Study of Particle Size Testing of Superfine WC Powder AITranslate

School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Methods of SEM,TEM,laser particle analyzer,X-ray diffraction and specific surface area are applied to test the particle size of self-made superfine WC powder. Discussion is made on the effect of the testing principle and particle shape on the testing accuracy of the particle size. Through analysis of the test results,study and comparison is made of superiority and limitation of several superfine particle characterization.

KeyWords AITranslate

WC superfine powder particle size testing

1Leclercq L,et al.Catalytic properties of transition metal carbides[J].Journal of Catalysis,1989,117:371.

2Garg D,et al.Tungsten carbide erosion resistant coating for aerospace components[C].San Diego:Materials Research Society,Fall Meeting,1989.

3夏阳华,熊惟皓,丰平.粉末粒度测试方法述评[J].硬质合金,2003,20(1):29-31. 被引量:7

4郭永彩,高潮,胡学东,谢利利.微细颗粒粒度分析方法与测试技术[J].重庆大学学报:自然科学版,2000,23(5):100-103. 被引量:18

5程鹏,高抒,李徐生.激光粒度仪测试结果及其与沉降法、筛析法的比较[J].沉积学报,2001,19(3):449-455. 被引量:128

6贺安之,卞保民.微粒光散射理论与测试技术研究[J].激光杂志,2000,21(3):47-49. 被引量:15

7赵春芳.不同方法测试粒度分布的比较研究[J].中国粉体技术,2004,10(2):22-24. 被引量:20

8韩喜江,张慧姣,徐崇泉,周德瑞,谢晓美.超微颗粒尺寸测量方法比较研究[J].哈尔滨工业大学学报,2004,36(10):1331-1334. 被引量:8

1杨守达,张寿德,陈先强.WC/Co复合粉制备超细晶挤压圆棒工艺之研究[J].中国钨业,2013,28(6):42-44. 被引量:2

1刘少存,吴鹏,童森,游天亨,曾广标.纳米WC-6%Co复合粉的放电等离子烧结研究[J].硬质合金,2017,34(6):413-418. 被引量:1

2朱二涛,张久兴,羊建高.喷雾转化法制备WC-Co复合粉末制备硬质合金的研究进展[J].稀有金属与硬质合金,2019,47(3):70-78. 被引量:2

1钟建华,刘艳霞,焦锡岩,袁志燕.一种多元镍基合金球磨工艺的研究[J].铸造技术,2015,36(5):1235-1237.

2钱根华.Si_3N_4超细粉末粒度测试方法的研究[J].机械工程材料,1992,16(1):23-26.

3王柱,魏明坤,毛京元,张跃.超细碳化钨钴复合粉末的合成[J].硬质合金,1996,13(1):20-22. 被引量:7

4刘维平.光透法测定粉末颗粒粒度[J].陶瓷工程,1997,31(6):42-44. 被引量:1

5夏阳华,熊惟皓,丰平.粉末粒度测试方法述评[J].硬质合金,2003,20(1):29-31. 被引量:7

6都有为.超细微粒的特性与应用[J].仪表材料,1990,21(4):212-216. 被引量:9

7袁玉燕,白华萍,李凤生.激光光散射法的原理及其在超细粉体粒度测试中的应用[J].兵器材料科学与工程,2001,24(5):59-62. 被引量:20

8张秀英,胡志国,赵春霞.离子交换树脂法制备氢氧化镍和氧化镍超细微粒[J].功能材料,2000,31(1):109-110. 被引量:33

9祝成波,尹艳红.铜精矿的机械力化学效应研究[J].上海有色金属,2009,30(4):158-162. 被引量:1

10张福根.现代粉体粒度测试技术[J].流程工业,2003(2):90-90.

Basic Information:

DOI:

Chinese Library Classification Number:TF122.1[冶金工程—粉末冶金]

Citation Information:

Methods of SEM,TEM,laser particle analyzer,X-ray diffraction and specific surface area are applied to test the particle size of self-made superfine WC powder. Discussion is made on the effect of the testing principle and particle shape on the testing accuracy of the particle size. Through analysis of the test results,study and comparison is made of superiority and limitation of several superfine particle characterization.

quote

GB/T 7714-2015 [1] LIU Rui, LI Jian, YI Dan-qing, et al. Study of Particle Size Testing of Superfine WC Powder[J]. Rare Metals and Cemented Carbides, 2006(1): 55-58.
MLA [1] LIU Rui, et al., "Study of Particle Size Testing of Superfine WC Powder." Rare Metals and Cemented Carbides, no. 1, 2006, pp. 55-58.
APA [1] LIU Rui, LI Jian, YI Dan-qing, HUANG Dao-yuan, & CAI Zhi-gang. (2006). Study of Particle Size Testing of Superfine WC Powder. Rare Metals and Cemented Carbides(1), 55-58.
IEEE [1] LIU Rui, LI Jian, YI Dan-qing, HUANG Dao-yuan, and CAI Zhi-gang, "Study of Particle Size Testing of Superfine WC Powder," Rare Metals and Cemented Carbides, no. 1, pp. 55-58, 2006. keywords: {WC;superfine powder;particle size testing}