Study of Separation of Tungsten and Molybdenum from High W-containing Molybdate Acid Sodium Solution by Fe(OH)_3 Adsorption AITranslate
Abstract AITranslate
Study is made of the possibility and technical requirements of separating tungsten from high W- containing Na2MO4 solution by Fe (OH)3 adsorption. The results showed that each absorption resulted in 70 % ~80 % tungsten separation from molybdenum at pH = 7.0 and with consumption 2~4 times more than that of WO4^2- . When WO3/Mo = 0. 445, WO3/Mo is reduced down to 0.17~ 0.18 through the first absorption. A new method is developed to neutralize sodium molybdate solution with HCl and NH4Cl as neutralizer, which can notably improve recovery and separating effect.
KeyWords AITranslate
1肖连生,张启修,龚柏藩,黄芍英.密实移动床——流化床离子交换除钼技术在工业上的应用[J].中国钨业,2001,16(2):26-29. 被引量:21
2李洪桂.有色金属提取手册—稀有高熔点金属(上)[M].北京:冶金工业出版社,1999.118.
3冶金过程强化学科组.“选择性沉淀法从钨酸盐溶液中除钼、砷、锡、锑”专利技术的新进展[J].中国钨业,2000,15(4):29-30. 被引量:7
4霍广生,孙培梅,李洪桂,李运姣,赵中伟,苏鹏抟.离子浮选法从钨酸盐溶液中分离钨钼[J].中国钨业,1999,14(3):35-36. 被引量:12
5范薇,黄普选,姚莉,康定学.氨浸法生产钼酸铵中钨的分离[J].无机盐工业,2001,33(5):3-4. 被引量:8
1赵中伟,李江涛,曹才放,霍广生,陈爱良,李洪桂.从钼酸盐溶液中深度除去杂质钨的研究[J].稀有金属与硬质合金,2008,36(1):1-4. 被引量:4
2张文朴.我国钼资源综合利用与再生研发进展评述[J].中国资源综合利用,2006,24(12):4-7. 被引量:8
3张文朴.我国钼资源中稀贵金属的综合利用与再生回收研发进展[J].稀有金属与硬质合金,2007,35(2):35-39. 被引量:5
4张文朴.我国钼资源及稀贵金属的回收与综合利用[J].资源再生,2007(11):26-29. 被引量:2
5刘能生,朱薇,肖连生.从钼酸盐溶液中分离微量钨的研究进展[J].中国钼业,2008,32(2):20-24. 被引量:2
6朱艳婧,杨元法,王莎,陈敏,徐明涛,赵亮亮.Fe(OH)_3催化苯酚羟基化反应[J].石油化工,2009,38(7):739-744. 被引量:4
7肖超,肖连生,曹佐英.从钼酸盐溶液中分离微量钨的机理研究[J].中国钼业,2011,35(2):29-32. 被引量:4
8杨亮,赵中伟,陈爱良,刘旭恒,霍广生.从钼酸铵溶液中除去砷的研究[J].中南大学学报:自然科学版,2011,42(8):2193-2197. 被引量:4
9赵中伟,曹才放,陈星宇.铁盐沉淀法分离宏量钨钼(英文)[J].中国有色金属学报:英文版,2011,21(12):2758-2763. 被引量:10
10张家靓,赵中伟,陈星宇,刘旭恒.W-Mo-H_2O体系钨钼分离的热力学分析[J].中国有色金属学报,2013,23(5):1463-1470. 被引量:16
1龚丹丹,周康根,陈伟,彭长宏,李俊杰.氯化镁焙烧-碱浸工艺处理钨矿研究[J].稀有金属,2020,0(1):72-78. 被引量:4
2邓桂春,邢楠楠,吕改芳,鞠政楠,叶琳琳.熔剂对低品位钼精矿焙烧时的影响[J].辽宁大学学报:自然科学版,2009,36(4):349-352. 被引量:2
3关文娟,肖连生,张贵清,李青刚,龚柏藩.利用低品位镍钼矿生产高纯多钼酸铵技术的工业应用[J].中国钼业,2010,34(1):42-45.
4冷明锋.吸附共沉淀法分离钼酸铵中的钨[J].中国钼业,2011,35(2):36-38. 被引量:3
5赵亮亮,杨元法,李艳妮,刘兰香,朱玉梅.对叔丁基苯酚羟基化反应的研究[J].石油化工,2011,40(6):624-629. 被引量:1
6王玉峰,王建平,戚开静,朝银银,柳振江.中国钼产业国际地位的变化及可持续发展建议[J].中国矿业,2011,20(9):9-12. 被引量:7
7徐志昌,张萍.乏催化剂综合回收工艺现状与展望[J].中国钼业,2011,35(6):21-37.
