daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Multifunctional Thiol-Containing Additives for Improved Photoluminescence and Photovoltaic Performance of Cs0.15FA0.85PbI3 Perovskites Multifunctional Thiol-Containing Additives for Improved Photoluminescence and Photovoltaic Performance of Cs0.15FA0.85PbI3 Perovskites AITranslate

University of Kentucky; University of Kentucky; University of Kentucky; University of Kentucky; University of Kentucky; University of Kentucky
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thiol containing molecules as both interfacial surface ligands and additives are promising modulators for enhancing photoluminescence (PL) properties, stability, and photovoltaic (PV) performance of metal halide perovskites. However, alkanethiols are much more effective for improving photoluminescence (PL) intensity and stability in metal halide perovskite nanocrystals than in their thin film analogues. Herein, we investigate how additional functional groups on a pyrimidine core can alter thiol reactivity and influence the PL, stability, and PV performance of organic metal halide perovskites. Through an investigation of five different pyrimidine derivatives, it is shown that all derivatives containing thiol groups form thiolates in the presence of the perovskite precursors and increase the photoluminescence intensity of the perovskite film. The largest all-around improvement to the PL intensity, stability, and photovoltaic performance of Cs0.15FA0.85PbI3 perovskites is realized through the addition of a hydroxyl group combined with a trifluoromethyl group to form 4-hydroxy-6-(trifluoromethyl)pyrimidine-2-thiol. This investigation helps illuminate how combinations of functional groups can be employed to further increase the beneficial effects over monofunctional additives in organic metal halide perovskites.

KeyWords AITranslate

organic metal halide perovskite thin films passivation photoluminescence photovoltaics
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01318

Chinese Library Classification Number:

Citation Information:

Thiol containing molecules as both interfacial surface ligands and additives are promising modulators for enhancing photoluminescence (PL) properties, stability, and photovoltaic (PV) performance of metal halide perovskites. However, alkanethiols are much more effective for improving photoluminescence (PL) intensity and stability in metal halide perovskite nanocrystals than in their thin film analogues. Herein, we investigate how additional functional groups on a pyrimidine core can alter thiol reactivity and influence the PL, stability, and PV performance of organic metal halide perovskites. Through an investigation of five different pyrimidine derivatives, it is shown that all derivatives containing thiol groups form thiolates in the presence of the perovskite precursors and increase the photoluminescence intensity of the perovskite film. The largest all-around improvement to the PL intensity, stability, and photovoltaic performance of Cs0.15FA0.85PbI3 perovskites is realized through the addition of a hydroxyl group combined with a trifluoromethyl group to form 4-hydroxy-6-(trifluoromethyl)pyrimidine-2-thiol. This investigation helps illuminate how combinations of functional groups can be employed to further increase the beneficial effects over monofunctional additives in organic metal halide perovskites.

quote

GB/T 7714-2015 [1] Md Aslam Uddin, Tareq Hossain, Nadeesha L. Kothalawala, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01318.
MLA [1] Md Aslam Uddin, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01318.
APA [1] Md Aslam Uddin, Tareq Hossain, Nadeesha L. Kothalawala, Syed Joy, DooYoung Kim, & Kenneth R. Graham. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01318
IEEE [1] Md Aslam Uddin, Tareq Hossain, Nadeesha L. Kothalawala, Syed Joy, DooYoung Kim, and Kenneth R. Graham, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01318. keywords: {organic metal halide perovskite thin films passivation photoluminescence photovoltaics}