daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Thermally Activated Shear Stiffening in Polymer-Grafted Nanoparticle Composites for High-Temperature Adhesives AITranslate

Stevens Institute of Technology; Stevens Institute of Technology; Stevens Institute of Technology; Stevens Institute of Technology; Stevens Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thermally activated shear stiffening viscoelastic fluid can help to improve the performance of viscoelastic dampers and high-temperature adhesives. Polymer nanocomposites with heterogeneous interphases are applied to design such adaptive materials. In this work, shear stiffening in polymer-grafted nanoparticle composites is investigated. We report the linear rheological responses of grafted particle composites before and after large-amplitude oscillatory shear application. We found that interfacial mixing of short grafts with chemically different long matrix chains led to the enhancement of plateau moduli and terminal relaxations, unlike with the long grafts. Moreover, we showed that the elastic modulus of grafted chains was enhanced upon deformation through inter-diffusion and entanglements of interfacial layers with the short matrix chains in both grafted systems. These results suggest that dynamic coupling between chemically different polymers away from nanoparticle surfaces is a design strategy to achieve the thermally stiffening behavior in polymer nanocomposites.

KeyWords AITranslate

polymer nanocomposites grafted nanoparticles interphases adsorption deformation rheology adaptive shear stiffening
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00097

Chinese Library Classification Number:

Citation Information:

Thermally activated shear stiffening viscoelastic fluid can help to improve the performance of viscoelastic dampers and high-temperature adhesives. Polymer nanocomposites with heterogeneous interphases are applied to design such adaptive materials. In this work, shear stiffening in polymer-grafted nanoparticle composites is investigated. We report the linear rheological responses of grafted particle composites before and after large-amplitude oscillatory shear application. We found that interfacial mixing of short grafts with chemically different long matrix chains led to the enhancement of plateau moduli and terminal relaxations, unlike with the long grafts. Moreover, we showed that the elastic modulus of grafted chains was enhanced upon deformation through inter-diffusion and entanglements of interfacial layers with the short matrix chains in both grafted systems. These results suggest that dynamic coupling between chemically different polymers away from nanoparticle surfaces is a design strategy to achieve the thermally stiffening behavior in polymer nanocomposites.

quote

GB/T 7714-2015 [1] Di Wu, Yang Ge, Ruhao Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00097.
MLA [1] Di Wu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00097.
APA [1] Di Wu, Yang Ge, Ruhao Li, Yi Feng, & Pinar Akcora. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00097