daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research on Separation of Lithium and Titanium from Waste Lithium Titanate Materials by Dilute Sulfuric Acid Preferential Leaching AITranslate

College of Metallurgical and Chemical Engineering,Jiangxi University of Science and Technology;College of Metallurgical and Chemical Engineering,Jiangxi University of Science and Technology;College of Metallurgical and Chemical Engineering,Jiangxi University of Science and Technology;College of Metallurgical and Chemical Engineering,Jiangxi University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using waste lithium titanate from anode materials of Li-ion batteries as the raw material and after pretreatment,Li and Ti in waste materials were separated and recovered by dilute sulfuric acid preferential leaching process. The effects were investigated of sulfuric acid concentration, liquid-solid ratio, leaching temperature and leaching time on the leaching rate of lithium and titanium in the acid leaching process. The experimental results show that the optimized dilute sulfuric acid preferential leaching process parameters are as follows: sulfuric acid concentration is 4 mol/L,liquid-solid ratio is 6:1 , leaching temperature is 80℃ and leaching time is 4 h. Under these conditions, the primary leaching rate of lithium can reach 90%,and that of titanium is 1.08%.

KeyWords AITranslate

lithium titanate waste dilute sulfuric acid leaching titanium lithium separation and recovery

1张永龙,胡学步,徐云兰,丁明亮.不同形貌结构Li_4Ti_5O_(12)负极材料的最新进展[J].化学学报,2013,71(10):1341-1353. 被引量:9

2钛酸锂电池技术在国内外的发展状况[J].功能材料信息,2017,0(4):60-64. 被引量:2

3张丽芬,陈白珍,石西昌,马立文,陈亚.偏钛酸型锂吸附剂的合成及吸附性能[J].中国有色金属学报,2010,20(9):1849-1854. 被引量:20

4宋昊,梁斌,吕莉,吴潘,李春.硫酸溶液中钛水解物晶型的控制[J].过程工程学报,2010,10(1):91-96. 被引量:4

1刘雯雯,文小强,郭春平,周有池,陈燕飞,张帆,肖颖奕.钛酸锂废料回收制备电池级碳酸锂的工艺研究[J].矿冶工程,2020,40(4):95-98. 被引量:1

2李林林,王昱杰,门一飞,杨伟,邹汉波,陈胜洲.湿法冶金回收技术中无机酸作为浸出剂的研究进展[J].储能科学与技术,2021,10(1):68-76. 被引量:1

3匡晨,王乾坤,陈杭,王俊娥,钟萍丽,吴星琳.铜电解液中砷净化及资源化利用新工艺研究[J].中国有色冶金,2023,52(4):34-43.

1周雄,廖敏会,陈安国,刘富亮.负极复合材料Li_(4)Ti_(5)O_(12)-Li_(3)VO_(4)/C的制备及性能[J].电池,2021,51(3):243-246.

2李崇,马娜妮,王子钰,张彩红,王慧萍.锂离子电池预锂化专利预警分析[J].电池工业,2023,27(3):142-147.

1张亚庆,史松,王凤,王克良,连明磊.萃取精馏分离甲醇-乙腈混合物的工艺模拟[J].山东化工,2019,48(2):153-154. 被引量:2

2李旺,刘佳丽.钛酸锂材料的制备及电极配方研究[J].钢铁钒钛,2019,40(2):50-54. 被引量:1

3张英杰,许斌,梁风,段建国,孟奇,郝涛,董鹏.废旧磷酸铁锂电池正极材料的回收研究现状[J].人工晶体学报,2019,48(5):800-808. 被引量:18

4张梦龙,何几文,田欢,魏昊,赵卓.废旧锂离子电池中有价金属的回收研究进展[J].化学工业与工程,2019,36(4):23-30. 被引量:10

5高学武,李茂林,曹艳,陈立君,黄仁庆,方刚.基于遥感的合肥市不透水层覆盖度研究[J].商丘师范学院学报,2018,34(9):52-55. 被引量:1

6张利辉,徐宇兴,刘振法,魏爱佳,李文.钛酸锂/石墨烯复合负极材料的制备及电化学性能[J].化工进展,2019,38(2):949-955. 被引量:4

7陈垒,陈振宇,赵龙涛.复合碳源包覆钛酸锂材料及实装18650电池的性能[J].电源技术,2019,43(5):758-761. 被引量:1

8王瑜东,杨凯,张明杰,李建玲,高飞,刘皓,耿萌萌.静电纺丝法制备空心钛酸锂材料[J].工程科学学报,2019,41(1):111-116. 被引量:3

9庄晓东,李荣兴,俞小花,谢刚,和晓才,徐庆鑫.固相法制备钛酸锂电极材料[J].材料导报,2019,33(16):2654-2659. 被引量:4

10华骏,颜文斌,高峰,蔡俊.过硫酸钠氧化浸出石煤中的钒及其动力学研究[J].稀有金属与硬质合金,2019,47(1):1-5. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF09[冶金工程—冶金物理化学]

Citation Information:

Using waste lithium titanate from anode materials of Li-ion batteries as the raw material and after pretreatment,Li and Ti in waste materials were separated and recovered by dilute sulfuric acid preferential leaching process. The effects were investigated of sulfuric acid concentration, liquid-solid ratio, leaching temperature and leaching time on the leaching rate of lithium and titanium in the acid leaching process. The experimental results show that the optimized dilute sulfuric acid preferential leaching process parameters are as follows: sulfuric acid concentration is 4 mol/L,liquid-solid ratio is 6:1 , leaching temperature is 80℃ and leaching time is 4 h. Under these conditions, the primary leaching rate of lithium can reach 90%,and that of titanium is 1.08%.

quote

GB/T 7714-2015 [1] DENG Hao-zhen, ZHANG Fan, WEN Xiao-qiang, et al. Research on Separation of Lithium and Titanium from Waste Lithium Titanate Materials by Dilute Sulfuric Acid Preferential Leaching[J]. Rare Metals and Cemented Carbides, 2019(3): 17-20.
MLA [1] DENG Hao-zhen, et al., "Research on Separation of Lithium and Titanium from Waste Lithium Titanate Materials by Dilute Sulfuric Acid Preferential Leaching." Rare Metals and Cemented Carbides, no. 3, 2019, pp. 17-20.
APA [1] DENG Hao-zhen, ZHANG Fan, WEN Xiao-qiang, & WANG Lin-sheng. (2019). Research on Separation of Lithium and Titanium from Waste Lithium Titanate Materials by Dilute Sulfuric Acid Preferential Leaching. Rare Metals and Cemented Carbides(3), 17-20.
IEEE [1] DENG Hao-zhen, ZHANG Fan, WEN Xiao-qiang, and WANG Lin-sheng, "Research on Separation of Lithium and Titanium from Waste Lithium Titanate Materials by Dilute Sulfuric Acid Preferential Leaching," Rare Metals and Cemented Carbides, no. 3, pp. 17-20, 2019. keywords: {lithium titanate waste;dilute sulfuric acid leaching;titanium;lithium;separation and recovery}