Influence of H_3BO_3 Content on the Luminescent Performance of CaTiO_3∶Pr3+ AITranslate
Abstract AITranslate
CaTiO3:Pr3+ was prepared by high-temperature solid phase carried out with H3BO3. Its emission spectrum, glow brightness and fluences of H3BO3 content on the emission intensity and luminescent discussed. The results show that the prepared CaTiO3 : Pr3+ is of the method, and doping afterglow time were modification was studied. The inperformance of CaTiO3 : Pr3+ were optimal afterglow performance when H3BO3 is at 15% molar fraction
KeyWords AITranslate
1Diallo P T, Boutinaud P,Mahiou R,et al. Red lumines-cence in Pr3+-doped calcium titanates[J].J Phys Status Solidi A,1997,160(1) :255-263.
2Diallo P T, Jenlouis K, Boutinaud P, et al. Improvement of the optical performances of Pr3+ in CaTiO3 [J]. J Alloys Compd, 2001,323-324 : 218-222.
3Royce M R, Matsuda S, Tamaki H. Red emitting long decay phosphors[P]. US Pat:5650094,1997-07-22.
4Pan Yuexiao,Su Qiang,Xu Huifang,et al. Synthesis and red luminescence of Pr3+ -doped CaTiO3 nanophosphor from polymer precursor[J]. J Solid Stat Chem, 2003, 174:69-73.
5Suh Kyung Soo,Lee Jin Ho,Cho Kyoung Ik,et al. Red phosphor for fluorescent display and preparation method thereof[P]. US Pat: 6373184,2002-04-16.
6刘利民,曾立华,廉世勋,张华京,毛向辉,彭夷安,刘莲英.CaTiO_3∶Pr^(3+)的合成及发光特性[J].湖南有色金属,1998,14(5):45-47. 被引量:14
7陈一诚,陈登铭,詹益松.杂质的添加对SrAl_2O_4∶Eu^(2+),Dy^(3+)余辉发光特性的改善[J].中国稀土学报,2001,19(6):502-506. 被引量:22
8林元华,唐子龙,张中太,王晓欣.不同添加剂对Sr_4Al_(14)O_(25)∶Eu,Dy长余辉光致发光性能的影响[J].硅酸盐学报,2001,29(3):218-220. 被引量:21
9吕兴栋,舒万艮,黄可龙,周文华.掺杂B^(3+)在SrAl_2O_4∶Eu,Dy中的作用及其机制研究[J].中国稀土学报,2004,22(3):312-317. 被引量:18
1夏昌奎,雷芳,施鹰,余爱民,肖维勤,余剑峰.Pr^(3+)掺杂CaTiO_3红色长余辉发光材料的湿法共混-高温固相制备和发光性能[J].中国陶瓷,2017,53(5):36-41. 被引量:1
2熊钦茂,彭晓东,龙红雨,范强,杨建会.H_3BO_3对CaTiO_3:Eu^(3+)荧光粉发光性能的影响[J].云南化工,2018,45(8):93-94. 被引量:1
3魏白光,吕秋月.烧结温度对长余辉发光材料Ca2Zn4Ti15O36:Pr^3+光性能的影响[J].吉林化工学院学报,2018,35(11):76-79. 被引量:1
4王乃芹.Zn掺杂CaTiO_(3)∶Pr^(3+)红色长余辉发光材料的制备及发光性能[J].中国照明电器,2022(1):44-47. 被引量:1
1何春梅,肖婕,孙文龙,胡萍,杨建会,范强.Li+掺杂Mg2TiO4:Mh4+荧光粉制备与发光性能研究[J].内江科技,2021,42(5):122-123.
2王俊兰,杨紫淇,娄三钢,张佩聪,邱克辉.CaTiO_3∶Pr^(3+)光催化降解亚甲基蓝的实验研究[J].功能材料,2018,49(9):9111-9114. 被引量:1
3马鹏飞,胥佳颖.异丙醇添加剂在钙钛矿太阳能电池中的应用[J].大学物理实验,2019,32(6):32-35. 被引量:2
4王乃芹,卢婷.Si掺杂对Ca_(0.8)Zn_(0.2)TiO_(3)∶Pr^(3+)红色长余辉发光材料的影响[J].中国照明电器,2022(11):20-23.
