daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Stress Engineering: The Response of Phase Change Materials to Mechanical Stimuli Stress Engineering: The Response of Phase Change Materials to Mechanical Stimuli AITranslate

Isfahan University of Technology; Isfahan University of Technology; Wright State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The phase transition (PT) in phase change materials (PCMs) can be triggered by external stimuli, e.g., light or heat, resulting in a drastic change in their physical properties, such as electrical resistivity. Due to this rapid PT, PCMs are promising candidates for various applications, including reconfigurable electronics, photonics, sensors, and memory devices. Here, a coupled phase-field model was developed to investigate the effect of mechanical stress as an overlooked factor on the PT of germanium–antimony–tellurium. The results suggest that mean compressive stress promotes crystal growth, while tensile stress hinders crystallization. Moreover, stress alters the shape of spherical nuclei and promotes the anisotropic growth. Finally, mushroom-shaped grains can be formed in the high-temperature regime due to the heterogeneous stress distribution around interacting nuclei. These findings suggest a pathway for tailoring microstructure and tuning/controlling crystallization time via mechanical stresses.

KeyWords AITranslate

phase change material isothermal annealing germanium−antimony−tellurium (GST) mechanical stress phase transition
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00605

Chinese Library Classification Number:

Citation Information:

The phase transition (PT) in phase change materials (PCMs) can be triggered by external stimuli, e.g., light or heat, resulting in a drastic change in their physical properties, such as electrical resistivity. Due to this rapid PT, PCMs are promising candidates for various applications, including reconfigurable electronics, photonics, sensors, and memory devices. Here, a coupled phase-field model was developed to investigate the effect of mechanical stress as an overlooked factor on the PT of germanium–antimony–tellurium. The results suggest that mean compressive stress promotes crystal growth, while tensile stress hinders crystallization. Moreover, stress alters the shape of spherical nuclei and promotes the anisotropic growth. Finally, mushroom-shaped grains can be formed in the high-temperature regime due to the heterogeneous stress distribution around interacting nuclei. These findings suggest a pathway for tailoring microstructure and tuning/controlling crystallization time via mechanical stresses.

quote

GB/T 7714-2015 [1] Mahdi Javanbakht, Sajjad Mohebbi, Hamed Attariani. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00605.
MLA [1] Mahdi Javanbakht, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00605.
APA [1] Mahdi Javanbakht, Sajjad Mohebbi, & Hamed Attariani. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00605
IEEE [1] Mahdi Javanbakht, Sajjad Mohebbi, and Hamed Attariani, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00605. keywords: {phase change material isothermal annealing germanium−antimony−tellurium (GST) mechanical stress phase transition}