8程远见,姜红,陈日志,邢卫红,金万勤.纳米晶氧化铜的制备及其催化苯酚氧化性能[J].石油化工,2012,41(4):391-395. 被引量:7
9张亨.钼酸铵的生产研究综述[J].杭州化工,2012,42(2):11-15. 被引量:3
10曹占芳,钟宏,刘广义,王帅.我国矿产资源的特点及其加工技术与专业教学现状[J].稀有金属与硬质合金,2012,40(5):18-22. 被引量:2
1吴免利,伊继光,赵虎,谢添,杨芬,张贵清.碱性离子交换制取钼酸铵溶液研究[J].中国有色冶金,2010,39(6):71-74. 被引量:3
2赵由才,于淑秋,陈家镛.N1923-TBP从Na_2MoO_4溶液中同时萃取分离磷和砷[J].稀有金属,1991,15(4):241-245.
3肖超,肖连生.沉淀-共沉淀法净化钼酸钠溶液实验研究[J].稀有金属与硬质合金,2010,38(4):10-12. 被引量:2
4丁扬力,肖连生,曹佐英,张贵清,曾理.N263从钼酸钠溶液中萃取分离钼钒[J].有色金属科学与工程,2017,8(1):15-20. 被引量:6
5牛旭斐,朱云,王晓丹,饶金元.氧化铝对钼浸出的影响[J].中国钼业,2009,33(6):38-40.
6陈星宇,肖露萍,赵中伟.钨钼冶炼过程中除钒[J].中国有色金属学报,2014,24(7):1883-1887. 被引量:5
7赵由才,于淑秋,陈家镛.伯胺-磷酸三丁酯协同萃取分离钼酸钠溶液中磷的机理研究[J].有色金属,1992(3):59-62. 被引量:1
8王文强,何利华,赵中伟.钨钼分离吸附剂的选择性判据[J].中国有色金属学报,2015,25(8):2236-2242. 被引量:2
9刘桂华,高君丽,李小斌,徐双.拜耳法高压溶出液中铁浓度变化规律的研究[J].矿冶工程,2007,27(5):38-40. 被引量:7
10申玉芳,张振军,邹正光.行星球磨法加工制备SiC超细粉[J].材料导报,2005,19(F05):152-154. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]
Citation Information:
Study is made of the possibility and technical requirements of separating tungsten from high W- containing Na2MO4 solution by Fe (OH)3 adsorption. The results showed that each absorption resulted in 70 % ~80 % tungsten separation from molybdenum at pH = 7.0 and with consumption 2~4 times more than that of WO4^2- . When WO3/Mo = 0. 445, WO3/Mo is reduced down to 0.17~ 0.18 through the first absorption. A new method is developed to neutralize sodium molybdate solution with HCl and NH4Cl as neutralizer, which can notably improve recovery and separating effect.
quote
| GB/T 7714-2015 | [1] LV Ying, SUN Fang. Study of Separation of Tungsten and Molybdenum from High W-containing Molybdate Acid Sodium Solution by Fe(OH)_3 Adsorption[J]. Rare Metals and Cemented Carbides, 2005(3): 1-3. |
| MLA | [1] LV Ying, and SUN Fang. "Study of Separation of Tungsten and Molybdenum from High W-containing Molybdate Acid Sodium Solution by Fe(OH)_3 Adsorption." Rare Metals and Cemented Carbides, no. 3, 2005, pp. 1-3. |
| APA | [1] LV Ying, & SUN Fang. (2005). Study of Separation of Tungsten and Molybdenum from High W-containing Molybdate Acid Sodium Solution by Fe(OH)_3 Adsorption. Rare Metals and Cemented Carbides(3), 1-3. |
| IEEE | [1] LV Ying and SUN Fang, "Study of Separation of Tungsten and Molybdenum from High W-containing Molybdate Acid Sodium Solution by Fe(OH)_3 Adsorption," Rare Metals and Cemented Carbides, no. 3, pp. 1-3, 2005. keywords: {Fe(OH)3 adsorption;high W- containing Na2MO4 solution;separation of tungsten and molybdenum} |