdong Dongpeng Holding Company Limited;Postdoctoral Workstation, Guangdong Dongpeng Holding Company Limited
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nonmagnetic electromagnetic wave (EMW)-absorbing materials have aroused research interest on account of their light weight, chemical stability, and excellent dielectric property. However, it is still a great challenge to fabricate one kind of nonmagnetic EMW-absorbing materials with a unique structure and excellent EMW-absorbing performance. Herein, lightweight (∼3.2 mg/cm3) honeycomb rGO/Ti3C2Tx MXene aerogel nanocomposites without magnetic metals were successfully fabricated via a green and convenient method in our work. Surprisingly, when the filler loading is only 5 wt % under the coaxial test, the minimum reflection loss (RL) value of the rGO/MXene-1:0.5 aerogel nanocomposite is −74.01 dB (99.99997% wave absorption) at 14.77 GHz with the thickness of only 1.80 mm. The effective absorption band (EAB) value under the arch test covers the whole C band, X band, and most of the C band. Furthermore, computer simulation technology (CST) data further demonstrated that the rGO/MXene-1:0.5 aerogel nanocomposite-covered model owns the smallest radar cross section (RCS) value, indicating that it possesses favorable radar wave attenuation capacity. Thus, the nonmagnetic honeycomb rGO/Ti3C2Tx MXene aerogel nanocomposites can be promising candidates for designing efficient lightweight EMW absorbers.

KeyWords AITranslate

nonmagnetic electromagnetic wave rGO/Ti3C2Tx MXene aerogel nanocomposites impedance matching porous effect
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01271

Chinese Library Classification Number:

Citation Information:

Nonmagnetic electromagnetic wave (EMW)-absorbing materials have aroused research interest on account of their light weight, chemical stability, and excellent dielectric property. However, it is still a great challenge to fabricate one kind of nonmagnetic EMW-absorbing materials with a unique structure and excellent EMW-absorbing performance. Herein, lightweight (∼3.2 mg/cm3) honeycomb rGO/Ti3C2Tx MXene aerogel nanocomposites without magnetic metals were successfully fabricated via a green and convenient method in our work. Surprisingly, when the filler loading is only 5 wt % under the coaxial test, the minimum reflection loss (RL) value of the rGO/MXene-1:0.5 aerogel nanocomposite is −74.01 dB (99.99997% wave absorption) at 14.77 GHz with the thickness of only 1.80 mm. The effective absorption band (EAB) value under the arch test covers the whole C band, X band, and most of the C band. Furthermore, computer simulation technology (CST) data further demonstrated that the rGO/MXene-1:0.5 aerogel nanocomposite-covered model owns the smallest radar cross section (RCS) value, indicating that it possesses favorable radar wave attenuation capacity. Thus, the nonmagnetic honeycomb rGO/Ti3C2Tx MXene aerogel nanocomposites can be promising candidates for designing efficient lightweight EMW absorbers.

quote

GB/T 7714-2015 [1] Yunfeng Bao, Siyao Guo, Ying Li, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01271.
MLA [1] Yunfeng Bao, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01271.
APA [1] Yunfeng Bao, Siyao Guo, Ying Li, Zhiqing Jia, Hailong Guan, Dongyi Lei, Jizhou Chen, Baomin Zhong, & Zhihong Li. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01271
IEEE [1] Yunfeng Bao, Siyao Guo, Ying Li, Zhiqing Jia, Hailong Guan, Dongyi Lei, Jizhou Chen, Baomin Zhong, and Zhihong Li, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01271. keywords: {nonmagnetic electromagnetic wave rGO/Ti3C2Tx MXene aerogel nanocomposites impedance matching porous effect}