Rare-earth-free, environmentally benign liquid luminogen are scarce. Herein, we report for the first time a deep eutectic solvent as a blue-emitting liquid luminogen with a quantum yield of ∼23%. DFT calculations deciphered the origin of blue emission. Its potential as a liquid scintillator was further demonstrated with γ-emitting radioactive sources.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00153
Chinese Library Classification Number:
Citation Information:
Rare-earth-free, environmentally benign liquid luminogen are scarce. Herein, we report for the first time a deep eutectic solvent as a blue-emitting liquid luminogen with a quantum yield of ∼23%. DFT calculations deciphered the origin of blue emission. Its potential as a liquid scintillator was further demonstrated with γ-emitting radioactive sources.
quote
| GB/T 7714-2015 | [1] Sushil M. Patil, Santosh K. Gupta, Dibakar Goswami, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00153. |
| MLA | [1] Sushil M. Patil, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00153. |
| APA | [1] Sushil M. Patil, Santosh K. Gupta, Dibakar Goswami, Ayan Ghosh, Mohit Tyagi, Bhaskar B. Dhotare, Tapan K. Ghanty, & Ruma Gupta. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00153 |
| IEEE | [1] Sushil M. Patil, Santosh K. Gupta, Dibakar Goswami, Ayan Ghosh, Mohit Tyagi, Bhaskar B. Dhotare, Tapan K. Ghanty, and Ruma Gupta, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00153. keywords: {DES hydrophobic blue emission photoluminescence DFT liquid scintillator} |