Effects of Physical Properties of Pr-Nd Oxide on its Electrolysis Preparation and Improvement Measures AITranslate
Abstract AITranslate
Physical properties of Pr-Nd oxide directly affect its electrolysis stability,current efficiency,energy consumption and other technical and economic indexes.Therefore,its physical properties must remain constant and uniform with less volatility.Through comparison of specific surface area,particle size and microstructure and combination with actual production,the effects are analyzed of physical properties of PrNd oxide on its electrolysis,and improvement measures are discussed for its physical properties to meet the requirements of electrolysis.
KeyWords AITranslate
1李旺兴,尹中林,刘战伟.浅谈氧化铝质量问题[J].轻金属,2007(11):8-12. 被引量:14
2吕鲜翠,唐海红.氧化铝质量的改善及其对铝电解的影响[J].中国有色冶金,2006,35(4):14-17. 被引量:18
3李慧琴,刘海旺,张瑞祥,许宗泽,胡珊珊,郝先库.灼烧温度对镨钕二元氧化物比表面积、密度影响的研究[J].稀土,2010,31(6):78-80. 被引量:6
4张瑞祥,李慧琴,刘海旺,许宗泽,胡珊珊,郝先库.灼烧温度对镨钕二元氧化物粒度和形貌影响的研究[J].稀土,2010,31(1):48-52. 被引量:10
5魏坤,何地宝,翟建伟.沉淀法制备稀土氧化物纳米粉体的研究[J].稀土,1999,20(4):27-30. 被引量:28
1张永华,吴锦绣,郭晓晖.降低氧化镨钕中氯根的工艺研究[J].有色金属:冶炼部分,2017(6):58-61. 被引量:3
2王洪伟,柳云龙.稀土冶炼副产品中提取铈的工艺研究[J].云南冶金,2018,47(5):42-44.
3周洁英,杨幼明.240#新型环烷酸萃取铝的研究[J].稀有金属,2021,45(1):85-92. 被引量:1
4马升峰,孟志军,李裕,许延辉,高天佐,关卫华,王荣,王永利.高浓度镨钕料液去除杂质铝的工艺研究(Ⅰ)[J].稀有金属与硬质合金,2021,49(2):9-14. 被引量:1
5孟志军,许延辉,高天佐,关卫华,李裕,马升峰.高浓度镨钕料液中杂质铝的去除工艺研究(Ⅱ)[J].稀有金属与硬质合金,2021,49(4):6-10.
1曾青云,郭守金,薛丽燕,曾繁钢,王莉.外场辅助制备低氯氧化镧前驱体[J].有色金属科学与工程,2018,9(5):7-13. 被引量:1
2马升峰,孟志军,李裕,许延辉,高天佐,关卫华,王荣,王永利.高浓度镨钕料液去除杂质铝的工艺研究(Ⅰ)[J].稀有金属与硬质合金,2021,49(2):9-14. 被引量:1
3孟志军,许延辉,高天佐,关卫华,李裕,马升峰.高浓度镨钕料液中杂质铝的去除工艺研究(Ⅱ)[J].稀有金属与硬质合金,2021,49(4):6-10.
4王强,林春雷,何秉轩,徐略渭,梁勇.NdCl_(3)-AlCl_(3)-H_(2)C_(2)O_(4)体系稀土沉淀热力学研究[J].中国稀土学报,2022,40(1):120-127. 被引量:2
5叶毅,李益民,曾纪术,周志伟,秦健春,李宽,潘务霞,江泽佐,何琦.碳酸氢钠沉淀法制备大粒度高纯度氧化镨钕研究[J].矿冶工程,2023,43(1):114-117.
1王生宁,段中波,洪亚旭.浅述氧化铝质量对铝电解过程的影响[J].酒钢科技,2015(2):18-24. 被引量:1
2韦火明,王英杰.推进标准化操作提高机烧矿强度攻关实践[J].北方钒钛,2009(3):28-31.
Basic Information:
DOI:
Chinese Library Classification Number:TF111.522[冶金工程—冶金物理化学]
Citation Information:
Physical properties of Pr-Nd oxide directly affect its electrolysis stability,current efficiency,energy consumption and other technical and economic indexes.Therefore,its physical properties must remain constant and uniform with less volatility.Through comparison of specific surface area,particle size and microstructure and combination with actual production,the effects are analyzed of physical properties of PrNd oxide on its electrolysis,and improvement measures are discussed for its physical properties to meet the requirements of electrolysis.
quote
| GB/T 7714-2015 | [1] LIU Yun-long, NIE Zhong-wen, LUO Qi-shun, et al. Effects of Physical Properties of Pr-Nd Oxide on its Electrolysis Preparation and Improvement Measures[J]. Rare Metals and Cemented Carbides, 2016(2): 50-53. |
| MLA | [1] LIU Yun-long, et al., "Effects of Physical Properties of Pr-Nd Oxide on its Electrolysis Preparation and Improvement Measures." Rare Metals and Cemented Carbides, no. 2, 2016, pp. 50-53. |
| APA | [1] LIU Yun-long, NIE Zhong-wen, LUO Qi-shun, & CHEN Yun. (2016). Effects of Physical Properties of Pr-Nd Oxide on its Electrolysis Preparation and Improvement Measures. Rare Metals and Cemented Carbides(2), 50-53. |
| IEEE | [1] LIU Yun-long, NIE Zhong-wen, LUO Qi-shun, and CHEN Yun, "Effects of Physical Properties of Pr-Nd Oxide on its Electrolysis Preparation and Improvement Measures," Rare Metals and Cemented Carbides, no. 2, pp. 50-53, 2016. keywords: {Pr-Nd oxide;physical property;electrolysis;effect;improvement measure} |