Organic-Transistor-Based NO2 Sensor Fabricated with Surface-Modified Faujasite-Type Zeolite as an Efficient Nanochannel for Gas Analytes Organic-Transistor-Based NO2 Sensor Fabricated with Surface-Modified Faujasite-Type Zeolite as an Efficient Nanochannel for Gas Analytes AITranslate

Incheon National University; Incheon National University; Incheon National University; Incheon National University; Sungkyunkwan University (SKKU); Incheon National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Recently, organic-transistor-based chemical gas sensors have attracted great interest; however, the properties of the sensor devices, such as their responsivity, response/recovery rates, and linearity, have not yet been fully developed to enable their practical and robust application. The poor device properties are, in principle, caused by the device configuration, which includes a thick and continuous active layer. In this study, we investigated the material properties of a multiscale porous faujasite-type framework, zeolite Y (FAU), which has been widely explored in industrial processes, and examined its potential as an analyte channel material inserted at an organic transistor active layer. A series of FAU powders were prepared via surface modification with organosilanes with different alkyl chain lengths, and the modified powders were subsequently compared. The microstructures, morphologies, and optical/electrical characteristics of polythiophene/surface-modified FAU hybrid films were systematically investigated. Organic-transistor-type nitrogen dioxide sensors based on the polythiophene/FAU hybrid films showed substantially improved sensing properties, including enhancements of their responsivity, response rate, and recovery rate. Moreover, the surface modification of the zeolite improved the sensor performance, possibly because of the optimized structural and surface characteristics of zeolitic cavity structures. These results provide invaluable information and keen insights into the design of transistor-type reactive gas sensors based on organic semiconductor/zeolite hybrid thin films.

KeyWords AITranslate

NO2 gas sensors inorganic−organic hybrid P3HT faujasite zeolite Y
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00650

Chinese Library Classification Number:

Citation Information:

Recently, organic-transistor-based chemical gas sensors have attracted great interest; however, the properties of the sensor devices, such as their responsivity, response/recovery rates, and linearity, have not yet been fully developed to enable their practical and robust application. The poor device properties are, in principle, caused by the device configuration, which includes a thick and continuous active layer. In this study, we investigated the material properties of a multiscale porous faujasite-type framework, zeolite Y (FAU), which has been widely explored in industrial processes, and examined its potential as an analyte channel material inserted at an organic transistor active layer. A series of FAU powders were prepared via surface modification with organosilanes with different alkyl chain lengths, and the modified powders were subsequently compared. The microstructures, morphologies, and optical/electrical characteristics of polythiophene/surface-modified FAU hybrid films were systematically investigated. Organic-transistor-type nitrogen dioxide sensors based on the polythiophene/FAU hybrid films showed substantially improved sensing properties, including enhancements of their responsivity, response rate, and recovery rate. Moreover, the surface modification of the zeolite improved the sensor performance, possibly because of the optimized structural and surface characteristics of zeolitic cavity structures. These results provide invaluable information and keen insights into the design of transistor-type reactive gas sensors based on organic semiconductor/zeolite hybrid thin films.

quote

GB/T 7714-2015 [1] Jun Hwa Park, Sungjoon Kweon, Duho Jang, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00650.
MLA [1] Jun Hwa Park, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00650.
APA [1] Jun Hwa Park, Sungjoon Kweon, Duho Jang, Min Bum Park, Boseok Kang, & Yeong Don Park. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00650
IEEE [1] Jun Hwa Park, Sungjoon Kweon, Duho Jang, Min Bum Park, Boseok Kang, and Yeong Don Park, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00650. keywords: {NO2 gas sensors inorganic−organic hybrid P3HT faujasite zeolite Y}