Study of RE Mo Ejector Material AITranslate

Zhuzhou Hard Alloy Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on TZC material for PIM Mo ejector,study and on the site tests were made in respect of the high temperature strength and hardness and microscopic structures of the TZC alloy with the addition of single RE cerium and also Ce Yt RE element.The results showed that the addition of Ce in the alloy can greatly improve the alloy hardness while addition of Yt can greatly improve the alloy high temperature strength.The addition of both Ce amd Yt at the same time will result in compound intensifying effect with much larger high temperature strength and hardness,allowing for~25%more ST billet through capacity

KeyWords AITranslate

Mo ejector RE addition high temperature property billet through times

1株洲硬质合金厂粉冶态钼顶头技术鉴定书[R].湘冶科字(80)003号.1980-04-10.

2刘戊生.镧、钇复合稀土钼合金的研究[J].中国钼业,1999,23(6):19-22. 被引量:4

1田丹,张俊,罗振中.粉冶钼基合金顶头的生产与质量控制[J].中国钼业,2008,32(2):49-51. 被引量:4

2周伟,卢静,陈双柏,蒋兵.物理破碎法改善钼粉性能对TZC钼合金顶头密度影响的研究[J].中国钼业,2010,34(4):35-38. 被引量:2

3史振琦,黄晓玲,易永鹏.影响钼合金顶头使用寿命因素浅析[J].中国钼业,2014,38(5):57-60. 被引量:6

4刘晓平,王快社,胡平,陈强.感应等离子体工艺对制备致密球形钼粉的影响[J].金属热处理,2015,40(10):76-80. 被引量:5

5郭磊,宋瑞,淡新国,金波,赵娟,张清,胡平.稀土钼合金制备工艺及强韧化机理研究现状[J].中国钼业,2017,41(2):45-51. 被引量:6

6潘以庆,田青超,徐文进.钼合金顶头制备技术研究进展[J].粉末冶金技术,2021,39(5):452-461. 被引量:1

7周红灯,徐文进,田青超.钼合金穿孔顶头失效分析[J].钢管,2023,52(1):78-83.

1周伟,卢静,陈双柏,蒋兵.物理破碎法改善钼粉性能对TZC钼合金顶头密度影响的研究[J].中国钼业,2010,34(4):35-38. 被引量:2

2刘秋萍.钼粉质量分析及对后续加工的影响[J].延安大学学报:自然科学版,2013,32(1):55-57. 被引量:2

3史振琦,黄晓玲,易永鹏.影响钼合金顶头使用寿命因素浅析[J].中国钼业,2014,38(5):57-60. 被引量:6

4居炎鹏,王爱琴.钼合金研究现状[J].粉末冶金工业,2015,25(4):58-62. 被引量:29

5王瑞雪,陈岁元,马雪耻,梁京,刘常升.激光直接沉积制备Mo-Ni-ZrO2高温耐磨复合合金梯度涂层[J].复合材料学报,2017,34(9):1989-1996. 被引量:4

6杨礼林,张启富,贺智勇,李晓刚.HfC添加对钼钨合金高温等离子烧蚀性能影响及机理分析[J].粉末冶金材料科学与工程,2018,23(2):137-146. 被引量:7

7于金程,秦丰,钱王欢,田学锋,陈玉平.高温高应变率下纯钼动态力学性能与失效行为[J].有色金属工程,2019,9(5):28-33. 被引量:1

8陈金童,刘广华,张明亚.高Cr合金钢穿孔毛管内螺旋产生原因及其改善措施[J].钢管,2019,48(5):45-47. 被引量:1

9赵虎.钼及钼合金烧结技术研究及发展[J].粉末冶金技术,2019,37(5):382-391. 被引量:11

10金园园,贺卫卫,陈斌科,汤慧萍,向长淑,朱纪磊,邱沙,王宇.球形难熔金属粉末的制备技术[J].航空制造技术,2019,62(22):64-72. 被引量:11

1吕海当,胡梅青,马正伟,施黎明,李旺.06Cr25Ni20(310S)不锈钢荒管开裂原因分析[J].大型铸锻件,2015(4):20-22. 被引量:2

2王治国,张新辉,孔祥华.穿轧钢管用的钼顶头[J].中国钼业,2008,32(3):36-36.

3田丹,张俊,罗振中.粉冶钼基合金顶头的生产与质量控制[J].中国钼业,2008,32(2):49-51. 被引量:4

4韩强,赵宝华.TZCR钼顶头的研制及外形设计[J].中国钼业,2002,26(3):40-41. 被引量:3

5王神怀.GH140高温合金的斜轧穿孔试验[J].长城技术,1991(4):8-11.

6左羽飞,张常乐,仙彬华.钼合金 顶头破坏行为及强韧化分析[J].稀有金属快报,2004,23(1):38-40. 被引量:2

7刘志刚,齐艳飞,边勇俊,陈洁,闫涛.0Cr18Ni9不锈钢管孔洞成因分析[J].物理测试,2015,33(5):51-53. 被引量:4

8王竞,王光煌.扩大Φ100mm穿孔机组产品规格的工艺试验[J].钢管,1998,27(3):20-23.

9常学增.穿孔机20CrNi8顶头的穿孔试验[J].钢管,1996,25(5):45-46. 被引量:2

10许莹.衡阳华菱钢管有限公司成功开发出Gr3低温用管[J].钢管,2014,43(1):66-66.

Basic Information:

DOI:

Chinese Library Classification Number:TG333.8[金属学及工艺—金属压力加工];TG146.412[金属学及工艺—金属材料]

Citation Information:

Based on TZC material for PIM Mo ejector,study and on the site tests were made in respect of the high temperature strength and hardness and microscopic structures of the TZC alloy with the addition of single RE cerium and also Ce Yt RE element.The results showed that the addition of Ce in the alloy can greatly improve the alloy hardness while addition of Yt can greatly improve the alloy high temperature strength.The addition of both Ce amd Yt at the same time will result in compound intensifying effect with much larger high temperature strength and hardness,allowing for~25%more ST billet through capacity

quote

GB/T 7714-2015 [1] CENG Jian-hui. Study of RE Mo Ejector Material[J]. Rare Metals and Cemented Carbides, 2001(2): 30-35.
MLA [1] CENG Jian-hui. "Study of RE Mo Ejector Material." Rare Metals and Cemented Carbides, no. 2, 2001, pp. 30-35.
APA [1] CENG Jian-hui. (2001). Study of RE Mo Ejector Material. Rare Metals and Cemented Carbides(2), 30-35.
IEEE [1] CENG Jian-hui, "Study of RE Mo Ejector Material," Rare Metals and Cemented Carbides, no. 2, pp. 30-35, 2001. keywords: {Mo ejector;RE addition;high temperature property;billet through times}