Nanoporous Fluorescent Microresonators for Non-wired Sensing of Volatile Organic Compounds down to the ppb Level AITranslate

University of Tsukuba; University of Tsukuba; University of Tsukuba; University of Tsukuba
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Luminescent resonators have been exploited as promising non-wired sensors for volatile organic compounds (VOCs). Nonetheless, their sensitivity is insufficient to detect dilute VOCs down to ppb concentration ranges due to the little physisorption quantity on the surface. Here, we report a nanoporous fluorescent resonator that exhibits an enhanced optical response to VOC molecules by accumulative physisorption in the pores and, thus, detects VOCs with concentration down to ppb ranges. A polymer with intrinsic microporosity is allowed to assemble into spherical microparticles (MSPIM-1) that exhibit whispering gallery-mode resonance. The resonance peak undergoes a spectral shift upon exposure to a model gaseous compound (pyridine) with an excellent sensitivity (0.40 nm ppm–1) and limit-of-detection (470 ppb) without losing its linearity down to 800 ppb. Adsorption of pyridine in the pores and the underlying molecular mechanism can be quantitatively evaluated based on the change in the refractive index. MSPIM-1 preferentially detects aromatic hydrocarbons and pyridine while is less responsive to highly polar or non-polar chemicals.

KeyWords AITranslate

optical resonator volatile organic compounds nanoporous ppb nonwired
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01500

Chinese Library Classification Number:

Citation Information:

Luminescent resonators have been exploited as promising non-wired sensors for volatile organic compounds (VOCs). Nonetheless, their sensitivity is insufficient to detect dilute VOCs down to ppb concentration ranges due to the little physisorption quantity on the surface. Here, we report a nanoporous fluorescent resonator that exhibits an enhanced optical response to VOC molecules by accumulative physisorption in the pores and, thus, detects VOCs with concentration down to ppb ranges. A polymer with intrinsic microporosity is allowed to assemble into spherical microparticles (MSPIM-1) that exhibit whispering gallery-mode resonance. The resonance peak undergoes a spectral shift upon exposure to a model gaseous compound (pyridine) with an excellent sensitivity (0.40 nm ppm–1) and limit-of-detection (470 ppb) without losing its linearity down to 800 ppb. Adsorption of pyridine in the pores and the underlying molecular mechanism can be quantitatively evaluated based on the change in the refractive index. MSPIM-1 preferentially detects aromatic hydrocarbons and pyridine while is less responsive to highly polar or non-polar chemicals.

quote

GB/T 7714-2015 [1] Noriharu Tanji, Hiroshi Yamagishi, Keitaro Fujita, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01500.
MLA [1] Noriharu Tanji, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01500.
APA [1] Noriharu Tanji, Hiroshi Yamagishi, Keitaro Fujita, & Yohei Yamamoto. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01500
IEEE [1] Noriharu Tanji, Hiroshi Yamagishi, Keitaro Fujita, and Yohei Yamamoto, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01500. keywords: {optical resonator;volatile organic compounds;nanoporous;ppb;nonwired}