The Latest Development of Perovskite-type Composite Metal Oxide AITranslate
Abstract AITranslate
The paper has summarized the preparation technologies for perovskite-type composite metal oxide,including citric acid method,chemical precipitation,sol-gel,hydrothermal synthesis,pyrolysis,solid state reaction.According to a series of characteristics of the oxide resulted from its cubic structure and oxygen vacancies,its application in the fields of gas-sensitive material,fuel cell,catalytic material,oxygen-permeable membrane are also described.
KeyWords AITranslate
1金万勤,徐南平.混合导体透氧膜材料的设计与应用[J].化工进展,2006,25(10):1143-1151. 被引量:4
2李红花,汪浩,严辉.ABO_3钙钛矿型复合氧化物光催化剂设计评述[J].化工进展,2006,25(11):1309-1313. 被引量:25
3娄向东,赵晓华,成庆堂,卢雁.ABO_3钙钛矿复合氧化物研究进展[J].传感器技术,2002,21(7):5-8. 被引量:17
4Ge L,Zhou W,Ran R,et al.Properties and performance of A-site deficient(Ba0.5 Sr0.5)1-x Co0.8 Fe0.2 O3-δ for oxygen permeating membrane[J].J Membr Sci,2007,306:318-328.
5刘石明,邢长生,钱晓良,肖建中.柠檬酸法和聚乙烯醇法制备La0.8Sr0.2Co0.5Fe0.5O3纳米材料工艺过程及微观形貌比较[J].材料科学与工程学报,2008,26(2):169-172. 被引量:6
6牛新书,陈晓丽,茹祥莉,李自强,魏平涛,王雪丽.柠檬酸络合法制备La_(1-x)Pb_xFeO_3及其光催化性能[J].中国稀土学报,2008,26(6):780-783. 被引量:4
7李嵩,文钟晟,季世军,孙俊才.阴极材料Ba_(0.5)Sr_(0.5)Co_(0.8)Fe_(0.2)O_(3-σ)合成工艺优化[J].材料科学与工艺,2008,16(3):322-325. 被引量:2
8云月厚,刘本康,张常在,张伟.化学共沉淀法制备的Ba_(0.5)Sr_(0.5)Co_(0.8)Fe_(0.2-x)CexO_3微波吸收特性研究[J].稀土,2008,29(4):53-58. 被引量:13
9孟波,谭小耀,孟秀霞.共沉淀和低温燃烧法制备Sr_(0.9)Ce_(0.9)Y_(0.1)O_(3-δ)陶瓷粉及性能[J].硅酸盐通报,2007,26(6):1129-1135. 被引量:3
10亓淑艳,郭丽琴,冯静,石兆辉,张密林,宁兆娟.钙钛矿型复合氧化物La_(1-x)Sr_xMnO_3和(La_(0.7)Sr_(0.3))_(1-y)K_yMnO_3的结构及磁性研究[J].稀土,2008,29(1):23-27. 被引量:4
1阮乐,张哲,李凝.钙钛矿型氧化物La_(1-x)Pr_xNiO_3的合成及表征[J].材料导报:纳米与新材料专辑,2014,28(2):296-298. 被引量:1
2詹海鹃,刘万毅.钙钛矿材料的结构、性能及催化研究进展[J].硅酸盐通报,2017,36(4):1198-1202. 被引量:4
3苗强,夏鑫,杨微,李芳,李其明.SDC-BCCF双相透氧膜材料的合成及透氧性能研究[J].膜科学与技术,2018,38(4):75-80. 被引量:3
1王吟,杜保保,张晓东,杨一琼.环境化学综合设计实验:钙钛矿的制备、表征及其微波诱导降解有机废水性能研究[J].化学教育(中英文),2019,40(2):63-67. 被引量:3
2刘伟,慕铭,陈颖颖,马雪莹,党鸿博,赵国升.低维度纳/微结构单斜BiVO_4聚集体光催化剂的研究进展[J].硅酸盐通报,2018,37(9):2845-2851. 被引量:4
3谭孟苹,王三军,饶凤飞.压强对有机-无机杂化钙钛矿(MAPbBr 3)电子结构调制的第一性原理研究[J].人工晶体学报,2018,47(8):1589-1595.
