Rapid Quantitative Determination of Cobalt Phase Structure of Cemented Carbides by X-Ray Diffraction AITranslate

Zigong Cemented Carbide Corp.,Ltd.;Zigong Cemented Carbide Corp.,Ltd.;Zigong Cemented Carbide Corp.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A large number of WC phase on the surface of cemented carbides was removed by chemical corrosion,and then an X-ray diffractometer was used to quickly determine the cobalt phase structure on alloy surface within the selected 2θ angle range.Jade software was used to analyze the characteristic peak areas of different cobalt phase structures,and mass fraction of different cobalt phase structures was calculated with K value method for phase quantification.The method is simple and fast,suitable for production analysis.

KeyWords AITranslate

cemented carbide cobalt phase structure phase quantification rapid determination X-ray diffraction chemical corrosion

1刘寿荣.WC—Co硬质合金中钴相结构的X射线定量相分析[J].稀有金属材料与工程,1992,21(4):61-64. 被引量:9

2龚伟平.热处理对YT14硬质合金钴相成分和结构的影响[J].惠州学院学报,1997,0(4):71-73. 被引量:2

3孙宝琦.关于WC-Co硬质合金的强度和结构问题(Ⅳ)[J].稀有金属与硬质合金,2004,32(4):33-37. 被引量:2

4周建华,孙宝琦.钴相梯度分布硬质合金的研究[J].稀有金属与硬质合金,2002,30(2):11-14. 被引量:17

5郑虎春,周建华,蒋超,刘新儒,秦琳.WC-Co梯度结构硬质合金研究进展[J].超硬材料工程,2012,24(2):14-18. 被引量:4

6黄钧声,吴惕言,李健纯.测定硬质合金中钴相相组成的X射线衍射法[J].硬质合金,2003,20(2):109-112. 被引量:4

7肖满斗,肖伟,江嘉鹭.WC-Co硬质合金的Co相结构[J].粉末冶金材料科学与工程,2010,15(6):611-614. 被引量:12

8刘武,吕满珊,孟力平.热-力循环对热处理硬质合金钴相结构的影响[J].中南工业大学学报,1995,26(3):373-376. 被引量:3

1何姣,方海燕,孙祺,李秋莹,任传婷.密闭溶解-ICP-AES法测定镍基合金中的硼[J].云南冶金,2020,49(5):88-91. 被引量:1

2占美栋,周景安,王新.都昌县2019-2020年度稻油轮作油菜生产分析[J].农民致富之友,2020(33):63-63.

3宋志飞,李肖飞,宋义敏.基于X射线衍射法的岩石残余应力测量研究[J].工业安全与环保,2020,46(11):44-46. 被引量:1

4刘文,张玉德,金云杰,蔡忠文,张选冬.火试金重量法测定金碳基催化剂中金含量[J].贵金属,2020,41(S01):196-198. 被引量:1

5李辉,余江,陈哲.基于混合石墨烯-二氧化钒超材料的太赫兹可调宽带吸收器[J].中国激光,2020,47(9):116-126. 被引量:20

6韩文学,江皓,卞健,云金虎,孙艳艳,张往祥,彭冶.10个观赏海棠品种叶片春季色彩变化及其与色素含量的相关性[J].浙江大学学报:农业与生命科学版,2020,46(5):562-570. 被引量:3

7吕绍杰,张永华,叶旭鸣.一种基于状态矩阵的全天球恒星识别方法研究[J].光学与光电技术,2020(2):93-97.

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

A large number of WC phase on the surface of cemented carbides was removed by chemical corrosion,and then an X-ray diffractometer was used to quickly determine the cobalt phase structure on alloy surface within the selected 2θ angle range.Jade software was used to analyze the characteristic peak areas of different cobalt phase structures,and mass fraction of different cobalt phase structures was calculated with K value method for phase quantification.The method is simple and fast,suitable for production analysis.

quote

GB/T 7714-2015 [1] JIAN Yu-mei, WANG Pei, LI Jun. Rapid Quantitative Determination of Cobalt Phase Structure of Cemented Carbides by X-Ray Diffraction[J]. Rare Metals and Cemented Carbides, 2020(5): 84-87.
MLA [1] JIAN Yu-mei, et al., "Rapid Quantitative Determination of Cobalt Phase Structure of Cemented Carbides by X-Ray Diffraction." Rare Metals and Cemented Carbides, no. 5, 2020, pp. 84-87.
APA [1] JIAN Yu-mei, WANG Pei, & LI Jun. (2020). Rapid Quantitative Determination of Cobalt Phase Structure of Cemented Carbides by X-Ray Diffraction. Rare Metals and Cemented Carbides(5), 84-87.
IEEE [1] JIAN Yu-mei, WANG Pei, and LI Jun, "Rapid Quantitative Determination of Cobalt Phase Structure of Cemented Carbides by X-Ray Diffraction," Rare Metals and Cemented Carbides, no. 5, pp. 84-87, 2020. keywords: {cemented carbide;cobalt phase structure;phase quantification;rapid determination;X-ray diffraction;chemical corrosion}