Self-Healing Chameleon Skin Functioning in the Air Environments AITranslate
Abstract AITranslate
Chameleons are famous for their uncommon ability to change skin colors rapidly by tuning the lattice distance of guanine nanocrystals within the dermal iridophores. This mechanism has inspired various artificial photonic crystal (PC) films with tunable structural colors. However, the structural colors of most reported films are facile to be destroyed by external factors such as friction, impact, or water evaporation. Herein, an artificial intelligent skin, which has an elastomer–colloidal photonic crystal–hydrogel sandwich structure, is presented in this work. The outer modified polydimethylsiloxane layer acts as the cuticle to protect the hydrogel layer from water evaporation and endows the skin with self-healing ability. The inner hydrophilic hydrogel layer embedded with the colloidal photonic crystals acts as the dermis layer, and the polystyrene colloids layer plays the role of the guanine nanocrystals. A programmed color change can be easily controlled by varying the elongation of the artificial skin, covering the full visible spectrum range. Moreover, skin with patterned stripes, which is similar to the panther chameleon skin that can manipulate multiple colors, has also been achieved. The present artificial skin will offer fresh perspectives on the preparation of artificial chameleon skin similar to the real dynamic flexible skin, which would promote the application of PCs in optical devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01529
Chinese Library Classification Number:
Citation Information:
Chameleons are famous for their uncommon ability to change skin colors rapidly by tuning the lattice distance of guanine nanocrystals within the dermal iridophores. This mechanism has inspired various artificial photonic crystal (PC) films with tunable structural colors. However, the structural colors of most reported films are facile to be destroyed by external factors such as friction, impact, or water evaporation. Herein, an artificial intelligent skin, which has an elastomer–colloidal photonic crystal–hydrogel sandwich structure, is presented in this work. The outer modified polydimethylsiloxane layer acts as the cuticle to protect the hydrogel layer from water evaporation and endows the skin with self-healing ability. The inner hydrophilic hydrogel layer embedded with the colloidal photonic crystals acts as the dermis layer, and the polystyrene colloids layer plays the role of the guanine nanocrystals. A programmed color change can be easily controlled by varying the elongation of the artificial skin, covering the full visible spectrum range. Moreover, skin with patterned stripes, which is similar to the panther chameleon skin that can manipulate multiple colors, has also been achieved. The present artificial skin will offer fresh perspectives on the preparation of artificial chameleon skin similar to the real dynamic flexible skin, which would promote the application of PCs in optical devices.
quote
| GB/T 7714-2015 | [1] Jinhui Liang, Jiahui Liu, Liqian Zhu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01529. |
| MLA | [1] Jinhui Liang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01529. |
| APA | [1] Jinhui Liang, Jiahui Liu, Liqian Zhu, Shuyuan Gao, Yuanyuan Liu, Xinyuan Teng, Run Wang, Xiaojuan Wang, Shengjie Wang, Jiqian Wang, & Yongqing Xia. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01529 |
| IEEE | [1] Jinhui Liang, Jiahui Liu, Liqian Zhu, Shuyuan Gao, Yuanyuan Liu, Xinyuan Teng, Run Wang, Xiaojuan Wang, Shengjie Wang, Jiqian Wang, and Yongqing Xia, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01529. keywords: {mechanochromic;selfhealing;camouflage;photonic crystals;elastomer−hydrogel} |