4杨萍,李凝,马浩,彭瀚.钙钛矿复合氧化物在催化领域中的应用进展[J].广东石油化工学院学报,2019,29(1):33-37. 被引量:1
5刘力魁,刘威,李佳,杨微,李芳,李其明.K0.1Sr0.9Co0.8Fe0.2O3-δ透氧膜材料的合成及透氧性能研究[J].膜科学与技术,2020,40(2):45-52.
6唐彬,詹海鹃,吴丹,吴之强,王刚,毕淑娴,刘万毅.Ni掺杂型钙钛矿复合炭材料的制备及其催化性能[J].硅酸盐通报,2020,39(10):3359-3366.
7解品红,李芳,裴瑜洁,夏媛玉,王雨生,李其明.SDC-SSF双相透氧膜的表面优化及其氧渗透性能[J].膜科学与技术,2022,42(3):84-90.
8裴瑜洁,解品红,王雨生,夏媛玉,李芳,李其明.基于萤石相粒子掺杂制备高稳定SrCo_(0.8)Fe_(0.2)O_(3-δ)基质透氧膜材料[J].膜科学与技术,2022,42(6):87-93.
1杨淑梅,邓淑华,黄慧民,余双平.二氧化锆负载催化剂的应用[J].工业催化,2003,11(10):39-43. 被引量:10
2王宝和,范方荣,张文博,崔丹丹,景殿策.煅烧工艺对纳米氧化镁粉体活性的影响[J].无机盐工业,2005,37(12):15-16. 被引量:7
3钱伯章.石墨烯强韧化碳纤维复合材料关键技术获突破[J].合成纤维,2017,46(3):55-55. 被引量:1
4韩巧凤,阚春,李丹,杨绪杰.SnO_2纳米晶的制备及性能研究[J].上海化工,2002,27(18):18-19. 被引量:6
5尹万云,裴立宅,黄向红,张千峰.煅烧温度对多组分SrFe_(0.5)CoO_(3-δ)氧化物结构的影响(英文)[J].安徽工业大学学报:自然科学版,2010,27(3):274-276.
6何涛.柠檬酸纳法制液体二氧化硫[J].内蒙古石油化工,2007,33(3):23-25. 被引量:6
7王溥修.对搪瓷柠檬酸法耐酸测定的几点看法[J].华东搪瓷,1990(3):13-14.
8新型.宁波材料所在石墨烯强韧化碳纤维复合材料关键技术方面取得重要进展[J].化工新型材料,2017,45(2):260-260.
9张伟党,钱海燕,孔庆刚.菱镁矿制备活性氧化镁研究[J].非金属矿,2007,30(5):9-11. 被引量:11
10大漠.我国石墨烯强韧化碳纤维复合材料关键技术获突破[J].航空制造技术,2017,0(1):14-14.
Basic Information:
DOI:
Chinese Library Classification Number:TQ132.3[化学工程—无机化工]
Citation Information:
The paper has summarized the preparation technologies for perovskite-type composite metal oxide,including citric acid method,chemical precipitation,sol-gel,hydrothermal synthesis,pyrolysis,solid state reaction.According to a series of characteristics of the oxide resulted from its cubic structure and oxygen vacancies,its application in the fields of gas-sensitive material,fuel cell,catalytic material,oxygen-permeable membrane are also described.
quote
| GB/T 7714-2015 | [1] ZHANG Bi-yu, WANG Peng, XIA Zheng-wei, et al. The Latest Development of Perovskite-type Composite Metal Oxide[J]. Rare Metals and Cemented Carbides, 2010(4): 63-68. |
| MLA | [1] ZHANG Bi-yu, et al., "The Latest Development of Perovskite-type Composite Metal Oxide." Rare Metals and Cemented Carbides, no. 4, 2010, pp. 63-68. |
| APA | [1] ZHANG Bi-yu, WANG Peng, XIA Zheng-wei, GU Hui-ju, BAO Wei-wei, & HUANG Xiang-hong. (2010). The Latest Development of Perovskite-type Composite Metal Oxide. Rare Metals and Cemented Carbides(4), 63-68. |
| IEEE | [1] ZHANG Bi-yu, WANG Peng, XIA Zheng-wei, GU Hui-ju, BAO Wei-wei, and HUANG Xiang-hong, "The Latest Development of Perovskite-type Composite Metal Oxide," Rare Metals and Cemented Carbides, no. 4, pp. 63-68, 2010. keywords: {perovskite-type composite metal oxides;preparation technology;gas-sensitive material;fuel cell;catalytic material;oxygen-permeable membrane} |