Size and Surface Chemistry Effects on the Synaptic Behavior of Halide Perovskite Thin Films Size and Surface Chemistry Effects on the Synaptic Behavior of Halide Perovskite Thin Films AITranslate

Shenzhen Campus of Sun Yat-sen University; Shenzhen Campus of Sun Yat-sen University; Shenzhen Campus of Sun Yat-sen University; Shenzhen Campus of Sun Yat-sen University; Shenzhen Campus of Sun Yat-sen University; Shenzhen Campus of Sun Yat-sen University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Halide perovskites are promising for energy-efficient and reconfigurable artificial synapses due to the unique charge transport characteristic, i.e., ionic-electronic coupling. This work attempts to detangle the size and surface chemistry effects on perovskite-based synaptic memristors that remain elusive to date. Herein, three different perovskite-based memristors were constructed for mimicking the synaptic behavior: device 1 based on CsPbBr3-nanocrystal (NC) film terminated with short alky ligands, device 2 based on naked CsPbBr3-NC film, and device 3 based on CsPbBr3 bulk film. In addition to emulating a series of essential synaptic functions, our results suggest that perovskite-NC films outperform their bulk counterpart in light of paired pulse facilitation (PPF) index and gain due to an increased trap density and enhanced ion transport. The incorporation of short alkyl ligands into the NC surface decreases the film conductance without suppression of charge transport, thereby reducing the on-state energy consumption. Using the best-performed NC device comprising a neuron network, we did a preliminary proof-of-concept demonstration of the potential for brain-inspired neuromorphic computing which was proved effective for digit recognition with a high accuracy of 94%. Our study signifies the importance of grain size and surface chemistry engineering for the development of high-performance robust synaptic memristors based on halide perovskites.

KeyWords AITranslate

halide perovskites grain size surface chemistry artificial synapse spiking neuro network
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01498

Chinese Library Classification Number:

Citation Information:

Halide perovskites are promising for energy-efficient and reconfigurable artificial synapses due to the unique charge transport characteristic, i.e., ionic-electronic coupling. This work attempts to detangle the size and surface chemistry effects on perovskite-based synaptic memristors that remain elusive to date. Herein, three different perovskite-based memristors were constructed for mimicking the synaptic behavior: device 1 based on CsPbBr3-nanocrystal (NC) film terminated with short alky ligands, device 2 based on naked CsPbBr3-NC film, and device 3 based on CsPbBr3 bulk film. In addition to emulating a series of essential synaptic functions, our results suggest that perovskite-NC films outperform their bulk counterpart in light of paired pulse facilitation (PPF) index and gain due to an increased trap density and enhanced ion transport. The incorporation of short alkyl ligands into the NC surface decreases the film conductance without suppression of charge transport, thereby reducing the on-state energy consumption. Using the best-performed NC device comprising a neuron network, we did a preliminary proof-of-concept demonstration of the potential for brain-inspired neuromorphic computing which was proved effective for digit recognition with a high accuracy of 94%. Our study signifies the importance of grain size and surface chemistry engineering for the development of high-performance robust synaptic memristors based on halide perovskites.

quote

GB/T 7714-2015 [1] Shuyao Han, Lue Zhou, Junli Huang, et al. ACS Applied Electronic Materials, 2024(6). DOI:10.1021/acsaelm.3c01498.
MLA [1] Shuyao Han, et al., ACS Applied Electronic Materials, no. 6, 2024, https://doi.org/10.1021/acsaelm.3c01498.
APA [1] Shuyao Han, Lue Zhou, Junli Huang, Yuncheng Mu, Yuhao Xie, & Shu Zhou. (2024). ACS Applied Electronic Materials(6). https://doi.org/10.1021/acsaelm.3c01498
IEEE [1] Shuyao Han, Lue Zhou, Junli Huang, Yuncheng Mu, Yuhao Xie, and Shu Zhou, ACS Applied Electronic Materials, no. 6, 2024, doi: 10.1021/acsaelm.3c01498. keywords: {halide perovskites grain size surface chemistry artificial synapse spiking neuro network}