Quality Problems and Improvement Measures of Electrolytic Nickel in Electroplating Industry AITranslate
Abstract AITranslate
In view of some problems including delamination, slag inclusion, electric melting unevenness with residue and fragment when electrolytic nickel is used in electroplating, the quality of electroplating products is affected. The causes are analyzed. Such factors in the electrolytic nickel production process as rising elec- trolyte pH, fierce current intensity movement, unclean surface of electrolytic nickel starting sheet, impure electrolyte and so on, are the main causes of electrolytic nickel quality defects. The corresponding improve ment measures and the proposal for accelerating the development of active electrolytic nickel are put for ward.
KeyWords AITranslate
1McDonald R G,Whittington B I. Atmospheric acid leac hing of nickel laterites review: part I sulphuric acid tech nologies[J]. Hydrometallurgy, 2008,91 : 33-55.
2Kaya S,Topkaya Y A. High pressure acid leaching of a refractory lateritic nickel ore[J]. Minerals Engineering, 2011,24..1 188-1 197.
3Bidault F,Brett D J L,Middleton P H,et al. Review of gas diffusion cathodes for alkaline fuel cells[J]. Journal of Power Sources, 2009,187 : 39-48.
4Duerr M,Gair S,Cruden A,et al. Dynamic electrochem ical model of an alkaline fuel cell stack[J]. Journal of Power Sources,2007,171:1 023-1 032.
5Hejze T,Besenhard J O, Kordesch K, et al. Current sta tus of combined systems using alkaline fuel cells and ammonia as a hydrogen carrier [J]. Journal of Power Sources, 2008,176 : 490-493.
6Uma Rani R, Sharma A K, Minu C, et al. Studies on black electroless nickel coatings on titanium alloys for spacecraft thermal control applications [J]. Journal of Applied Electrochemistry, 2010,40 ( 2 ) : 333-338.
7Ripenbein T, Golodnitsky D, Nathan M, et al. Electroless nickel current collector for 3D-microbatteries[J]. Journal of Applied Electrochemistry,2010,40(2):435-441.
8Amirjan M,Zangeneh-Madar K, Parvin N. Preparation of tungsten base composite powder by electroless nickel plating[J]. Powder Metallurgy,2010,53(3) :218-225.
1张贝贝,王春霞,吴光辉,胡小萍,林茜.热轧温度对电解厚镍性能影响的研究[J].电镀与精饰,2017,39(2):9-13.
2徐仰涛,刘鲁滨,代玉杰.镍离子浓度对电沉积镍组织结构的影响[J].金属热处理,2017,42(7):18-22. 被引量:2
3张仲利.含硫活性电解镍板的研究[J].山东冶金,2019,41(2):37-39.
4张虎,张四增,孔晓华.新技术支撑金川电镀专用镍产业化发展[J].中国金属通报,2020(11):10-11.
5徐仰涛,刘志健,朱珍旭,王雅宁.铜离子对工业电解液中镍电结晶行为的影响[J].中国有色金属学报,2021,31(4):984-994. 被引量:2
6卢苏君,王超,徐仰涛,朱纪念,宗红星,苏玉娟.电解镍与电积镍的结构和性能对比[J].中国有色金属学报,2022,32(8):2380-2392.
7李孟星,孟祥海,柳亚斌,张宏博,李欣,李运刚.NiO在NaCl-KCl-NaF熔盐体系中的溶解度及溶解机理[J].有色金属工程,2019,9(3):57-61.
1张青芳,曾明,陈超,王翠琼,蒋银燕.电化学石英晶体微天平研究电沉积镍[J].精细化工中间体,2017,47(5):67-70.
2苏晓冰,吴蒙华,贾卫平,于昇元,贾婷婷.基于无掩模定域性电沉积的3D打印平面微结构工艺研究[J].现代制造工程,2022(5):18-23.
3夏日辉,王春霞,田礼熙.杂质铜离子对电镀镍层组织形貌及耐蚀性的影响[J].表面技术,2022,51(10):276-283.
4王美涵,周博阳,高源,侯朝霞,张钧.电化学沉积Ni_(x)O_(y)薄膜及电致变色性能研究进展[J].沈阳大学学报:自然科学版,2023,35(3):185-191.
1廖寄乔,邬建平,巴多佳.我国钨粉质量现状[J].硬质合金,1998,15(4):246-248. 被引量:2
2刘越表,郭金梅.提高重轨质量的途径[J].包钢科技,2003,29(4):30-32. 被引量:2
3郭晓丽.提高硫酸铜质量的生产实践[J].有色矿冶,1999,15(6):23-27.
4陈增琪,曹广畴.国外薄板坯连铸技术的发展及加速开发我国薄板坯连铸技术的建议[J].钢铁厂设计,1989(1):13-24.
5李献军.真空自耗电弧炉熔炼技术和铸锭质量问题[J].钛工业进展,2001,18(3):16-22. 被引量:31
6辛根富,郜斌.调整产品结构 加速开发废钢加工设备[J].废钢铁,1990(3):62-63.
7李京军,夏文勇,付军.LF炉精炼优质碳素结构钢的生产实践[J].江西冶金,2005,25(6):13-15.
8K.Briem,张育钦.一种节能的铝碎屑干燥法[J].轻金属,1989(3):55-57.
9肖印杰.联合法生产海绵钛存在的质量问题及措施[J].有色矿冶,1998,14(3):26-29. 被引量:5
10叶匡吾.关于我国球团矿质量问题的探讨[J].烧结球团,2005,30(5):1-4. 被引量:29
Basic Information:
DOI:
Chinese Library Classification Number:TF815[冶金工程—有色金属冶金]
Citation Information:
In view of some problems including delamination, slag inclusion, electric melting unevenness with residue and fragment when electrolytic nickel is used in electroplating, the quality of electroplating products is affected. The causes are analyzed. Such factors in the electrolytic nickel production process as rising elec- trolyte pH, fierce current intensity movement, unclean surface of electrolytic nickel starting sheet, impure electrolyte and so on, are the main causes of electrolytic nickel quality defects. The corresponding improve ment measures and the proposal for accelerating the development of active electrolytic nickel are put for ward.
quote
| GB/T 7714-2015 | [1] HOU Xiao-chuan, PENG Jun. Quality Problems and Improvement Measures of Electrolytic Nickel in Electroplating Industry[J]. Rare Metals and Cemented Carbides, 2012(5): 70-72. |
| MLA | [1] HOU Xiao-chuan, and PENG Jun. "Quality Problems and Improvement Measures of Electrolytic Nickel in Electroplating Industry." Rare Metals and Cemented Carbides, no. 5, 2012, pp. 70-72. |
| APA | [1] HOU Xiao-chuan, & PENG Jun. (2012). Quality Problems and Improvement Measures of Electrolytic Nickel in Electroplating Industry. Rare Metals and Cemented Carbides(5), 70-72. |
| IEEE | [1] HOU Xiao-chuan and PENG Jun, "Quality Problems and Improvement Measures of Electrolytic Nickel in Electroplating Industry," Rare Metals and Cemented Carbides, no. 5, pp. 70-72, 2012. keywords: {electrolytic nickel;electroplating;quality problem;improvement measure;active electrolytic nickel} |