Research Progress on the Gradient Cemented Carbides with Cubic-Phase Free Surface Layer and their Cutting Application AITranslate
Abstract AITranslate
The research results on the gradient cemented carbides with cubic-phase free surface layer are summarized.The effects of chemical composition, particle size of raw materials and sintering atmosphere on the microstructure, elemental distribution and properties of the gradient cemented carbides with cubic-phase free surface layer are systematically introduced.The application of the gradient cemented carbides as coating substrate and the cutting application of the coated gradient cemented carbide tools are summarized.It is pointed that the research on the surface treatment technology of the gradient cemented carbides with cubic-phase free surface layer is an important direction to tap their application potential.
KeyWords AITranslate
1Tian-En Yang,Lan Sun,Ji Xiong,Zhi-Xing Guo,Lei Wang,Ding Cao.Adherent coating on gradient cemented carbide with ultrafine Ti(C_(0.5),N_(0.5))[J].稀有金属:英文版,2015,0(6):413-420. 被引量:4
2杨天恩,SUN Lan,熊计,GUO Zhixing,ZHENG Xiaoming.Microstructure and Properties of Gradient Cemented Carbide with Nano-TiN[J].武汉理工大学学报:材料科学英文版,2014(1):102-108. 被引量:2
1王禹哲,李民辉,徐国忠,葛媛媛,王帅栋,白金锋.中间相沥青基泡沫炭孔胞结构调控[J].炭素技术,2022,41(6):30-35.
2吴兴刚,王峰.钼粉—轧制钼杆生产过程中的质量控制[J].中国钼业,2022,46(6):59-61.
3王淼,卫俊涛,宋旭东,徐德良,张红,张书.石油焦煅烧脱硫研究进展[J].炭素技术,2022,41(5):23-28. 被引量:1
4张金池,刘贵清,解雪,张帆,王芳,刘昱辰,吴祖璇.转炉钢渣弱酸体系高效浸出工艺研究[J].中国资源综合利用,2023,41(1):11-14.
5李重典,黄龙,龚佳琳,唐启佳.烧结气氛对Ti(C,N)-8%Mo_(2)C-8%NbC-4%Co-12%Ni金属陶瓷微观组织与性能的影响[J].硬质合金,2022,39(6):475-481.
6刘畅,赵香香,刘晓飞,杨春瑜,张娜.富硒锌重组米挤压工艺优化及糊化特性研究[J].粮食与油脂,2023,36(1):52-57.
7任岩,段盼盼,冷科,盖欣,喻冲.大晶粒UO_(2)芯块制备的研究现状[J].科技视界,2022(26):34-37.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The research results on the gradient cemented carbides with cubic-phase free surface layer are summarized.The effects of chemical composition, particle size of raw materials and sintering atmosphere on the microstructure, elemental distribution and properties of the gradient cemented carbides with cubic-phase free surface layer are systematically introduced.The application of the gradient cemented carbides as coating substrate and the cutting application of the coated gradient cemented carbide tools are summarized.It is pointed that the research on the surface treatment technology of the gradient cemented carbides with cubic-phase free surface layer is an important direction to tap their application potential.
quote
| GB/T 7714-2015 | [1] YANG Tian-en, DENG Cheng-jun, SHI Xian-ke, et al. Research Progress on the Gradient Cemented Carbides with Cubic-Phase Free Surface Layer and their Cutting Application[J]. Rare Metals and Cemented Carbides, 2022(6): 90-98. |
| MLA | [1] YANG Tian-en, et al., "Research Progress on the Gradient Cemented Carbides with Cubic-Phase Free Surface Layer and their Cutting Application." Rare Metals and Cemented Carbides, no. 6, 2022, pp. 90-98. |
| APA | [1] YANG Tian-en, DENG Cheng-jun, SHI Xian-ke, XIONG Ji, & DENG Zheng-hua. (2022). Research Progress on the Gradient Cemented Carbides with Cubic-Phase Free Surface Layer and their Cutting Application. Rare Metals and Cemented Carbides(6), 90-98. |
| IEEE | [1] YANG Tian-en, DENG Cheng-jun, SHI Xian-ke, XIONG Ji, and DENG Zheng-hua, "Research Progress on the Gradient Cemented Carbides with Cubic-Phase Free Surface Layer and their Cutting Application," Rare Metals and Cemented Carbides, no. 6, pp. 90-98, 2022. keywords: {gradient cemented carbide;cubic-phase free surface layer;particle size of raw materials;coating substrate;cutting} |