Effects of Cationic Species in Salts on the Electrical Conductivity of Doped PEDOT:PSS Films AITranslate
Abstract AITranslate
The electrical conductivity of poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS) films with four salts that have various cations but the same bis(trifluoromethanesulfonyl)amide (TFSI) anion was studied. We found that doping salts of small-sized cations led to better conductivity because of the improved crystalline order and p-doped level of PEDOT, as revealed by the grazing-incidence wide-angle X-ray scattering (GIWAXS) and UV–vis spectrum. This phenomenon can be rationalized with the fact that small-sized cations with stronger Coulombic interactions can lead to high doping and rearrangement of PEDOT:PSS. These findings will help to develop recipes based on the PEDOT:PSS/salt composite toward the applications for printed flexible electronics.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01084
Chinese Library Classification Number:
Citation Information:
The electrical conductivity of poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS) films with four salts that have various cations but the same bis(trifluoromethanesulfonyl)amide (TFSI) anion was studied. We found that doping salts of small-sized cations led to better conductivity because of the improved crystalline order and p-doped level of PEDOT, as revealed by the grazing-incidence wide-angle X-ray scattering (GIWAXS) and UV–vis spectrum. This phenomenon can be rationalized with the fact that small-sized cations with stronger Coulombic interactions can lead to high doping and rearrangement of PEDOT:PSS. These findings will help to develop recipes based on the PEDOT:PSS/salt composite toward the applications for printed flexible electronics.
quote
| GB/T 7714-2015 | [1] Xin Li, Zhen Liu, Zekun Zhou, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01084. |
| MLA | [1] Xin Li, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01084. |
| APA | [1] Xin Li, Zhen Liu, Zekun Zhou, Haiyang Gao, Guodong Liang, Daniel Rauber, Christopher W. M. Kay, & Peng Zhang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01084 |
| IEEE | [1] Xin Li, Zhen Liu, Zekun Zhou, Haiyang Gao, Guodong Liang, Daniel Rauber, Christopher W. M. Kay, and Peng Zhang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01084. keywords: {PEDOT:PSS;electrical conductivity;doping;structure−property relation;GIWAXS} |