Intrinsically Microporous Polyimides from Norbornyl Bis-benzocyclobutene-Containing Diamines and Rigid Dianhydrides for Membrane-Based Gas Separation AITranslate

Zhejiang University of Technology;Ningbo Institute of Material Technology and Engineering; Ningbo University; Zhejiang University of Technology;Ningbo Institute of Material Technology and Engineering;Ningbo Institute of Material Technology and Engineering
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A series of polyimides of intrinsic microporosity (PIM-PIs) were prepared from commercially available rigid dianhydrides (pyromellitic dianhydride (PMDA), cyclo-[2.2.2]oct-7-ene-2-exo,3-exo,5-exo,6-exo-2,3:5,6-dianhydride (BTA), and 1,2,3,4-cyclobutanetetracarboxylic dianhydride (CBDA)) and diamines with norbornyl bis-benzocyclobutene (N2BC) segments (CANAL-2, CANAL-3, and CANAL-4). The physical and gas transport properties of these polymers were systematically investigated. The fractional free volumes (FFV), interchain distances, surface areas, and cumulative micropore volumes of these PIM-PIs were in the range of 0.156–0.185, 0.593–0.619 nm, 422–615 m2 g–1, and 0.059–0.072 cm3 g–1, respectively, showing a general trend of BTA > PMDA > CBDA for certain diamines. Thus, BTA-CANAL-2 concomitantly exhibited higher gas permeability and perm-selectivity relative to its analogues, viz., PMDA-CANAL-2, CBDA-CANAL-2, and 6FDA-CANAL-2 (6FDA: 4,4′-(hexafluoroisopropylidene)diphthalic anhydride). Specifically, it showed H2 permeability of 1685 barrer, H2/CH4 selectivity of 14, and H2/N2 selectivity of 15, which surpassed the 2008 Robeson’s upper bounds. The W-shaped, cage-like architecture of BTA residues imparted the resulting PIM-PIs with both high FFV and high cumulative micropore volumes, which was the reason for their excellent gas separation performance.

KeyWords AITranslate

PIMPI rigid dianhydride CANAL diamine microstructure gas separation performance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01923

Chinese Library Classification Number:

Citation Information:

A series of polyimides of intrinsic microporosity (PIM-PIs) were prepared from commercially available rigid dianhydrides (pyromellitic dianhydride (PMDA), cyclo-[2.2.2]oct-7-ene-2-exo,3-exo,5-exo,6-exo-2,3:5,6-dianhydride (BTA), and 1,2,3,4-cyclobutanetetracarboxylic dianhydride (CBDA)) and diamines with norbornyl bis-benzocyclobutene (N2BC) segments (CANAL-2, CANAL-3, and CANAL-4). The physical and gas transport properties of these polymers were systematically investigated. The fractional free volumes (FFV), interchain distances, surface areas, and cumulative micropore volumes of these PIM-PIs were in the range of 0.156–0.185, 0.593–0.619 nm, 422–615 m2 g–1, and 0.059–0.072 cm3 g–1, respectively, showing a general trend of BTA > PMDA > CBDA for certain diamines. Thus, BTA-CANAL-2 concomitantly exhibited higher gas permeability and perm-selectivity relative to its analogues, viz., PMDA-CANAL-2, CBDA-CANAL-2, and 6FDA-CANAL-2 (6FDA: 4,4′-(hexafluoroisopropylidene)diphthalic anhydride). Specifically, it showed H2 permeability of 1685 barrer, H2/CH4 selectivity of 14, and H2/N2 selectivity of 15, which surpassed the 2008 Robeson’s upper bounds. The W-shaped, cage-like architecture of BTA residues imparted the resulting PIM-PIs with both high FFV and high cumulative micropore volumes, which was the reason for their excellent gas separation performance.

quote

GB/T 7714-2015 [1] Pu Yuan, Mengru Zhang, Yuanyuan Pang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01923.
MLA [1] Pu Yuan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01923.
APA [1] Pu Yuan, Mengru Zhang, Yuanyuan Pang, Aimin Chen, Zhen Wang, & Jingling Yan. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01923
IEEE [1] Pu Yuan, Mengru Zhang, Yuanyuan Pang, Aimin Chen, Zhen Wang, and Jingling Yan, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01923. keywords: {PIMPI;rigid dianhydride;CANAL diamine;microstructure;gas separation performance}