The Research and Development on Solid Electrolytic Tantalum Capacitor AITranslate

Zhuzhou Hongda Electronics Co., Ltd.;Zhuzhou Hongda Electronics Co., Ltd.;Zhuzhou Hongda Electronics Co., Ltd.;Zhuzhou Hongda Electronics Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The Paper summarized the following latest development and research on the electrolytic tantalum capacitor: ①substitute conducting polymer or superfine powder of precious metal for traditional electrolyte MnO_2;②substitute niobium for tantalum completely or partly;③adopt pint-sized chip tantalum capacitor.

KeyWords AITranslate

electrolytic tantalum capacitor conducting polymer electrolytic niobium capacitor

1宋登元.导电聚合物──新型半导体器件材料[J].半导体技术,1994,10(3):1-3. 被引量:2

2孟景溪(译).在空气和无氧条件下合成聚吡咕[J].钽铌工艺进展,1998,(3):25-25.

3屈乃琴,陈久录.国内外片式钽电容器的开发与发展[J].稀有金属与硬质合金,2000,28(3):50-52. 被引量:2

4潘伦桃(译).钽固体电解电容器[J].钽铌工业进展,2001,(2):21-21.

1熊平.导电高分子在固体钽电解电容器中的应用[J].成都电子机械高等专科学校学报,2004,7(4):1-4. 被引量:1

2夏凤金,刘培生,周茂奇.多孔钽的制备方法[J].科技创新导报,2008,5(1):83-84. 被引量:3

3甘卫平,刘继宇,刘泓,李祥,马贺然.钽电容器用钽壳内壁RuO_2薄膜电极的表征及电化学性能[J].无机材料学报,2010(8):882-886. 被引量:2

4田东斌,潘齐凤,龙道学,李美霞,王富权,陈果,曾金萍.高压大容量有机固体电解质片式钽电容器可靠性试验[J].电子元件与材料,2017,36(10):80-85. 被引量:2

5田东斌,潘齐凤,张选红,马建华,刘桥,杨邦朝.高压有机片式钽电容器高温可靠性研究[J].电子科技大学学报,2018,47(5):761-765.

6王宇,任建波,李泱,顾崟,张湃.199D系列钽电容器典型缺陷模式及检测方法研究[J].集成电路应用,2020,37(7):22-24.

1王大鹏,李琪佳,王志强.医用多孔钽的性能及其在膝关节损伤中的应用[J].中国组织工程研究与临床康复,2011,15(29):5463-5466. 被引量:6

2甘卫平,黄小清,李祥.超级电容器用(RuO_2/SiO_2)·nH_2O复合薄膜电极的研究[J].材料导报,2012,26(10):147-151. 被引量:2

3解永旭,韩鹏,马跃忠.医用钽丝生产工艺研究[J].金属制品,2013,39(6):21-23. 被引量:1

4龙萍,许立坤,崔秀芳,金国.钌镧氧化物涂层析氯反应动力学比较研究[J].无机材料学报,2015,30(5):493-499.

5杨国深,魏峰,董仕晋,刘歌,鲍建楠.水性导电涂料PEDOT/PSS的研究进展[J].染料与染色,2015,52(5):24-29. 被引量:1

6康新婷,李亚宁,李广忠,李烨.烧结温度对多孔钽性能影响[J].稀有金属材料与工程,2017,46(4):1092-1096. 被引量:7

7田东斌,龙道学,潘齐凤,张选红.高压超大容量有机电解质片式钽电容器高温稳定性试验[J].电子器件,2019,42(4):811-814.

8李福成,张学清,柳金洲,包富贵.FTW150K高比容钽粉研制钽电容器电介质膜形成工艺的研究[J].宁夏大学学报:自然科学版,2020,41(2):164-167.

1郭磊,王志法.加工方法对钽板力学性能以及织构的影响[J].稀有金属与硬质合金,2005,33(3):18-22. 被引量:6

2刘英,杨敏鸽,王俊勃,王亚亮,张力.机械合金化制备电触头材料的研究与进展[J].材料导报:纳米与新材料专辑,2008,22(1):299-302. 被引量:4

3徐红梅,严红革.机械合金化技术在功能材料中制备的应用[J].材料导报,2004,18(F10):189-191. 被引量:2

4王向东,张宝红,张治民.直齿圆柱齿轮精锻技术的发展现状与趋势[J].锻压装备与制造技术,2006,41(2):21-24. 被引量:14

5张声飞.高频固体钽电解电容器电性能与钽粉[J].电子元件与材料,1999,18(1):39-41. 被引量:3

6袁韧,张新明,周卓平.退火温度对钽丝再结晶织构的影响[J].稀有金属与硬质合金,2002,30(3):17-21. 被引量:2

7江涛,陈阳,成铭,万海荣,王园园,杨美丽.NiAl金属间化合物材料的制备技术及其研究发展趋势和应用现状[J].科技创新导报,2015,12(25):80-81. 被引量:2

8关绍康,王利国,朱世杰,王西科,沈宁福.快速凝固合金的研究发展趋势[J].现代铸铁,2004,24(4):22-26. 被引量:9

9袁韧,张新明,周卓平.钽丝的织构和再结晶行为研究[J].材料导报,2002,16(6):68-70. 被引量:2

10徐燕飞,余芬芬,谢少凡.导电聚合物在金属防腐蚀中的应用进展[J].材料保护,2016,49(1):52-55. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]

Citation Information:

The Paper summarized the following latest development and research on the electrolytic tantalum capacitor: ①substitute conducting polymer or superfine powder of precious metal for traditional electrolyte MnO_2;②substitute niobium for tantalum completely or partly;③adopt pint-sized chip tantalum capacitor.

quote

GB/T 7714-2015 [1] LIU Jian-qing, LI Jian, DAI Yan-yang, et al. The Research and Development on Solid Electrolytic Tantalum Capacitor[J]. Rare Metals and Cemented Carbides, 2002(2): 41-44.
MLA [1] LIU Jian-qing, et al., "The Research and Development on Solid Electrolytic Tantalum Capacitor." Rare Metals and Cemented Carbides, no. 2, 2002, pp. 41-44.
APA [1] LIU Jian-qing, LI Jian, DAI Yan-yang, & ZHONG Hai-yun. (2002). The Research and Development on Solid Electrolytic Tantalum Capacitor. Rare Metals and Cemented Carbides(2), 41-44.
IEEE [1] LIU Jian-qing, LI Jian, DAI Yan-yang, and ZHONG Hai-yun, "The Research and Development on Solid Electrolytic Tantalum Capacitor," Rare Metals and Cemented Carbides, no. 2, pp. 41-44, 2002. keywords: {electrolytic tantalum capacitor;conducting polymer;electrolytic niobium capacitor}