Properties and Densification Behavior of High Content of SiC Particles Reinforced Al-based Composites Prepared by HPT AITranslate
Abstract AITranslate
SiCP/Al composites were prepared by high pressure torsion(HPT).Changes were analyzed of microstructure,hardness,relative density and SiC particle distribution of the composites with different SiC volume fraction.Densification mechanism was discussed of the composites during high pressure torsion formation.The results show that with the increasing SiC volume fraction,relative density of the composite continually decreases,while both hardness and uniformity of SiC distribution increase firstly and then decrease.And its hardness progressively increases along the radial direction of the sample.With SiC volume fraction increasing,the phenomenon of SiC particle breakage and reunification is more serious.
KeyWords AITranslate
1P.M. James,M. Ford,A.P. Jivkov.A Novel Particle Failure Criterion for Cleavage Fracture Modelling Allowing Measured Brittle Particle Distributions[J]. Engineering Fracture Mechanics . 2014
2Ping LI,Xiang ZHANG,Ke-min XUE,Xiao LI.Effect of equal channel angular pressing and torsion on SiC-particle distribution of SiC p –Al composites[J]. Transactions of Nonferrous Metals Society of China . 2012
3Alexander P. Zhilyaev,Terence G. Langdon.Using high-pressure torsion for metal processing: Fundamentals and applications[J]. Progress in Materials Science . 2008 (6)
4A. Contreras,C. Angeles-Chávez,O. Flores,R. Perez.Structural, morphological and interfacial characterization of Al–Mg/TiC composites[J]. Materials Characterization . 2006 (8)
5P.A. Karnezis,G. Durrant,B. Cantor.Characterization of Reinforcement Distribution in Cast Al-Alloy/SiC p Composites[J]. Materials Characterization . 1998 (2)
6I. V. Alexandrov,R. K. Islamgaliev,R. Z. Valiev,Y. T. Zhu,T. C. Lowe.Microstructures and properties of nanocomposites obtained through SPTS consolidation of powders[J]. Metallurgical and Materials Transactions A . 1998 (9)
1谢瑞,李萍,刘国凯,马俊林,薛克敏,贺鹏.不同粒径的SiC体积配比对SiC_p/Al基复合材料显微组织和拉伸性能的影响[J].粉末冶金工业,2016,26(6):24-29. 被引量:1
2薛克敏,钱陈豪,李萍,李晓.高压扭转圈数对碳化硅颗粒铝基复合材料组织和性能的影响[J].塑性工程学报,2012,19(2):92-95. 被引量:7
3李晓,李萍,薛克敏,王成,章凯.高压扭转法对SiC_p-Al基复合材料颗粒分布的影响[J].材料工程,2012,40(2):50-54. 被引量:11
4石文超,李萍,李晓,薛克敏.颗粒体积分数对高压扭转的SiCp/Al基复合材料拉伸性能影响[J].粉末冶金工业,2013,23(1):46-51. 被引量:3
5李晓,李萍,张倩倩,王成,章凯.SiCp/Al基复合材料的高压扭转试验[J].精密成形工程,2010,2(6):29-31. 被引量:1
6魏少华,樊建中,张琪,左涛,邹利华.等温锻造对SiC_p/Al复合材料颗粒分布的影响[J].宇航材料工艺,2009,39(4):52-57. 被引量:8
7孙大智,薛克敏,王成国,李萍.SiC颗粒粒径对高压扭转SiC_P/Al复合材料致密度和拉伸性能的影响[J].稀有金属与硬质合金,2016,44(2):64-67. 被引量:2
8杨国英,陈建华,任智森.颗粒增强铸造铝基复合材料的研究[J].轻合金加工技术,1998,26(5):39-42. 被引量:9
9贺鹏,薛克敏,王成国,李萍,石文超.HPT法对SiCp/Al复合材料颗粒断裂的影响[J].塑性工程学报,2015,22(2):117-120. 被引量:3
10王磊,张建云,周贤良.电子封装用SiC颗粒增强Al基复合材料制备工艺综述[J].金属材料研究,2005,31(2):32-35. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TB333[一般工业技术—材料科学与工程]
Citation Information:
SiCP/Al composites were prepared by high pressure torsion(HPT).Changes were analyzed of microstructure,hardness,relative density and SiC particle distribution of the composites with different SiC volume fraction.Densification mechanism was discussed of the composites during high pressure torsion formation.The results show that with the increasing SiC volume fraction,relative density of the composite continually decreases,while both hardness and uniformity of SiC distribution increase firstly and then decrease.And its hardness progressively increases along the radial direction of the sample.With SiC volume fraction increasing,the phenomenon of SiC particle breakage and reunification is more serious.
quote
| GB/T 7714-2015 | [1] MA Jun-lin, LI Ping, XU Jie, et al. Properties and Densification Behavior of High Content of SiC Particles Reinforced Al-based Composites Prepared by HPT[J]. Rare Metals and Cemented Carbides, 2015(5): 58-63. |
| MLA | [1] MA Jun-lin, et al., "Properties and Densification Behavior of High Content of SiC Particles Reinforced Al-based Composites Prepared by HPT." Rare Metals and Cemented Carbides, no. 5, 2015, pp. 58-63. |
| APA | [1] MA Jun-lin, LI Ping, XU Jie, TIAN Ye, & XUE Ke-min. (2015). Properties and Densification Behavior of High Content of SiC Particles Reinforced Al-based Composites Prepared by HPT. Rare Metals and Cemented Carbides(5), 58-63. |
| IEEE | [1] MA Jun-lin, LI Ping, XU Jie, TIAN Ye, and XUE Ke-min, "Properties and Densification Behavior of High Content of SiC Particles Reinforced Al-based Composites Prepared by HPT," Rare Metals and Cemented Carbides, no. 5, pp. 58-63, 2015. keywords: {SiCP/Al composite;high pressure torsion;SiC volume fraction;hardness;SiC particle distribution;densification} |