Ti–Dopamine Hybrid Nanoparticles with UV-Blocking and Durable Poly(butylene adipate-co-terephthalate) Materials AITranslate

Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University; Jiangnan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The increased demand for environmental protection and sustainable development has promoted the progress of renewable and biodegradable materials, especially in the field of packaging and agriculture. Such a status makes poly(butylene adipate-co-terephthalate) (PBAT) a kind of popular polyester material with an expanded utilization rate for its good mechanical properties and processability. However, a poor barrier property and light aging resistance are always the core issues during application. In order to overcome these shortcomings, Ti–dopamine (TiDA) nanoparticles were synthesized by hybridizing dopamine and a titanium precursor, resulting in a mixed phase of rutile and brookite, which was highly beneficial to light resistance. When TiDA was blended with PBAT at a low concentration (0.5–2.0 wt %), the PBAT composite films showed a great comprehensive performance. While maintaining good mechanical properties (tensile strength over 30 MPa and strain over 800%), the water vapor permeability was reduced by nearly 40%. The UV light of all wave bands could be blocked mostly by PBAT/TD composite films, which also had enhanced aging resistance, retaining over 20 MPa tensile strength and almost 100% strain after aging with UV radiation for 100 h. In summary, the PBAT/TD film material was promising for potential production in the field of agriculture and packaging.

KeyWords AITranslate

titanium dopamine hybrid nanoparticles UVblocking and aging resistant poly(butylene adipatecoterephthalate)
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01714

Chinese Library Classification Number:

Citation Information:

The increased demand for environmental protection and sustainable development has promoted the progress of renewable and biodegradable materials, especially in the field of packaging and agriculture. Such a status makes poly(butylene adipate-co-terephthalate) (PBAT) a kind of popular polyester material with an expanded utilization rate for its good mechanical properties and processability. However, a poor barrier property and light aging resistance are always the core issues during application. In order to overcome these shortcomings, Ti–dopamine (TiDA) nanoparticles were synthesized by hybridizing dopamine and a titanium precursor, resulting in a mixed phase of rutile and brookite, which was highly beneficial to light resistance. When TiDA was blended with PBAT at a low concentration (0.5–2.0 wt %), the PBAT composite films showed a great comprehensive performance. While maintaining good mechanical properties (tensile strength over 30 MPa and strain over 800%), the water vapor permeability was reduced by nearly 40%. The UV light of all wave bands could be blocked mostly by PBAT/TD composite films, which also had enhanced aging resistance, retaining over 20 MPa tensile strength and almost 100% strain after aging with UV radiation for 100 h. In summary, the PBAT/TD film material was promising for potential production in the field of agriculture and packaging.

quote

GB/T 7714-2015 [1] Zheng Zhang, Ting Li, Xuhui Zhang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01714.
MLA [1] Zheng Zhang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01714.
APA [1] Zheng Zhang, Ting Li, Xuhui Zhang, Jing Huang, Bihua Xia, Jie Jiang, Mingqing Chen, Weifu Dong, & Yang Wang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01714
IEEE [1] Zheng Zhang, Ting Li, Xuhui Zhang, Jing Huang, Bihua Xia, Jie Jiang, Mingqing Chen, Weifu Dong, and Yang Wang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01714. keywords: {titanium;dopamine;hybrid nanoparticles;UVblocking and aging resistant;poly(butylene adipatecoterephthalate)}