Study on Dissolution Behavior of CaSO4-WO3System in H2SO4Solution AITranslate

Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

By using the method of bisulfate and tungsten ore roasting,arsenic in tungsten ore could be converted into volatile arsenide and absorbed by the alkaline solution,fundamentally changing the easy-dispersion trend of arsenic in the tungsten smelting system and greatly reducing the formation of the arsenic-containing hazardous waste in tungsten smelting.Simultaneously,the tungsten ore is roasted into MnSO4,Fe2(SO4)3+WO3or CaSO4+WO3products,and the next step is to separate tungsten and impurities in the roasted products effectively to obtain relatively pure tungsten compounds.In general,MnSO4and Fe2(SO4)3could be effectively dissolved by cheap sulfuric acid,but whether CaSO4and WO3could be dissolved in the same way is unknown.Based on this,the dissolution behavior of CaSO4-WO3system in sulfuric acid was systematically studied in this paper.The results show that in the sulfuric acid system,the solubility of CaSO4is significantly greater than that of WO3,and their solubility difference varies little with the concentration of sulfuric acid but greatly with temperature.The effective separation of CaSO4and WO3can be achieved by controlling certain acidity and temperature.

KeyWords AITranslate

tungsten ore CaSO4 WO3 dissolution behavior sulfuric acid separation

1赵中伟,陈星宇,刘旭恒,李江涛.新形势下钨提取冶金面临的挑战与发展[J].矿产保护与利用,2017,37(1):98-102. 被引量:18

2何艺,徐双,靳晓勤,林晓,陶莉,许海青.中国钨渣产生特性及资源化利用技术研究现状[J].中国钨业,2018,33(5):51-56. 被引量:8

3何利华,刘旭恒,赵中伟,梁勇.钨矿物原料碱分解的理论与工艺[J].中国钨业,2012,27(2):22-27. 被引量:15

4肖连生.中国钨提取冶金技术的进步与展望[J].有色金属科学与工程,2013,4(5):6-10. 被引量:20

5李会强,唐忠阳,何利华,陈星宇.离子交换技术在钨冶金中的应用与进展[J].中国钨业,2014,29(5):34-39. 被引量:13

6赵文迪,章晓林,王其宏,景满,申培伦.钨钼分离工艺及机理研究进展[J].有色金属工程,2019,9(4):41-48. 被引量:5

7万林生,邓登飞,赵立夫,李红超,徐国钻,梁勇.钨绿色冶炼工艺研究方向和技术进展[J].有色金属科学与工程,2013,4(5):15-18. 被引量:18

8赵中伟,孙丰龙,杨金洪,方奇,姜文伟,刘旭恒,陈星宇,李江涛.我国钨资源、技术和产业发展现状与展望[J].中国有色金属学报,2019,29(9):1902-1916. 被引量:39

9王宇斌,文堪,王森,汪潇,杨留栓.同离子效应对半水硫酸钙形貌的调控机理[J].高校化学工程学报,2018,32(6):1444-1449. 被引量:11

10万林生,徐国钻,严永海,聂华平,赵立夫,肖学有.中国钨冶炼工艺发展历程及技术进步[J].中国钨业,2009,24(5):63-66. 被引量:20

1唐波,刘乾锋,樊贺飞,张强,王二东.不同金属基底改性Zn负极的电化学性能研究[J].石油化工高等学校学报,2022,35(6):66-73.

2肖杰,何浩,王祥柱,陈群,李东阳.粒度和温度对纳米Ca(OH)_(2)溶解行为的影响[J].广西科技大学学报,2023,34(1):112-120.

3罗天骏,薛云,周羽,马福秋,赵强.乏燃料连续溶解过程的动态仿真模型研究[J].原子能科学技术,2023,57(1):34-46.

4郝璐,冯振华.碘量法测定铜铅合金中铜的方法改进[J].冶金分析,2022,42(10):77-82.

5Ahmed Atef ELIWA,Amal Essam MUBARK,Nasr Abelaziz ABDELFATTAH,Ebrahim Abd El GAWAD.利用柠檬酸浸泡技术最大化利用磷石膏废弃物回收稀土和残留磷酸盐[J].中南大学学报:英文版,2022,29(12):3896-3911. 被引量:1

6石维,王利书,尹海魁,郭海刚,程东娟,杨建斌,黄国铭,徐治国,侯梁.聚丙烯酰胺改性生物质炭对盐碱化土壤盐分洗脱的影响[J].水土保持学报,2023,37(2):371-376. 被引量:1

7杨忠毅,蒋兴良,张志劲,胡建林,杨鑫,刘冬雄.基于离子聚类配对的绝缘子表面可溶污秽化合物成分检测方法[J].高电压技术,2022,48(11):4287-4296. 被引量:1

8刘水平,黄国蕾.微波强化啤酒麦糟深度净化含As(Ⅲ)水的试验研究[J].广东化工,2022,49(24):174-176.

9何容,张广成.漫话《滕王亭子》美刺之讼——兼释“伤心”一词[J].杜甫研究学刊,1991(1):42-45.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]

Citation Information:

By using the method of bisulfate and tungsten ore roasting,arsenic in tungsten ore could be converted into volatile arsenide and absorbed by the alkaline solution,fundamentally changing the easy-dispersion trend of arsenic in the tungsten smelting system and greatly reducing the formation of the arsenic-containing hazardous waste in tungsten smelting.Simultaneously,the tungsten ore is roasted into MnSO4,Fe2(SO4)3+WO3or CaSO4+WO3products,and the next step is to separate tungsten and impurities in the roasted products effectively to obtain relatively pure tungsten compounds.In general,MnSO4and Fe2(SO4)3could be effectively dissolved by cheap sulfuric acid,but whether CaSO4and WO3could be dissolved in the same way is unknown.Based on this,the dissolution behavior of CaSO4-WO3system in sulfuric acid was systematically studied in this paper.The results show that in the sulfuric acid system,the solubility of CaSO4is significantly greater than that of WO3,and their solubility difference varies little with the concentration of sulfuric acid but greatly with temperature.The effective separation of CaSO4and WO3can be achieved by controlling certain acidity and temperature.

quote

GB/T 7714-2015 [1] HE Bing-xuan, XU Lüe-wei, XU Guo-zuan, et al. Study on Dissolution Behavior of CaSO4-WO3System in H2SO4Solution[J]. Rare Metals and Cemented Carbides, 2022(6): 1-5.
MLA [1] HE Bing-xuan, et al., "Study on Dissolution Behavior of CaSO4-WO3System in H2SO4Solution." Rare Metals and Cemented Carbides, no. 6, 2022, pp. 1-5.
APA [1] HE Bing-xuan, XU Lüe-wei, XU Guo-zuan, HU Hao-dong, LEI Xin, LIANG Yong, & LIU De-gang. (2022). Study on Dissolution Behavior of CaSO4-WO3System in H2SO4Solution. Rare Metals and Cemented Carbides(6), 1-5.
IEEE [1] HE Bing-xuan, XU Lüe-wei, XU Guo-zuan, HU Hao-dong, LEI Xin, LIANG Yong, and LIU De-gang, "Study on Dissolution Behavior of CaSO4-WO3System in H2SO4Solution," Rare Metals and Cemented Carbides, no. 6, pp. 1-5, 2022. keywords: {tungsten ore;CaSO;WO;dissolution behavior;sulfuric acid;separation}