daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study of Rapid Precipitation of Crystalline Neodymium Carbonate AITranslate

Hunan Rare Earth Metal Materials Research Institute Hunan Shenghua Rare Earth Metal Materials Co., Ltd.;Hunan Rare Earth Metal Materials Research Institute Hunan Shenghua Rare Earth Metal Materials Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The reaction expression of precipitation and crystallization is put forward based on the pH value change during neodymium chloride precipitation by ammonium hydrocarbonate.Study is made of the influence of feed rate,dosage,aging time on the process of neodymium carbonate crystallization.The technological condition for rapid precipitation of crystalline neodymium carbonate is verified.

KeyWords AITranslate

rapid precipitation crystalline neodymium carbonate new technology

1王毅军,郭军勋.晶型碳酸镨钕沉淀制备工艺的研究[J].稀有金属与硬质合金,2003,31(2):12-14. 被引量:15

2李永绣,黎敏,何小彬,胡平贵,辜子英.碳酸稀土的沉淀与结晶过程[J].中国有色金属学报,1999,9(1):165-170. 被引量:55

1王毅军,郭军勋.快速沉淀晶型碳酸钕的试验研究[J].湿法冶金,2004,23(1):40-42. 被引量:5

2冷忠义,许延辉.直接从盐酸介质中制得低氯根碳酸钕[J].稀土信息,1997,3(12):5-5.

3冷忠义,许延辉.碳酸氢铵沉淀制取氧化钕取得新进展[J].稀土信息,1997,3(9):7-7.

4叶云蔚,陆庆桃.氯化钕熔盐电解的阴极过程[J].湖南有色金属,1990,0(4):32-35.

5刘其城,熊子佳,李灵均,李海滨,龚独明.纳米氧化铜的快速沉淀法制备及表征[J].湖南大学学报:自然科学版,2014,41(2):108-113. 被引量:1

6杨明,吴迪,叶信宇,焦芸芬,吴龙,黄昕,李琴.草酸沉淀反萃余液制备大粒度氧化钕工艺研究[J].有色金属科学与工程,2015,6(1):106-110. 被引量:6

7王毅军,郭军勋.晶型碳酸镨钕沉淀制备工艺的研究[J].稀有金属与硬质合金,2003,31(2):12-14. 被引量:15

8张俊卿,吴志华,韩莉.从少铕氯化稀土中提取氧化铈的研究──碳酸氢铵作为沉淀剂的探讨[J].包头钢铁学院学报,1995,14(1):42-44.

9秦剑,王耀武.真空热还原生产金属钙的现状与问题[J].世界有色金属,2012(12):38-40. 被引量:1

10施惠娟,毛铭华,梁唤珍,康萤,陶昌源.沉淀—水热法制备超细Al(OH)_3γ—AlOOH和Al_2O_3[J].有色金属,1990(4):53-57.

Basic Information:

DOI:

Chinese Library Classification Number:TF111.3[冶金工程—冶金物理化学]

Citation Information:

The reaction expression of precipitation and crystallization is put forward based on the pH value change during neodymium chloride precipitation by ammonium hydrocarbonate.Study is made of the influence of feed rate,dosage,aging time on the process of neodymium carbonate crystallization.The technological condition for rapid precipitation of crystalline neodymium carbonate is verified.

quote

GB/T 7714-2015 [1] WANG Yi-jun, GUO Jun-xun. Study of Rapid Precipitation of Crystalline Neodymium Carbonate[J]. Rare Metals and Cemented Carbides, 2004(1): 5-7.
MLA [1] WANG Yi-jun, and GUO Jun-xun. "Study of Rapid Precipitation of Crystalline Neodymium Carbonate." Rare Metals and Cemented Carbides, no. 1, 2004, pp. 5-7.
APA [1] WANG Yi-jun, & GUO Jun-xun. (2004). Study of Rapid Precipitation of Crystalline Neodymium Carbonate. Rare Metals and Cemented Carbides(1), 5-7.
IEEE [1] WANG Yi-jun and GUO Jun-xun, "Study of Rapid Precipitation of Crystalline Neodymium Carbonate," Rare Metals and Cemented Carbides, no. 1, pp. 5-7, 2004. keywords: {rapid precipitation;crystalline neodymium carbonate;new technology}