Stretchable, Self-Healing, and Remodelable Ionogel via In Situ Phase Separation as a Highly Sensitive Multimode Sensor AITranslate

Donghua University; Donghua University; Donghua University; Donghua University; Donghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

An ionogel with high mechanical performance, self-healing ability, adhesion, and remodelability is designed via a simple one-pot process. In situ phase separation occurred and enhanced the ionogel in the process of ultraviolet (UV)-induced polymerization based on the low solubility of poly(acrylic acid) (PAA) in ionic liquids. The degree of in situ phase separation can be regulated by the varying content of AA. By virtue of the admired performance, the resulting ionogel can detect not only mechanical strain or pressure signals to monitor external changes but also joint movements and even subtle changes in a person’s facial expressions with high sensitivity. In addition, it can be applied in a temperature sensor and exhibits a wide temperature detection range (0–120 °C) and a low threshold detection (0.1 °C). Therefore, the ionogels hold broad application prospects in flexible sensors, human–machine interfaces, and other fields.

KeyWords AITranslate

ionogel microphase separations selfhealing ability straintemperature sensor high sensitivity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01611

Chinese Library Classification Number:

Citation Information:

An ionogel with high mechanical performance, self-healing ability, adhesion, and remodelability is designed via a simple one-pot process. In situ phase separation occurred and enhanced the ionogel in the process of ultraviolet (UV)-induced polymerization based on the low solubility of poly(acrylic acid) (PAA) in ionic liquids. The degree of in situ phase separation can be regulated by the varying content of AA. By virtue of the admired performance, the resulting ionogel can detect not only mechanical strain or pressure signals to monitor external changes but also joint movements and even subtle changes in a person’s facial expressions with high sensitivity. In addition, it can be applied in a temperature sensor and exhibits a wide temperature detection range (0–120 °C) and a low threshold detection (0.1 °C). Therefore, the ionogels hold broad application prospects in flexible sensors, human–machine interfaces, and other fields.

quote

GB/T 7714-2015 [1] Jianfei Tie, Zhiping Mao, Linping Zhang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01611.
MLA [1] Jianfei Tie, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01611.
APA [1] Jianfei Tie, Zhiping Mao, Linping Zhang, Yi Zhong, & Hong Xu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01611
IEEE [1] Jianfei Tie, Zhiping Mao, Linping Zhang, Yi Zhong, and Hong Xu, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01611. keywords: {ionogel;microphase separations;selfhealing ability;straintemperature sensor;high sensitivity}