The Latest Development and Current Status of Molybdenite Roasting Process AITranslate

School of Chemistry, Central South University;School of Chemistry, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

<Abstrcat>In the paper is reviewed the direct pyrolysis and roasting processes by rotary kiln,reverberatory furnace,multiple hearth furnace,fluidized bed,flash roaster as well as additives co-roasting process for molybdenite.Suggestion is put forward on the development of molybdenum roasting process.

KeyWords AITranslate

molybdenite roasting multiple hearth furnace fluidized bed rotary kiln MoO_3

1Peinhard N L,et al.Process for the production of molybdenum,molybdenum oxide produced from this process and use thereof[P].WO Pat:02059042A1,2002-01-23.

2李庆奎.对提高我国钼冶炼、加工业技术水平的几点看法[J].稀有金属与硬质合金,2001,29(1):40-41. 被引量:4

3张文钲.用高新技术改造钼企业 保持钼业可持续发展[J].中国钼业,2002,26(2):3-6. 被引量:5

4孙晓白.试剂钼酸钠的制备[J].甘肃化工,1990(4):6-8. 被引量:2

5赵晓军.提高钼精矿氧化焙烧合格率及钼收得率的几点措施[J].铁合金,1994,25(6):32-33. 被引量:4

6任宝江.回转窑焙烧钼精矿的生产实践[J].有色金属:冶炼部分,1999(2):18-20. 被引量:7

7Mchugh N F,et al.Roasting of molybdenite concentrates containing flotation oils[P].US:4523948,1985-06-18.

8任宝江.钼精矿回转窑隔层焙烧法[J].中国钼业,1999,23(3):40-42. 被引量:3

9Mchugh L F,et al.Climax conversion Ⅲ[C].Vancouver:The ⅩⅥ Canadian Institute of Mining and Metallurgy Annu Meeting,1977.

10Grimes,G R,et al.Climax conversion practice Ⅱ[J].J Met,1971,23(2):17.

1姚远,罗东卫,符新科.辉钼精矿焙烧工艺评述[J].中国有色冶金,2008,37(2):24-26. 被引量:9

2都基峻,田刚,张凡.钼冶炼工艺的循环经济探讨[J].环境工程,2011,29(S1):381-384. 被引量:3

3唐军利,刘东新,唐丽霞,郭军刚.从钼精矿、氧化钼、钼酸铵质量对比看中外生产技术差异[J].中国钼业,2008,32(2):42-44. 被引量:6

4李大成,洪涛,唐丽霞.钼精矿流态化焙烧工艺及过程分析[J].中国钼业,2008,32(5):18-21. 被引量:11

5王多刚,郭培民,赵沛.辉钼矿直接氢还原工艺的热力学研究[J].有色金属:冶炼部分,2010(3):2-4. 被引量:13

6陈星宇,赵中伟,郝明明,刘旭恒.Cu_2S-MoS_2二元系相图的测定(英文)[J].中国有色金属学报:英文版,2013,23(1):271-275. 被引量:2

7张鸿彪,牟文宁,宋佩,卢媛嫄,孙雷雷.钼矿冶炼新工艺发展概论[J].材料导报:纳米与新材料专辑,2013,27(2):87-90. 被引量:5

8陈晓煜,周俊文,刘秉国,彭金辉,郭胜惠.辉钼精矿在微波场中的升温行为研究[J].无机盐工业,2015,47(7):12-15. 被引量:4

9牟文宁,张鸿彪,苏志强,宋佩.低品位钼矿钠化焙烧-水浸过程钼的转化研究[J].稀有金属,2015,39(9):854-860. 被引量:5

10师留印,杨剑飞,刘会武,贾秀敏,黄永,张引亮,郭晓栋.某包裹型铀钼矿氧化焙烧——酸浸工艺试验研究[J].铀矿冶,2019,38(2):103-107. 被引量:3

