Study on Preparation and Properties of Al/Ni Dual Doped Lithium Manganate Thin Film Electrode Materials by Electrostatic Spray Deposition AITranslate

School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing;School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing;School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing;School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Al/Ni dual doped lithium manganate thin film electrode materials were prepared by electrostatic spray deposition,and XRD,SEM,cyclic voltammetry and constant current charge-discharge technique were employed to characterize phase,morphology and electrochemical performance of the materials.The results show that the electrostatic spray deposition technology can prepare doped modified lithium manganate thin film electrode materials with high crystallinity,compact morphology and excellent electrochemical performance.Al/Ni dual doping can significantly improve cycle performance and rate performance of lithium manganate materials.

KeyWords AITranslate

lithium manganate electrode material thin film electrode lithium battery electrostatic spray deposition doping modification

1邱诗铭,蔡敏,王胜杰,黄莹莹,谭义秋.二氧化锰掺铌制备锰酸锂[J].电源技术,2022,46(1):13-16.

1王储,王庆杰,张红梅,石斌.高镍三元正极材料LiNi0.8Co0.1Mn0.1O2的研究进展[J].电源技术,2019,43(12):2022-2025. 被引量:1

2于占军,段向阳,王献立,李明玉.薄膜电极材料超级电容性能综合实验设计[J].实验技术与管理,2019,36(12):57-61. 被引量:3

3梁青青,李泽雄,刘崎峰.掺杂改性NaTaO3光催化剂的研究进展[J].化工新型材料,2019,47(11):36-39. 被引量:1

4陈娜,卢威,卢春民,叶志国.纳米网状MnO2薄膜电极的制备[J].南昌航空大学学报:自然科学版,2019,33(3):68-73.

5樊静静,周正元,李燕梅,程昊.有序介孔碳修饰电极的制备及电化学检测赛庚啶[J].广西科技大学学报,2020,31(1):97-103. 被引量:2

6邓光矿,李华成,杨英全,司徒露露,黄丽萍.锰酸锂包覆试验研究[J].化学工程与技术,2019,9(6):444-455.

7彭雨佳,彭振锋,邱阳,魏云,周钰杰,周川冀越,王贵欣.膨胀石墨对锂硫电池性能的影响[J].成都大学学报:自然科学版,2019,38(4):418-422.

8蒋红星,孙俣哲,孙升,张统一.单晶锌电极在应变电荷耦合下的溶解机制-跨尺度计算与机器学习[J].上海金属,2020,42(1):104-110.

9卜晓阳,郑修,李丽.碳量子点-金纳米复合材料修饰电极测定亚硝酸盐[J].唐山师范学院学报,2019,41(6):1-5. 被引量:1

10张涛,张卫珂.不同形貌Bi2WO6/CNOs复合材料的电化学性能研究[J].人工晶体学报,2019,48(12):2265-2269.

Basic Information:

DOI:

Chinese Library Classification Number:TM912.9[电气工程—电力电子与电力传动]

Citation Information:

Al/Ni dual doped lithium manganate thin film electrode materials were prepared by electrostatic spray deposition,and XRD,SEM,cyclic voltammetry and constant current charge-discharge technique were employed to characterize phase,morphology and electrochemical performance of the materials.The results show that the electrostatic spray deposition technology can prepare doped modified lithium manganate thin film electrode materials with high crystallinity,compact morphology and excellent electrochemical performance.Al/Ni dual doping can significantly improve cycle performance and rate performance of lithium manganate materials.

quote

GB/T 7714-2015 [1] DING Xia-nan, WANG Meng, WANG Li-fan, et al. Study on Preparation and Properties of Al/Ni Dual Doped Lithium Manganate Thin Film Electrode Materials by Electrostatic Spray Deposition[J]. Rare Metals and Cemented Carbides, 2019(6): 69-73.
MLA [1] DING Xia-nan, et al., "Study on Preparation and Properties of Al/Ni Dual Doped Lithium Manganate Thin Film Electrode Materials by Electrostatic Spray Deposition." Rare Metals and Cemented Carbides, no. 6, 2019, pp. 69-73.
APA [1] DING Xia-nan, WANG Meng, WANG Li-fan, & WA NG Xin-dong. (2019). Study on Preparation and Properties of Al/Ni Dual Doped Lithium Manganate Thin Film Electrode Materials by Electrostatic Spray Deposition. Rare Metals and Cemented Carbides(6), 69-73.
IEEE [1] DING Xia-nan, WANG Meng, WANG Li-fan, and WA NG Xin-dong, "Study on Preparation and Properties of Al/Ni Dual Doped Lithium Manganate Thin Film Electrode Materials by Electrostatic Spray Deposition," Rare Metals and Cemented Carbides, no. 6, pp. 69-73, 2019. keywords: {lithium manganate;electrode material;thin film electrode;lithium battery;electrostatic spray deposition;doping modification}