Effect of Na-Mn Co-Doping on the Structure and Performance of LiFePO4Cathode Materials AITranslate

Faculty of Materials and Metallurgy Chemistry,Jiangxi University of Science and Technology;Faculty of Materials and Metallurgy Chemistry,Jiangxi University of Science and Technology;Faculty of Materials and Metallurgy Chemistry,Jiangxi University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Li0.97Na0.03Fe7/8Mn1/8PO4cathode materials were successfully prepared by carbothermal reduction method.The crystal structure,morphology,elemental distribution,and electrochemical performance of the material were studied by XRD,SEM,EDS,and electrochemical tests,with first-principle calculation being used to analyze the mechanism of the material′s improved performance.The results show that on the one hand,Na-Mn doping leads to the lattice distortion in LiFePO4and the expansion of lattice volume,expanding the lithium ion migration channels and providing more space for lithium ion insertion and extraction.On the other hand,the material exhibits excellent high-rate performance and cycle stability in electrochemical performance.Na-Mn doping is advantageous in improving the lithium-ion diffusion coefficient and conductivity of the material,thereby improving its electrochemical performance.The first-principle calculation results show that Na-Mn co-doping induces lattice expansion of LiFePO4,increases lattice volume,narrows energy band gap,enhances electronic density of states near Fermi level,and improves the electronic conductivity and lithium ion mobility of the material.

KeyWords AITranslate

Na-Mnco-doping LiFePO4 cathode material crystal structure electrochemical performance en-ergy band first-principle calculation

1郑世富,黄佩佩,张建勇,易元刚,杨杰,罗成兵.锂离子电池发展趋势及回收工艺对比[J].江西化工,2024,40(1):16-18.

2张学宾,谷继华,封存利,鲁龙龙,张彦敏,宋克兴,皇涛.Cu-4Ag合金微细丝拉拔极限预测模型[J].塑性工程学报,2024,31(2):157-162.

3赵萍.分析生产制造企业成本管理的优化策略[J].市场瞭望,2023(19):57-59.

4Lei Wang,Yan Jiang,Shao-Yuan Li,Xiu-Hua Chen,Feng-Shuo Xi,Xiao-Han Wan,Wen-Hui Ma,Rong Deng.Scalable synthesis of N-doped Si/G@voids@C with porous structures for high-performance anode of lithium-ion batteries[J].Rare Metals,2023,42(12):4091-4102.

5Huanhui Chen,Xing Cao,Moujie Huang,Xiangzhong Ren,Yubin Zhao,Liang Yu,Ya Liu,Liubiao Zhong,Yejun Qiu.In-situ interfacial passivation and self-adaptability synergistically stabilizing all-solid-state lithium metal batteries[J].Journal of Energy Chemistry,2024,88(1):282-292.

6何逸,郑传波,戚浩宇,刘珍光.TP2紫铜在工业环境中腐蚀行为的研究[J].中国腐蚀与防护学报,2024,44(1):71-81.

7王茂成,李赣,程浩,姜维,陈广,李海波.双波长近红外拉曼光谱仪及在腐蚀产物分析中的应用[J].光谱学与光谱分析,2024,44(3):756-761.

Basic Information:

DOI:

Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]

Citation Information:

Li0.97Na0.03Fe7/8Mn1/8PO4cathode materials were successfully prepared by carbothermal reduction method.The crystal structure,morphology,elemental distribution,and electrochemical performance of the material were studied by XRD,SEM,EDS,and electrochemical tests,with first-principle calculation being used to analyze the mechanism of the material′s improved performance.The results show that on the one hand,Na-Mn doping leads to the lattice distortion in LiFePO4and the expansion of lattice volume,expanding the lithium ion migration channels and providing more space for lithium ion insertion and extraction.On the other hand,the material exhibits excellent high-rate performance and cycle stability in electrochemical performance.Na-Mn doping is advantageous in improving the lithium-ion diffusion coefficient and conductivity of the material,thereby improving its electrochemical performance.The first-principle calculation results show that Na-Mn co-doping induces lattice expansion of LiFePO4,increases lattice volume,narrows energy band gap,enhances electronic density of states near Fermi level,and improves the electronic conductivity and lithium ion mobility of the material.

quote

GB/T 7714-2015 [1] LIU Qing-sheng, FU Qin-wu, YU Xiu-yuan. Effect of Na-Mn Co-Doping on the Structure and Performance of LiFePO4Cathode Materials[J]. Rare Metals and Cemented Carbides, 2024(1): 90-98.
MLA [1] LIU Qing-sheng, et al., "Effect of Na-Mn Co-Doping on the Structure and Performance of LiFePO4Cathode Materials." Rare Metals and Cemented Carbides, no. 1, 2024, pp. 90-98.
APA [1] LIU Qing-sheng, FU Qin-wu, & YU Xiu-yuan. (2024). Effect of Na-Mn Co-Doping on the Structure and Performance of LiFePO4Cathode Materials. Rare Metals and Cemented Carbides(1), 90-98.
IEEE [1] LIU Qing-sheng, FU Qin-wu, and YU Xiu-yuan, "Effect of Na-Mn Co-Doping on the Structure and Performance of LiFePO4Cathode Materials," Rare Metals and Cemented Carbides, no. 1, pp. 90-98, 2024. keywords: {Na-Mnco-doping;LiFePO;cathode material;crystal structure;electrochemical performance;en-ergy band;first-principle calculation}