daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of SiO2 Particles on the Crystallization and Formation of Hydrogen Bonding in Biobased Polyamide 56 AITranslate

East China University of Science and Technology; East China University of Science and Technology; East China University of Science and Technology; East China University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

As PA56 cannot have 100% intermolecular hydrogen bonds (HBs) regardless of how the molecular chains are arranged, the crystallization properties of PA56 are not as good as those of petroleum-based nylon. To replace petroleum-based nylon and broaden the applications, it is necessary to improve the crystallization properties of PA56 and elaborate the relationship between crystallization and hydrogen bonding. In this work, nano-SiO2 with different particle sizes was chosen as the nucleation agent of biobased PA56, and the isothermal and nonisothermal crystallization of PA56 were investigated by differential scanning calorimetry (DSC). It was shown that SiO2 can significantly improve the crystallization properties of PA56 composites, especially for SiO2 with a smaller size. Furthermore, the influence of SiO2 on the formation of hydrogen bonds during the crystallization process was also studied by in situ Fourier transform infrared (FTIR) spectroscopy. The addition of SiO2 into PA56 plays a role in the increase of the conversion of the free carbonyl group to the hydrogen-bonded carbonyl group, which accelerates the formation of intermolecular HBs. The increase of HBs may be the factor for the improvement of the crystallization rate.

KeyWords AITranslate

biobased PA56 crystallization SiO2 in situ FTIR 2DIR spectra hydrogen bonding
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00505

Chinese Library Classification Number:

Citation Information:

As PA56 cannot have 100% intermolecular hydrogen bonds (HBs) regardless of how the molecular chains are arranged, the crystallization properties of PA56 are not as good as those of petroleum-based nylon. To replace petroleum-based nylon and broaden the applications, it is necessary to improve the crystallization properties of PA56 and elaborate the relationship between crystallization and hydrogen bonding. In this work, nano-SiO2 with different particle sizes was chosen as the nucleation agent of biobased PA56, and the isothermal and nonisothermal crystallization of PA56 were investigated by differential scanning calorimetry (DSC). It was shown that SiO2 can significantly improve the crystallization properties of PA56 composites, especially for SiO2 with a smaller size. Furthermore, the influence of SiO2 on the formation of hydrogen bonds during the crystallization process was also studied by in situ Fourier transform infrared (FTIR) spectroscopy. The addition of SiO2 into PA56 plays a role in the increase of the conversion of the free carbonyl group to the hydrogen-bonded carbonyl group, which accelerates the formation of intermolecular HBs. The increase of HBs may be the factor for the improvement of the crystallization rate.

quote

GB/T 7714-2015 [1] Zijing Xun, Guocheng He, Yu Huang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00505.
MLA [1] Zijing Xun, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00505.
APA [1] Zijing Xun, Guocheng He, Yu Huang, & Ruobing Yu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00505
IEEE [1] Zijing Xun, Guocheng He, Yu Huang, and Ruobing Yu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00505. keywords: {biobased PA56;crystallization;SiO2;in situ FTIR;2DIR spectra;hydrogen bonding}