Development of a Rubber Recycling Process Based on a Single-Component Interfacial Adhesive AITranslate

Massachusetts Institute of Technology; Massachusetts Institute of Technology; Massachusetts Institute of Technology; Massachusetts Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A simple and cost-effective adhesive-based rubber recycling process was designed as an alternative to devulcanization. Interfacial bonding between vulcanized and virgin rubbers is improved by incorporating adhesives and coating processes during rubber reblending and reducing interfacial defects that cause premature failure. In flat laminates, the bond strength between vulcanized and virgin materials doubles when a vulcanizing fluid and thin adhesive layer are introduced. These components are combined into single-component adhesives (SCAs), which improve bond strength sixfold over no treatment, using half the raw material as the multilayer adhesive. When SCAs are coated onto vulcanized rubber particles prior to reblending, the best rubbers exhibit nearly 50% increases in mechanical strength and toughness vs the untreated control and statistically identical extensibility; all treatments improved mechanical strength. This simple, inexpensive, and scalable process can be implemented with one step beyond standard reblending and curing, providing a promising alternative to devulcanization for polymer recycling.

KeyWords AITranslate

recycling rubber devulcanization isoprene rubber composite ground rubber
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01343

Chinese Library Classification Number:

Citation Information:

A simple and cost-effective adhesive-based rubber recycling process was designed as an alternative to devulcanization. Interfacial bonding between vulcanized and virgin rubbers is improved by incorporating adhesives and coating processes during rubber reblending and reducing interfacial defects that cause premature failure. In flat laminates, the bond strength between vulcanized and virgin materials doubles when a vulcanizing fluid and thin adhesive layer are introduced. These components are combined into single-component adhesives (SCAs), which improve bond strength sixfold over no treatment, using half the raw material as the multilayer adhesive. When SCAs are coated onto vulcanized rubber particles prior to reblending, the best rubbers exhibit nearly 50% increases in mechanical strength and toughness vs the untreated control and statistically identical extensibility; all treatments improved mechanical strength. This simple, inexpensive, and scalable process can be implemented with one step beyond standard reblending and curing, providing a promising alternative to devulcanization for polymer recycling.

quote

GB/T 7714-2015 [1] Michelle A. Calabrese, Wui Yarn Chan, Sarah H. M. AvRon, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01343.
MLA [1] Michelle A. Calabrese, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01343.
APA [1] Michelle A. Calabrese, Wui Yarn Chan, Sarah H. M. AvRon, & Bradley D. Olsen. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01343
IEEE [1] Michelle A. Calabrese, Wui Yarn Chan, Sarah H. M. AvRon, and Bradley D. Olsen, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01343. keywords: {recycling;rubber;devulcanization;isoprene rubber;composite;ground rubber}