Recent Progress of Very Low Thermal Expansion Coefficient Materials AITranslate
Abstract AITranslate
The paper summarized the negative thermal expansion coefficient compounds and their contraction mechanism reported in recent 20 years. The focal point is on the recent progress of the very low thermal expansion coefficient materials and isotropic heat contraction compounds as well as the contraction model which was described to be the coupled rotation of the essentially rigid polyhedral bullding blocks of the structure.
KeyWords AITranslate
1张文朴.我国含钼新材料研究进展评述[J].中国钼业,2004,28(4):9-12. 被引量:2
2韩海滨,张可成,李金平.ZrW_2O_8负膨胀陶瓷材料进展[J].硅酸盐通报,2005,24(1):85-88. 被引量:7
3饶敏,董学畅,杨春梅,胡秋芬,杨光宇.2-(2-喹啉偶氮)-1,3-二羟基苯分光光度法测定钒的研究[J].化学试剂,2005,27(1):35-36. 被引量:6
4李明,艾华林,李海涛,胡秋芬.2-(2-喹啉偶氮)-4-甲基-1,3-二羟基苯分光光度法测定钒[J].光谱实验室,2005,22(1):145-147. 被引量:6
5佟林松,樊建中,肖伯律.低热膨胀铝基复合材料的研究进展[J].稀有金属,2008,32(3):375-380. 被引量:23
6殷海荣,吕承珍,李慧,林社宝.先进负热膨胀材料的最新研究进展[J].中国陶瓷,2008,44(9):14-17. 被引量:9
7刁志聪,林伟林.负热膨胀材料的研究现状及展望[J].中国钨业,2010,25(2):38-42. 被引量:3
8赵帅,赵萍.固溶体在无机非金属材料中的应用[J].山东轻工业学院学报:自然科学版,2012,26(4):80-82. 被引量:1
9王献立,付林杰,许坤.负热膨胀材料的研究及应用[J].信息记录材料,2018,19(12):38-39. 被引量:2
10武丽华,王雅婷,冯建业,曾雄伟,王天栋.晶化温度对锂铝硅微晶玻璃热膨胀系数和热稳定性的影响[J].玻璃,2015,42(12):23-26. 被引量:2
1林盼盼,于凯凯,林铁松,何鹏,刘守相,徐李刚,龙伟民,鲍丽,马佳.锂霞石复合玻璃钎料连接碳化硅陶瓷接头的应力缓释机理[J].硅酸盐学报,2020,0(3):408-415. 被引量:3
2严学华,程晓农,张美芬.溶胶-凝胶法合成亚微米α-ZrW_2O_8的研究[J].材料工程,2006,34(z1):47-49. 被引量:1
3刘红飞,程晓农,张志萍,付廷波.工艺参数和热处理温度对ZrW_2O_8薄膜制备的影响[J].真空科学与技术学报,2008,28(S1):42-46. 被引量:2
4程晓农,孙秀娟,杨娟,徐桂芳.固相法合成负热膨胀性粉体ZrW_2O_8[J].江苏大学学报:自然科学版,2005,26(4):350-353. 被引量:30
5张文朴.落实科学发展观 再造中国钼业辉煌[J].中国钼业,2005,29(5):11-14.
6朱秀芳,曹秋娥.2005年云南冶金分析年评[J].云南冶金,2006,35(2):65-74. 被引量:3
7邱杰,严学华,程晓农,王春生.先进近零膨胀陶瓷研究进展[J].材料导报,2006,20(7):31-34. 被引量:6
8赵丽杰,赵丽萍,王建雅.改进催化光度法测定水中的微量钒[J].化工环保,2006,26(5):436-439. 被引量:4
9马冲先,吴诚.金属材料分析[J].分析试验室,2006,25(12):103-122. 被引量:8
10严学华,程晓农,肖兆娟,徐桂芳.ZrW_2O_8薄膜的物相转变与负热膨胀系数[J].江苏大学学报:自然科学版,2007,28(2):135-137. 被引量:2
1云大钦,谷臣清,王晓芳.负热膨胀材料ZrV_2O_7与金属Al的复合行为及特性[J].复合材料学报,2005,22(5):25-30. 被引量:5
2郭靖远.低热膨胀系数主晶相抗热震陶瓷[J].工业技术与职业教育,1990,0(4):45-47.
3王志鹏,宋文博,赵艳,蒋毅坚,梁二军.A_2(MoO_4)_3(A=Al,Cr,Fe)结构与相变的Raman光谱研究(英文)[J].光散射学报,2011,23(3):250-256. 被引量:5
4陈骏,邓金侠,于然波,孙策,胡澎浩,邢献然.热收缩化合物——负热膨胀性及成因[J].物理,2010,39(10):691-698. 被引量:2
5佟林松,樊建中,肖伯律.低热膨胀铝基复合材料的研究进展[J].稀有金属,2008,32(3):375-380. 被引量:23
6LIND Cora.可控热膨胀聚合物复合材料的挑战和机遇(英文)[J].硅酸盐学报,2009,37(5):689-695. 被引量:1
7张志萍,刘红飞,程晓农.化学共沉淀法合成低热膨胀ZrW_2O_8/ZrO_2复合材料[J].复合材料学报,2008,25(4):137-142. 被引量:2
8李刚,孙跃,费维栋.Fe_3O_4颗粒对硼酸铝晶须增强铝复合材料热膨胀行为的影响[J].金属学报,2006,42(1):83-86. 被引量:2
9杜学丽,田华,郭瑞松,陈玉如.新型负膨胀系数材料ZrW_2 O_8的合成与特性[J].天津理工学院学报,2002,18(3):64-66. 被引量:3
10刘红飞,张志萍,程晓农.脉冲激光沉积ZrW_2O_8/ZrO_2复合薄膜及其靶材制备[J].真空科学与技术学报,2009,29(6):686-689. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TB39[一般工业技术—材料科学与工程]
Citation Information:
The paper summarized the negative thermal expansion coefficient compounds and their contraction mechanism reported in recent 20 years. The focal point is on the recent progress of the very low thermal expansion coefficient materials and isotropic heat contraction compounds as well as the contraction model which was described to be the coupled rotation of the essentially rigid polyhedral bullding blocks of the structure.
quote
| GB/T 7714-2015 | [1] ZHAO Xin-hua, ZHANG Shan-ying. Recent Progress of Very Low Thermal Expansion Coefficient Materials[J]. Rare Metals and Cemented Carbides, 1998(3): 31-37. |
| MLA | [1] ZHAO Xin-hua, and ZHANG Shan-ying. "Recent Progress of Very Low Thermal Expansion Coefficient Materials." Rare Metals and Cemented Carbides, no. 3, 1998, pp. 31-37. |
| APA | [1] ZHAO Xin-hua, & ZHANG Shan-ying. (1998). Recent Progress of Very Low Thermal Expansion Coefficient Materials. Rare Metals and Cemented Carbides(3), 31-37. |
| IEEE | [1] ZHAO Xin-hua and ZHANG Shan-ying, "Recent Progress of Very Low Thermal Expansion Coefficient Materials," Rare Metals and Cemented Carbides, no. 3, pp. 31-37, 1998. keywords: {negative thermal expansion compounds;thermal contraction compounds;ZrV_2O_7;ZrW_2O_8.} |