Theoretical Analysis of Initial Activation of Lithium-Lead Alloy AITranslate
Abstract AITranslate
The activation level and impurity control index were calculated and analyzed initially based on irradiation dose rate.And the aim is to provide basic data for out-pile tritium release experiment from lithium-lead alloy and for the establishment of the personnel safety operation rule and regulation to ensure the absolute safety of irradiation experiments and tritium release experiments.The results show that the dose rate of Li-Pb alloy is reduced up to the dose rate level requirement of radiochemical laboratory operation,and the impurity control level is low under 15-hours irradiation at the neutron dose rate of 1013N/(cm2·s) and 10-months cooling and storage.However,the general chemical laboratory operation requirement cannot be met even by 100-months storage.
KeyWords AITranslate
1谢波,王和义.ITER液态锂铅回路鼓泡柱中提取氚的理论计算[J].原子能科学技术,2008,42(12):1115-1119. 被引量:9
2谢波,杨通在,陈晓军.锂铅合金离线产氚实验的设计[J].稀有金属与硬质合金,2008,36(3):10-14. 被引量:1
3谢波,吴曦,翁葵平.锂铅合金中微量杂质元素的测定[J].稀有金属与硬质合金,2009,37(3):29-32. 被引量:2
4WANG Peixuan, SONG Jiashu. Helium in materials and the permeation of tritium[M]. Beijing: National Defense Industry Press, 2002.54.
5Malara C. Tritium extraction from Pb-17Li by bubble columns[J]. Fusion Technology, 1995,28 : 693.
6郁金南.材料辐照效应[M].北京:化学工业出版社,2006.118.
1谢波,翁葵平.锂铅合金中氚扩散行为的理论研究[J].分子科学学报,2009,25(5):352-356. 被引量:7
2谢波,胡睿,刘云怒.聚变-裂变混合堆液态锂铅包层中氚提取系统设计[J].科技导报,2008,26(23):23-26. 被引量:2
3汪卫华,朱志强,李晋岭,黄群英,高胜,FDS团队.液态金属回路DRAGON-Ⅱ锂铅合金流动与传热三维数值模拟[J].核科学与工程,2010,30(2):166-171. 被引量:2
4谢波,王和义,翁葵平,刘云怒,官锐,侯建平.纯Fe和316L不锈钢在液态锂铅合金中的腐蚀行为[J].核化学与放射化学,2008,30(1):23-28. 被引量:5
5谢波,吴宜灿,陈晓军,翁葵平,刘俊,肖成建,FDS团队.锂铅合金释氚实验研究[J].原子核物理评论,2011,28(3):371-376. 被引量:2
6崔安智,郭景儒,唐培家,苏树新,刘大鸣,张淑兰.放射化学中子活化分析法测定高放废液中的129Ⅰ[J].原子能科学技术,1992,26(2):48-51. 被引量:3
7谢波,杨通在.液态锂铅合金电磁泵的设计(Ⅰ)——液态锂铅合金电磁泵理想模型的建立[J].化学工程与装备,2009(8):4-7. 被引量:1
8谢波,翁葵平,侯建平,杨光玲,曾军.气-液接触法提取液态锂铅合金中的氢[J].核聚变与等离子体物理,2013,33(1):83-87. 被引量:1
9谢波,杨通在,官锐,翁葵平.旋转喷嘴鼓泡法提取液态锂铅合金中的氢[J].核聚变与等离子体物理,2010,30(2):183-188. 被引量:4
10张林,张义门,张玉明,张书霞,汤晓燕,王悦湖.4H-SiC肖特基二极管γ射线探测器的模型与分析[J].强激光与粒子束,2008,20(5):854-858. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TL627[核科学技术—核技术及应用]
Citation Information:
The activation level and impurity control index were calculated and analyzed initially based on irradiation dose rate.And the aim is to provide basic data for out-pile tritium release experiment from lithium-lead alloy and for the establishment of the personnel safety operation rule and regulation to ensure the absolute safety of irradiation experiments and tritium release experiments.The results show that the dose rate of Li-Pb alloy is reduced up to the dose rate level requirement of radiochemical laboratory operation,and the impurity control level is low under 15-hours irradiation at the neutron dose rate of 1013N/(cm2·s) and 10-months cooling and storage.However,the general chemical laboratory operation requirement cannot be met even by 100-months storage.
quote
| GB/T 7714-2015 | [1] XIE Bo, GU Mei, XIAO Cheng-jian. Theoretical Analysis of Initial Activation of Lithium-Lead Alloy[J]. Rare Metals and Cemented Carbides, 2011(2): 47-49. |
| MLA | [1] XIE Bo, et al., "Theoretical Analysis of Initial Activation of Lithium-Lead Alloy." Rare Metals and Cemented Carbides, no. 2, 2011, pp. 47-49. |
| APA | [1] XIE Bo, GU Mei, & XIAO Cheng-jian. (2011). Theoretical Analysis of Initial Activation of Lithium-Lead Alloy. Rare Metals and Cemented Carbides(2), 47-49. |
| IEEE | [1] XIE Bo, GU Mei, and XIAO Cheng-jian, "Theoretical Analysis of Initial Activation of Lithium-Lead Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 47-49, 2011. keywords: {Li-Pb alloy;activation analysis;irradiation dose rate;neutron} |