daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Oriented Conjugated Copolymer Films with Controlled Crystal Forms and Molecular Stacking Modes for Enhanced Charge Transport and Photoresponsivity AITranslate

Beijing University of Chemical Technology; Qingdao University of Science & Technology; Beijing University of Chemical Technology; China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Qingdao University of Science & Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Most of conjugated copolymers are semicrystalline. The crystal modification and crystalline morphology have an obvious effect on their charge transport. Therefore, controlling the crystal structures of conjugated copolymers is necessary for optimizing charge transport. Herein, large-area oriented poly[2,6-(4,4-bis-(2-ethylhexyl)-4H-cyclopenta[2,1-b;3,4-b′]dithiophene)-alt-4,7(2,1,3-benzothiadiazole)] (PCPDTBT) crystalline films are produced by the epitaxial crystallization on oriented polyethylene (PE) substrates based on perfect two-dimensional lattice matching. Furthermore, the stacking modes of PCPDTBT crystals has been successfully controlled by epitaxy combined with chlorobenzene (CB) annealing or addition of 1,8-diiodooctane (DIO). PCPDTBT films spin-coated from CB solution on a PE substrate exist in both edge-on and face-on molecular chain orientations. The amount of edge-on stacking in CB-annealed PCPDTBT/PE films is much higher than that in the DIO-processed films. Moreover, the oriented PCPDTBT films exposed to CB vapor are confirmed to adopt the dimer crystal form. The addition of DIO can significantly improve the orientation extent of PCPDTBT main chains with a π-stacked form. The highly oriented films with a π-stacked form demonstrate excellent carrier mobility (2.1 × 10–2 cm2 V–1 s–1) measured along the direction of PCPDTBT chains. The carrier mobility of DIO-processed PCPDTBT films along molecular chains is 76 times higher than that measured in the perpendicular direction of molecular chains. As a result, the ratio of anisotropic photoresponsivity of DIO-processed oriented PCPDTBT films can reach to 100. This work demonstrates a facile method to fabricate large-area and highly oriented PCPDTBT crystalline films with controlled crystal forms, which have potential applications in phototransistors.

KeyWords AITranslate

conjugated copolymer epitaxial crystallization largearea oriented film molecular stacking model carrier mobility Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00144

Chinese Library Classification Number:

Citation Information:

Most of conjugated copolymers are semicrystalline. The crystal modification and crystalline morphology have an obvious effect on their charge transport. Therefore, controlling the crystal structures of conjugated copolymers is necessary for optimizing charge transport. Herein, large-area oriented poly[2,6-(4,4-bis-(2-ethylhexyl)-4H-cyclopenta[2,1-b;3,4-b′]dithiophene)-alt-4,7(2,1,3-benzothiadiazole)] (PCPDTBT) crystalline films are produced by the epitaxial crystallization on oriented polyethylene (PE) substrates based on perfect two-dimensional lattice matching. Furthermore, the stacking modes of PCPDTBT crystals has been successfully controlled by epitaxy combined with chlorobenzene (CB) annealing or addition of 1,8-diiodooctane (DIO). PCPDTBT films spin-coated from CB solution on a PE substrate exist in both edge-on and face-on molecular chain orientations. The amount of edge-on stacking in CB-annealed PCPDTBT/PE films is much higher than that in the DIO-processed films. Moreover, the oriented PCPDTBT films exposed to CB vapor are confirmed to adopt the dimer crystal form. The addition of DIO can significantly improve the orientation extent of PCPDTBT main chains with a π-stacked form. The highly oriented films with a π-stacked form demonstrate excellent carrier mobility (2.1 × 10–2 cm2 V–1 s–1) measured along the direction of PCPDTBT chains. The carrier mobility of DIO-processed PCPDTBT films along molecular chains is 76 times higher than that measured in the perpendicular direction of molecular chains. As a result, the ratio of anisotropic photoresponsivity of DIO-processed oriented PCPDTBT films can reach to 100. This work demonstrates a facile method to fabricate large-area and highly oriented PCPDTBT crystalline films with controlled crystal forms, which have potential applications in phototransistors.

quote

GB/T 7714-2015 [1] Junjie Wang, Yuchao Liu, Lei Hua, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00144.
MLA [1] Junjie Wang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00144.
APA [1] Junjie Wang, Yuchao Liu, Lei Hua, Tianyu Wang, Huanli Dong, Huihui Li, Xiaoli Sun, Zhongjie Ren, & Shouke Yan. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00144
IEEE [1] Junjie Wang, Yuchao Liu, Lei Hua, Tianyu Wang, Huanli Dong, Huihui Li, Xiaoli Sun, Zhongjie Ren, and Shouke Yan, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00144. keywords: {conjugated copolymer;epitaxial crystallization;largearea oriented film;molecular stacking model;carrier mobility;Show More}