In Situ Vertical Growth of Fe–Ni Layered Double-Hydroxide Arrays on Fe–Ni Alloy Foil: Interfacial Layer Enhanced Electrocatalyst with Small Overpotential for Oxygen Evolution Reaction AITranslate

Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Layer double hydroxide (LDH) has been widely applied to electrocatalysis, especially toward the oxygen evolution reaction (OER), owing to its flexible layered structure and multifunctionality. Herein, FeNi LDH nanosheet arrays are directly synthesized on various metal foils by a facile hydrothermal method. Compared with single Fe or Ni substrates, the obtained FeNi LDH/FeNi foil exhibited an ultrasmall onset overpotential of ∼90 mV, high catalytic activity (overpotential of 130 mV @ 10 mA/cm2), and durable stability in 0.1 M KOH electrolyte. We also demonstrate, by utilizing density functional theory calculations, that the growth of the hydroxide interfacial layer between LDH and FeNi foil makes the LDH possess more favorable adsorption to the OH intermediate during OER than the pure LDH. This reveals that the vertical FeNi LDH arrays on the FeNi alloy substrate are prone to be an efficient catalyst toward OER.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01466

Chinese Library Classification Number:

Citation Information:

Layer double hydroxide (LDH) has been widely applied to electrocatalysis, especially toward the oxygen evolution reaction (OER), owing to its flexible layered structure and multifunctionality. Herein, FeNi LDH nanosheet arrays are directly synthesized on various metal foils by a facile hydrothermal method. Compared with single Fe or Ni substrates, the obtained FeNi LDH/FeNi foil exhibited an ultrasmall onset overpotential of ∼90 mV, high catalytic activity (overpotential of 130 mV @ 10 mA/cm2), and durable stability in 0.1 M KOH electrolyte. We also demonstrate, by utilizing density functional theory calculations, that the growth of the hydroxide interfacial layer between LDH and FeNi foil makes the LDH possess more favorable adsorption to the OH intermediate during OER than the pure LDH. This reveals that the vertical FeNi LDH arrays on the FeNi alloy substrate are prone to be an efficient catalyst toward OER.

quote

GB/T 7714-2015 [1] Qian Xiang, Fan Li, Wenlong Chen, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01466.
MLA [1] Qian Xiang, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01466.
APA [1] Qian Xiang, Fan Li, Wenlong Chen, Yanling Ma, Yi Wu, Xin Gu, Yong Qin, Peng Tao, Chengyi Song, Wen Shang, Hong Zhu, Tao Deng, & Jianbo Wu. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01466
IEEE [1] Qian Xiang, Fan Li, Wenlong Chen, Yanling Ma, Yi Wu, Xin Gu, Yong Qin, Peng Tao, Chengyi Song, Wen Shang, Hong Zhu, Tao Deng, and Jianbo Wu, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01466.