Greening Biobased Polybenzoxazine Network: Three Benefits in One Go AITranslate

Shiv Nadar Institute of Eminence; Shiv Nadar Institute of Eminence; Shiv Nadar Institute of Eminence; Shiv Nadar Institute of Eminence
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Eco-friendly initiators and environmentally safe flame-retardant (FR) adhesives are highly desired to empower sustainability in polymers. However, incorporating all of the properties simultaneously in a single step is challenging to achieve high-performance biomass sourced polymers. Herein, biobased benzoxazine monomers sourced from agro-waste phenol (cardanol, C) were synthesized using a facile solventless catalyst-free approach. Owing to their requirement of high ROP temperature (∼ 250 °C), prolonged polymerization cycle, issues of high flammability, and poor adhesive strength of the resultant polybenzoxazines limit their applications. To alleviate these issues, blends of naturally occurring phytic acid (PA) with the monomers resulted in fast polymerization kinetics (∼90% monomer conversion in 1 h) with the formation of hybrid polybenzoxazine networks at a mild temperature (∼100 °C). PA enacted as a green initiator and reactive halogen-free biobased FR and revealed favorable interactions across the polymer framework. Benefitting from the design, physical, ionic, and covalent cross-linking network of polymers with PA accounted for the extra-strong adhesive strength (71.1 kg/cm2, nearly 3.7 times higher than that of the pristine polybenzoxazine). Upon burning, the hybrid polybenzoxazines exhibited extremely low flammability, superior smoke suppression and formed intumescent char as supported by the limiting oxygen index, vertical burning, and cone calorimetry measurements. The present study indicated that the benign by design approach is a way forward to green thermosets offering excellent combination properties and potential applications in the future.

KeyWords AITranslate

phytic acid halogenfree flame retardant cardanol adhesion ecofriendly
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00154

Chinese Library Classification Number:

Citation Information:

Eco-friendly initiators and environmentally safe flame-retardant (FR) adhesives are highly desired to empower sustainability in polymers. However, incorporating all of the properties simultaneously in a single step is challenging to achieve high-performance biomass sourced polymers. Herein, biobased benzoxazine monomers sourced from agro-waste phenol (cardanol, C) were synthesized using a facile solventless catalyst-free approach. Owing to their requirement of high ROP temperature (∼ 250 °C), prolonged polymerization cycle, issues of high flammability, and poor adhesive strength of the resultant polybenzoxazines limit their applications. To alleviate these issues, blends of naturally occurring phytic acid (PA) with the monomers resulted in fast polymerization kinetics (∼90% monomer conversion in 1 h) with the formation of hybrid polybenzoxazine networks at a mild temperature (∼100 °C). PA enacted as a green initiator and reactive halogen-free biobased FR and revealed favorable interactions across the polymer framework. Benefitting from the design, physical, ionic, and covalent cross-linking network of polymers with PA accounted for the extra-strong adhesive strength (71.1 kg/cm2, nearly 3.7 times higher than that of the pristine polybenzoxazine). Upon burning, the hybrid polybenzoxazines exhibited extremely low flammability, superior smoke suppression and formed intumescent char as supported by the limiting oxygen index, vertical burning, and cone calorimetry measurements. The present study indicated that the benign by design approach is a way forward to green thermosets offering excellent combination properties and potential applications in the future.

quote

GB/T 7714-2015 [1] Vaishaly Duhan, Nagarjuna Amarnath, Shivani Yadav, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00154.
MLA [1] Vaishaly Duhan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00154.
APA [1] Vaishaly Duhan, Nagarjuna Amarnath, Shivani Yadav, & Bimlesh Lochab. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00154
IEEE [1] Vaishaly Duhan, Nagarjuna Amarnath, Shivani Yadav, and Bimlesh Lochab, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00154. keywords: {phytic acid;halogenfree flame retardant;cardanol;adhesion;ecofriendly}