daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Quantification of the Retention and Disassembly of Virus Particles by a PEI-Functionalized Microfiltration Membrane AITranslate

University of Twente; University of Twente; University of Twente; University of Twente;Wetsus, European Centre of Excellence for Sustainable Water Technology; University of Twente; University of Twente; University of Twente
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Monitoring the performance of polymer-functionalized surfaces that aim at removing and inactivating viruses is typically labor-intensive and time-consuming. This hampers the development and optimization of such surfaces. Here we present experiments of low complexity that can be used to characterize and quantify the antiviral properties of polymer-functionalized surfaces. We showcase our approach on polyethylenimine (PEI)-coated poly(ether sulfone) (PES) microfiltration membranes. We use a fluorescently labeled model virus to quantify both virus removal and inactivation. We directly quantify the log removal of intact viruses by this membrane using single particle counting. Additionally, we exploit the change in photophysical properties upon disassembly of the virus to show that viruses are inactivated by the PEI coating. Although only a small fraction of intact viruses can pass the membrane, a considerable fraction of inactivated, disassembled viruses are found in the filtrate. Fluorescence microscopy experiments show that most of the viruses left behind on the microfiltration membrane are in the inactivated, disassembled state. Combined, our fluorescence microscopy and spectroscopy experiments show that not only does the model virus adsorb to the PEI coating on the membrane but also the interaction with PEI results in the disassembly of the virus capsid.

KeyWords AITranslate

virucidal surface fluorescence microscopy fluorescence spectroscopy microfiltration virus inactivation virus retention
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00560

Chinese Library Classification Number:

Citation Information:

Monitoring the performance of polymer-functionalized surfaces that aim at removing and inactivating viruses is typically labor-intensive and time-consuming. This hampers the development and optimization of such surfaces. Here we present experiments of low complexity that can be used to characterize and quantify the antiviral properties of polymer-functionalized surfaces. We showcase our approach on polyethylenimine (PEI)-coated poly(ether sulfone) (PES) microfiltration membranes. We use a fluorescently labeled model virus to quantify both virus removal and inactivation. We directly quantify the log removal of intact viruses by this membrane using single particle counting. Additionally, we exploit the change in photophysical properties upon disassembly of the virus to show that viruses are inactivated by the PEI coating. Although only a small fraction of intact viruses can pass the membrane, a considerable fraction of inactivated, disassembled viruses are found in the filtrate. Fluorescence microscopy experiments show that most of the viruses left behind on the microfiltration membrane are in the inactivated, disassembled state. Combined, our fluorescence microscopy and spectroscopy experiments show that not only does the model virus adsorb to the PEI coating on the membrane but also the interaction with PEI results in the disassembly of the virus capsid.

quote

GB/T 7714-2015 [1] Swarupa Chatterjee, Robert Molenaar, Wiebe M. de Vos, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00560.
MLA [1] Swarupa Chatterjee, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00560.
APA [1] Swarupa Chatterjee, Robert Molenaar, Wiebe M. de Vos, Hendrik D. W. Roesink, R. Martijn Wagterveld, Jeroen J. L. M. Cornelissen, Mireille M. A. E. Claessens, & Christian Blum. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00560
IEEE [1] Swarupa Chatterjee, Robert Molenaar, Wiebe M. de Vos, Hendrik D. W. Roesink, R. Martijn Wagterveld, Jeroen J. L. M. Cornelissen, Mireille M. A. E. Claessens, and Christian Blum, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00560. keywords: {virucidal surface;fluorescence microscopy;fluorescence spectroscopy;microfiltration;virus inactivation;virus retention}