1何树荣.工业氧化钼实用生产技术及进展[J].材料开发与应用,2013,28(1):96-101. 被引量:5

2都基峻,田刚,张凡.钼冶炼工艺的循环经济探讨[J].环境工程,2011,29(S1):381-384. 被引量:3

3公彦兵,沈裕军,丁喻,周新东.辉钼矿湿法冶金研究进展[J].矿冶工程,2009,29(1):78-81. 被引量:16

4赵景龙.关于贵州沉积型钼镍矿焙烧工艺的探讨[J].铜业工程,2010(1):62-65. 被引量:3

5王多刚,郭培民,赵沛.碳热还原辉钼矿过程的物相变化规律研究[J].有色金属:冶炼部分,2010(4):6-8. 被引量:3

6丁喻,钟祥,周新东,蔡云卓,刘黄.云南某钼加工厂钼酸铵生产流程查定及技术分析[J].中国钼业,2010,34(4):14-17. 被引量:2

7田刚,都基峻,张凡,刘宇,石应杰.纯氧密闭干法焙烧硫化钼生产氧化钼工艺研究[J].环境工程技术学报,2011,1(2):157-161. 被引量:3

8王锐,张建洲,刘彩霞.钼酸铵的清洁生产工艺[J].化工环保,2011,31(3):265-268. 被引量:5

9沈裕军,杨文魁,公彦兵,丁喻.碱性加压浸出三次氨浸渣中钼的实验研究[J].矿冶工程,2011,31(4):73-76. 被引量:5

10郭培民,庞建明,赵沛.新一代钼冶金技术与新型炼钢钼产品开发[J].有色金属:冶炼部分,2012(6):54-57. 被引量:12

1古隆建.我国火法提钒技术的进展及现状[J].钒钛,1992(6):29-38. 被引量:7

2高建平,李炎,魏世忠,龙锐.钢结硬质合金的研究新进展[J].稀有金属与硬质合金,2006,34(4):55-58. 被引量:9

3甘可可,李溪滨.钢结硬质合金研究进展及现状[J].粉末冶金材料科学与工程,2002,7(3):214-220. 被引量:2

4王永安,白孟田,朱寿康.双层搅拌流化床焙烧锡精矿[J].有色金属,1991(1):50-54.

5琚成新,宫玉川.多膛炉焙烧钼精矿的温度调节与控制[J].中国科技博览,2010(30):322-323.

6琚成新,宫玉川.多膛炉焙烧钼精矿的温度调节与控制[J].中国钼业,2010,34(5):28-31. 被引量:9

7蔡可而,牛太同,薛国文,冯伟宏.拜耳法中分解添加剂的研制[J].中国有色金属,2014(14):66-69.

8金保昇,蓝计香,章名耀.采用流化床焙烧硫酸锶矿降低能源消耗[J].能源研究与利用,1990(2):9-11.

9王锦鸿,邵戈,阳筠,安宁,唐亮.提高次氧化锌铟浸出率试验研究[J].湖南有色金属,2013,29(4):27-29.

10刘吉,杨再明,罗亚林,刘利.循环流化床焙烧生产高温氧化铝[J].有色金属工程,2012,2(4):36-40.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]

Citation Information:

<Abstrcat>In the paper is reviewed the direct pyrolysis and roasting processes by rotary kiln,reverberatory furnace,multiple hearth furnace,fluidized bed,flash roaster as well as additives co-roasting process for molybdenite.Suggestion is put forward on the development of molybdenum roasting process.

quote

GB/T 7714-2015 [1] FU Jian-gang, ZHONG Hong. The Latest Development and Current Status of Molybdenite Roasting Process[J]. Rare Metals and Cemented Carbides, 2005(2): 43-46.
MLA [1] FU Jian-gang, and ZHONG Hong. "The Latest Development and Current Status of Molybdenite Roasting Process." Rare Metals and Cemented Carbides, no. 2, 2005, pp. 43-46.
APA [1] FU Jian-gang, & ZHONG Hong. (2005). The Latest Development and Current Status of Molybdenite Roasting Process. Rare Metals and Cemented Carbides(2), 43-46.
IEEE [1] FU Jian-gang and ZHONG Hong, "The Latest Development and Current Status of Molybdenite Roasting Process," Rare Metals and Cemented Carbides, no. 2, pp. 43-46, 2005. keywords: {molybdenite;roasting;multiple hearth furnace;fluidized bed;rotary kiln;MoO_3}