daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Elucidating Reversible Electrochemical Redox of Li6PS5Cl Solid Electrolyte AITranslate

University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; Lawrence Livermore National Laboratory; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego; University of California San Diego
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sulfide-based solid electrolytes are promising candidates for all solid-state batteries (ASSBs) due to their high ionic conductivity and ease of processability. However, their narrow electrochemical stability window causes undesirable electrolyte decomposition. Existing literature on Li-ion ASSBs report an irreversible nature of such decompositions, while Li–S ASSBs show evidence of some reversibility. Here, we explain these observations by investigating the redox mechanism of argyrodite Li6PS5Cl at various chemical potentials. We found that Li–In | Li6PS5Cl | Li6PS5Cl–C half-cells can be cycled reversibly, delivering capacities of 965 mAh g–1 for the electrolyte itself. During charging, Li6PS5Cl forms oxidized products of sulfur (S) and phosphorus pentasulfide (P2S5), while during discharge, these products are first reduced to a Li3PS4 intermediate before forming lithium sulfide (Li2S) and lithium phosphide (Li3P). Finally, we quantified the relative contributions of the products toward cell impedance and proposed a strategy to reduce electrolyte decomposition and increase cell Coulombic efficiency.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01693

Chinese Library Classification Number:

Citation Information:

Sulfide-based solid electrolytes are promising candidates for all solid-state batteries (ASSBs) due to their high ionic conductivity and ease of processability. However, their narrow electrochemical stability window causes undesirable electrolyte decomposition. Existing literature on Li-ion ASSBs report an irreversible nature of such decompositions, while Li–S ASSBs show evidence of some reversibility. Here, we explain these observations by investigating the redox mechanism of argyrodite Li6PS5Cl at various chemical potentials. We found that Li–In | Li6PS5Cl | Li6PS5Cl–C half-cells can be cycled reversibly, delivering capacities of 965 mAh g–1 for the electrolyte itself. During charging, Li6PS5Cl forms oxidized products of sulfur (S) and phosphorus pentasulfide (P2S5), while during discharge, these products are first reduced to a Li3PS4 intermediate before forming lithium sulfide (Li2S) and lithium phosphide (Li3P). Finally, we quantified the relative contributions of the products toward cell impedance and proposed a strategy to reduce electrolyte decomposition and increase cell Coulombic efficiency.

quote

GB/T 7714-2015 [1] Darren H. S. Tan, Erik A. Wu, Han Nguyen, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01693.
MLA [1] Darren H. S. Tan, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01693.
APA [1] Darren H. S. Tan, Erik A. Wu, Han Nguyen, Zheng Chen, Maxwell A. T. Marple, JeanMarie Doux, Xuefeng Wang, Hedi Yang, Abhik Banerjee, & Ying Shirley Meng. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01693
IEEE [1] Darren H. S. Tan, Erik A. Wu, Han Nguyen, Zheng Chen, Maxwell A. T. Marple, JeanMarie Doux, Xuefeng Wang, Hedi Yang, Abhik Banerjee, and Ying Shirley Meng, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01693.