Recyclable Biobased Dynamic Cross-Linking Epoxy Thermosets Containing Vinylogous Urethane Bonds with Shape Memory Properties AITranslate
Abstract AITranslate
A series of recyclable biobased dynamic cross-linking epoxy polymers containing vinylogous urethane bonds (ISVUEs) were constructed under solvent-free conditions by using diglycidyl ether of isosorbide and isosorbide-bis-acetoacetate derived from biobased isosorbide and cured with trifunctional and difunctional primary amines. The influence of amine curing agents and dynamic bond contents on the cross-linking density, thermal stability, and tensile and recycle properties of ISVUEs was investigated. The results showed that triamine as the cross-linker endowed a significant effect on the properties of ISVUEs. The tensile strength of the polymer with tris (2-aminoethyl) amine as the triamine reached 40.3 MPa, with only a small increase in tensile strength in three recycling cycles. The polymer with polyetheramine T403 as the triamine showed an elongation at break of 171.9% and a shape recovery of up to 84.5%, which exhibited a good shape memory effect. Meanwhile, the ISVUEs exhibit good recyclable properties when the amount of dynamic bond content is 66.7%. The design provides a strategy for introducing vinylogous urethane bonds into biobased epoxy polymers with potential smart applications such as textiles, medical implants, and soft robotics.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01879
Chinese Library Classification Number:
Citation Information:
A series of recyclable biobased dynamic cross-linking epoxy polymers containing vinylogous urethane bonds (ISVUEs) were constructed under solvent-free conditions by using diglycidyl ether of isosorbide and isosorbide-bis-acetoacetate derived from biobased isosorbide and cured with trifunctional and difunctional primary amines. The influence of amine curing agents and dynamic bond contents on the cross-linking density, thermal stability, and tensile and recycle properties of ISVUEs was investigated. The results showed that triamine as the cross-linker endowed a significant effect on the properties of ISVUEs. The tensile strength of the polymer with tris (2-aminoethyl) amine as the triamine reached 40.3 MPa, with only a small increase in tensile strength in three recycling cycles. The polymer with polyetheramine T403 as the triamine showed an elongation at break of 171.9% and a shape recovery of up to 84.5%, which exhibited a good shape memory effect. Meanwhile, the ISVUEs exhibit good recyclable properties when the amount of dynamic bond content is 66.7%. The design provides a strategy for introducing vinylogous urethane bonds into biobased epoxy polymers with potential smart applications such as textiles, medical implants, and soft robotics.
quote
| GB/T 7714-2015 | [1] Ruhan Yang, Weijie Li, Ruibin Mo, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01879. |
| MLA | [1] Ruhan Yang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01879. |
| APA | [1] Ruhan Yang, Weijie Li, Ruibin Mo, & Xinya Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01879 |
| IEEE | [1] Ruhan Yang, Weijie Li, Ruibin Mo, and Xinya Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01879. keywords: {recyclable;biobased epoxy;vinylogous urethane;shape memory;isosorbide} |