Preparation of High-performance Lithium-rich Manganese-based Cathode Materials by Electrospinning AITranslate

School of Metallurgical and Ecological Engineering,Univerity of Science and Technology Beijing;School of Metallurgical and Ecological Engineering,Univerity of Science and Technology Beijing;School of Metallurgical and Ecological Engineering,Univerity of Science and Technology Beijing;School of Metallurgical and Ecological Engineering,Univerity of Science and Technology Beijing
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The lithium-rich manganese-based cathode material of Li1.2[Mn0.54Ni0.13Co0.13]O2 was prepared by electrospinning in order to overcome the shortcomings of low first-cycle efficiency and poor rate performance of lithium-rich manganese-based materials.The experimental results show that the nanofibers prepared by electrospinning have three-dimensional structure and larger specific surface area,which can improve the reactivity and reduce the conduction impedance of lithium ions,thus improving the rate performance and discharge capacity of the materials.At 5 C rate,the discharge specific capacity of the spinning fibers is 175 mA·h/g,while that of the precipitated particles is only 154 mA·h/g.In addition,the first-cycle efficiency is improved from 72.87% to 81.93%,and discharge capacity is also improved.Thus Li-rich manganese-based materials prepared by electrospinning have better performance.

KeyWords AITranslate

Li-rich manganese-based cathode material electrospinning nanofiber coprecipitation three-dimensional structure

1罗标,张永新,肖启振,李朝晖,雷钢铁.静电纺丝技术在锂离子电池正极材料中的应用与展望[J].功能材料,2016,47(12):12064-12070. 被引量:2

1张雨薇,刘成龙,徐志江.新能源汽车锂电池富锂锰基正极材料掺杂改性[J].电源技术,2019,43(10):1596-1600. 被引量:4

2马调调.PLLA/PCL共混纤维的力学性能研究[J].橡塑技术与装备,2019,45(20):20-26.

3李子卿,邵敬爱,张俊杰,朱丹晨,杨伟栋,张世红,陈汉平.生物质基活性炭负载镍对Cr~Ⅵ的催化吸附性能研究[J].工程热物理学报,2019,40(10):2432-2439.

4刘志远,李俊鹏,朱哲.BaTiO3纳米纤维微结构和压电性能表征及其三维畴变观测[J].湘潭大学学报:自然科学版,2019,41(3):104-112. 被引量:1

5李晓茹.氯化钙/甲酸溶解体系下丝素纳米纤维膜的制备及其性能[J].纺织科学与工程学报,2019,36(4):62-67. 被引量:2

6宋维东.泡沫陶瓷的制备工艺及研究进展[J].中国粉体工业,2019,0(5):15-18. 被引量:5

7曾辉,朱仁贤,刘云鹏,郑静,周群.裸芯片堆叠组装技术研究[J].混合微电子技术,2019,30(2):28-33. 被引量:1

8陈奇慧,程凯,王俊磊,王雪芹.TiO2纳米管负载改性方法研究进展[J].化工新型材料,2019,0(9):28-31. 被引量:2

9黄雅盼,孙晓刚,李锐,梁国东,魏成成,胡浩.三(2-羧乙基)膦阻隔层对锂硫电池穿梭效应的抑制[J].高等学校化学学报,2019,40(11):2375-2381. 被引量:2

10杨林,陈勇前,王有治,罗晓锋,黄强.阻聚剂ZJ-701在过氧化物硫化体系胶料中的防焦烧作用研究[J].橡胶工业,2019,66(11):843-847. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]

Citation Information:

The lithium-rich manganese-based cathode material of Li1.2[Mn0.54Ni0.13Co0.13]O2 was prepared by electrospinning in order to overcome the shortcomings of low first-cycle efficiency and poor rate performance of lithium-rich manganese-based materials.The experimental results show that the nanofibers prepared by electrospinning have three-dimensional structure and larger specific surface area,which can improve the reactivity and reduce the conduction impedance of lithium ions,thus improving the rate performance and discharge capacity of the materials.At 5 C rate,the discharge specific capacity of the spinning fibers is 175 mA·h/g,while that of the precipitated particles is only 154 mA·h/g.In addition,the first-cycle efficiency is improved from 72.87% to 81.93%,and discharge capacity is also improved.Thus Li-rich manganese-based materials prepared by electrospinning have better performance.

quote

GB/T 7714-2015 [1] NIU Bang-bang, LI Jian-ling, LIU Yan-ying, et al. Preparation of High-performance Lithium-rich Manganese-based Cathode Materials by Electrospinning[J]. Rare Metals and Cemented Carbides, 2019(5): 55-59.
MLA [1] NIU Bang-bang, et al., "Preparation of High-performance Lithium-rich Manganese-based Cathode Materials by Electrospinning." Rare Metals and Cemented Carbides, no. 5, 2019, pp. 55-59.
APA [1] NIU Bang-bang, LI Jian-ling, LIU Yan-ying, & ZHANG Yong-jie. (2019). Preparation of High-performance Lithium-rich Manganese-based Cathode Materials by Electrospinning. Rare Metals and Cemented Carbides(5), 55-59.
IEEE [1] NIU Bang-bang, LI Jian-ling, LIU Yan-ying, and ZHANG Yong-jie, "Preparation of High-performance Lithium-rich Manganese-based Cathode Materials by Electrospinning," Rare Metals and Cemented Carbides, no. 5, pp. 55-59, 2019. keywords: {Li-rich manganese-based cathode material;electrospinning;nanofiber;coprecipitation;three-dimensional structure}