daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High Efficiency Low-Temperature Processed Perovskite Solar Cells Integrated with Alkali Metal Doped ZnO Electron Transport Layers AITranslate

Kookmin University; Korea Institute of Science and Technology; Sungkyunkwan University; Korea Institute of Science and Technology; Sungkyunkwan University; Kookmin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Herein, we achieved, air-stable low-temperature processed PSC (L-PSC) using alkali-metal modified ZnO ETLs. Using a simple chemical alkali-metal modification method, the surface defects of the ZnO were effectively passivated. As a result, the interfacial decomposition reactions were suppressed, while raising the Fermi energy level and enhancing electron mobility. The improved interfacial charge transfer and internal electric field in the developed L-PSC using K modified ZnO (ZnO-K) exhibited an improved power conversion efficiency (PCE) of 19.90% with negligible hysteresis, while a pristine ZnO based L-PSC exhibited a PCE of 16.10% with significant hysteresis. The ZnO-K based L-PSC also exhibited remarkably higher long-term air-storage stability (91% retention after 800 h) than pristine ZnO based L-PSCs (36% retention after 800 h) due to the suppressed decomposition reactions. The PCE and air stability of our L-PSC with the modified ZnO are among the highest reported for PSCs processed at ≤150 °C.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00493

Chinese Library Classification Number:

Citation Information:

Herein, we achieved, air-stable low-temperature processed PSC (L-PSC) using alkali-metal modified ZnO ETLs. Using a simple chemical alkali-metal modification method, the surface defects of the ZnO were effectively passivated. As a result, the interfacial decomposition reactions were suppressed, while raising the Fermi energy level and enhancing electron mobility. The improved interfacial charge transfer and internal electric field in the developed L-PSC using K modified ZnO (ZnO-K) exhibited an improved power conversion efficiency (PCE) of 19.90% with negligible hysteresis, while a pristine ZnO based L-PSC exhibited a PCE of 16.10% with significant hysteresis. The ZnO-K based L-PSC also exhibited remarkably higher long-term air-storage stability (91% retention after 800 h) than pristine ZnO based L-PSCs (36% retention after 800 h) due to the suppressed decomposition reactions. The PCE and air stability of our L-PSC with the modified ZnO are among the highest reported for PSCs processed at ≤150 °C.

quote

GB/T 7714-2015 [1] Randi Azmi, Sunbin Hwang, Wenping Yin, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00493.
MLA [1] Randi Azmi, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00493.
APA [1] Randi Azmi, Sunbin Hwang, Wenping Yin, TaeWook Kim, Tae Kyu Ahn, & SungYeon Jang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00493
IEEE [1] Randi Azmi, Sunbin Hwang, Wenping Yin, TaeWook Kim, Tae Kyu Ahn, and SungYeon Jang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00493.