1赵艳茹,韩培林,刘春辉.聚乙二醇对水热法制备CaTiO_3:Pr^(3+)发光性能的影响[J].化学试剂,2013,35(5):448-450. 被引量:2
2王飞,刘利军,王其洪,于凯立,邵泽.新型红色长余辉发光材料Gd_2O_2S:Eu^(3+),Si^(4+),Ti^(4+)的合成及性能表征(英文)[J].中山大学学报:自然科学版,2009,48(S2):109-112.
3周新木,张丽,曾慧慧,董雪平,陈慧勤.红色长余辉发光材料BaMg_2Si_2O_7∶Pr,Mn的制备及性质研究[J].稀土,2010,31(1):11-15. 被引量:4
4宋艳华,甘树才,邓岳锋,洪广言,孟健.红色长余辉材料Zn_3(PO_4)_2:Mn^(2+),Ga^(3+)的合成及光谱性质[J].发光学报,2006,27(4):484-488. 被引量:6
5陈芮,王莎莎,雷雨霫,李金燕.Eu^(3+)、Dy^(3+)对CaTiO_3:Pr^(3+)红色磷光体发光性能的影响[J].化学与生物工程,2009,26(8):29-31. 被引量:2
6陈钻宇,李文宇.纳米红色长余辉发光材料的合成及其发光特性[J].丽水学院学报,2017,39(2):45-51. 被引量:1
7李随源,刘晓花.硅酸盐长余辉发光材料的研究进展与展望[J].焦作师范高等专科学校学报,2009,25(4):70-74. 被引量:2
8刘正伟,刘应亮,袁定胜,张静娴,容建华,黄浪欢.CaWO_4中Eu^(3+)的长余辉发光[J].无机化学学报,2004,20(12):1433-1436. 被引量:15
9王飞,刘大春,杨斌,刘利军,戴永年.掺杂离子对Gd_2O_2S:Eu^(3+)磷光体结构和发光性能的影响[J].中国有色金属学报,2012,22(4):1107-1112. 被引量:8
10陈海英,王明文,刘世香,陈学娟.基质掺杂对CdSiO_3∶Sm^(3+)体系红色长余辉发光材料的影响[J].安徽化工,2008,34(5):19-21. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:O614.334[理学—无机化学]
Citation Information:
CaTiO3:Pr3+ was prepared by high-temperature solid phase carried out with H3BO3. Its emission spectrum, glow brightness and fluences of H3BO3 content on the emission intensity and luminescent discussed. The results show that the prepared CaTiO3 : Pr3+ is of the method, and doping afterglow time were modification was studied. The inperformance of CaTiO3 : Pr3+ were optimal afterglow performance when H3BO3 is at 15% molar fraction
quote
| GB/T 7714-2015 | [1] QI Xiao-xia, WANG Zhi-ming. Influence of H_3BO_3 Content on the Luminescent Performance of CaTiO_3∶Pr3+[J]. Rare Metals and Cemented Carbides, 2010(1): 16-17. |
| MLA | [1] QI Xiao-xia, and WANG Zhi-ming. "Influence of H_3BO_3 Content on the Luminescent Performance of CaTiO_3∶Pr3+." Rare Metals and Cemented Carbides, no. 1, 2010, pp. 16-17. |
| APA | [1] QI Xiao-xia, & WANG Zhi-ming. (2010). Influence of H_3BO_3 Content on the Luminescent Performance of CaTiO_3∶Pr3+. Rare Metals and Cemented Carbides(1), 16-17. |
| IEEE | [1] QI Xiao-xia and WANG Zhi-ming, "Influence of H_3BO_3 Content on the Luminescent Performance of CaTiO_3∶Pr3+," Rare Metals and Cemented Carbides, no. 1, pp. 16-17, 2010. keywords: {red long- lasting phosphor;CaTiO3:Pr3+;H3BO3 content;hightemperature solid - phase method} |