The Latest Development of the Treatment Technology for Ni-Mo Ores AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The mineral composition characterization of Ni-Mo ores is analyzed, the latest development of the treatment technology for Ni-Mo ores is reviewed, and the advantages and disadvantages are compared between hydrometallurgical process and pyrometallurgical process for Ni-Mo ores. It is pointed out that the hydrometallurgical process is superior in treating Ni-Mo ores over pyrometallurgical process. Some problems present in the existing metallurgical processes of Ni-Mo ores are also pointed out. Furthermore,the development trend of the treatment technology for Ni-Mo ores is prospected.

KeyWords AITranslate

Ni-Mo ore beneficiation process hydrometallurgy pyrometallurgy the latest development

1范德廉,杨秀珍,王连芳,陈南生.某地下寒武统含镍钼多元素黑色岩系的岩石学及地球化学特点[J].地球化学,1973(3):143-164. 被引量:109

2皮关华,徐徽,陈白珍,石西昌,李俊丽.从难选镍钼矿中回收钼的研究[J].湖南有色金属,2007,23(1):9-12. 被引量:42

3李青刚,肖连生,张贵清,张启修.镍钼矿生产钼酸铵全湿法生产工艺及实践[J].稀有金属,2007,31(S1):85-89. 被引量:52

4潘家永,马东升,夏菲,陈少华,曹双林,郭国林,谢贵珍.湘西北下寒武统镍-钼多金属富集层镍与钼的赋存状态[J].矿物学报,2005,25(3):283-288. 被引量:45

5梁有彬,朱文凤.湘西北天门山地区镍钼矿床铂族元素富集特征及成因探讨[J].地质找矿论丛,1995,10(1):55-65. 被引量:28

6曾明果.遵义黄家湾镍钼矿地质特征及开发前景[J].贵州地质,1998,15(4):305-310. 被引量:52

1赵中伟,黄少波,霍广生,张刚,曹才放.复杂镍浸出液萃取净化的研究[J].有色金属:冶炼部分,2010(1):5-8. 被引量:6

2关文娟,肖连生,张贵清,李青刚,龚柏藩.利用低品位镍钼矿生产高纯多钼酸铵技术的工业应用[J].中国钼业,2010,34(1):42-45.

3聂琪.试论我国钼矿选矿方法及研究现状[J].云南冶金,2010,39(2):34-36. 被引量:28

4张文朴.加强钼资源综合利用与再生研发 促进我国生态钼业建设[J].中国钼业,2010,34(2):13-18. 被引量:3

5沈明伟.钼镍矿提钼强化浸出试验研究[J].矿产综合利用,2010(3):12-15. 被引量:8

6杨晓霞.镍矿的湿法冶金研究现状与发展前景[J].世界有色金属,2010(7):44-45. 被引量:6

7张舞剑,李姣.镍钼矿冶炼废水的处理[J].湖南有色金属,2010,26(5):42-45. 被引量:7

8肖朝龙,肖连生,龚柏藩,郭超.镍钼矿全湿法浸出工艺研究[J].稀有金属与硬质合金,2010,38(4):1-5. 被引量:17

9刘美.矿样中镍的二次强化浸出及X-射线衍射分析[J].科学技术与工程,2011,11(6):1166-1170.

10刘美.硫化钼镍矿加碱焙烧后钼镍的回收率分析[J].化学与粘合,2011,33(2):75-78. 被引量:1

1周平,周强.2010年云南选矿年评[J].云南冶金,2011,40(2):20-32.

2肖朝龙,肖连生,龚柏凡.采用N235从镍钼矿盐酸浸出液中萃取钼的研究[J].中国钼业,2011,35(2):7-11. 被引量:7

3李琳,吕宪俊,栗鹏.钼矿选矿工艺发展现状[J].中国矿业,2012,21(2):99-103. 被引量:52

4马琼.铜镍硫化矿冶金过程的铜镍分离与精炼方法探究[J].甘肃冶金,2012,34(2):40-43. 被引量:3

5周艳飞,崔立凤.江西某钼矿选矿试验研究[J].有色金属:选矿部分,2012(3):39-43. 被引量:4

6宋永胜,曹亦俊,马子龙.柱机联合浮选工艺在铜钼矿分选中的应用[J].中国钼业,2012,36(2):30-34. 被引量:3

7何静,王涛,黄玲,罗超,王小能.铅电解废液除锌工艺研究[J].有色金属:冶炼部分,2012(7):12-15. 被引量:3

8张邦胜,蒋开喜,王海北.全湿法处理钼镍矿的新工艺[J].四川有色金属,2012(3):26-28. 被引量:2

9张宏雷,朱国才,闫红,张明珠,张伟灵,赵玉娜.从生物质还原的氧化锰矿中回收钴镍的试验研究[J].稀有金属,2012,36(5):811-816. 被引量:4

10邓攀,曾颜亮,王坤,刘德刚.钼资源的回收技术现状及发展[J].山西冶金,2012,35(5):1-3. 被引量:5

1赵景富.镍红土矿火法冶金工艺现状及展望[J].中国有色冶金,2017,46(1):26-29. 被引量:3

2张志华,毛拥军.红土镍矿处理工艺研究现状[J].湖南有色金属,2012,28(4):31-35. 被引量:19

3侯慧芬.从废铅酸蓄电池中回收有价金属[J].上海有色金属,2001,22(4):181-186. 被引量:18

4胡慧英,赵庆雷,张志华,张志雄.镍钼矿处理工艺研究现状[J].金属材料与冶金工程,2013,41(3):42-46. 被引量:2

5潘志胜,王谦,何生平,李玉刚.连铸保护渣组分对粘度的影响[J].四川冶金,2010,32(5):17-21. 被引量:3

6皮关华,孔凡祥,贾露萍,王长江,杜建新.瑞木红土镍矿高压酸浸的生产实践[J].中国有色冶金,2015,0(6):11-14. 被引量:7

7Keith R.Suttill,柴成栋.硫化矿精矿湿法与火法冶金工艺的发展与比较[J].湿法冶金,1991(2):52-56.

8胡杰,王玉昌.工业计算机网络及在转炉中的应用[J].设备管理与维修,2004(11):22-23.

9王君天.杭钢100吨VD炉真空脱气工艺的开发与完善[J].浙江冶金,2015(3):30-34.

10简启发.从废旧稀土钴永磁材料中回收钴的研究[J].江西有色金属,1999,13(3):34-36. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]

Citation Information:

The mineral composition characterization of Ni-Mo ores is analyzed, the latest development of the treatment technology for Ni-Mo ores is reviewed, and the advantages and disadvantages are compared between hydrometallurgical process and pyrometallurgical process for Ni-Mo ores. It is pointed out that the hydrometallurgical process is superior in treating Ni-Mo ores over pyrometallurgical process. Some problems present in the existing metallurgical processes of Ni-Mo ores are also pointed out. Furthermore,the development trend of the treatment technology for Ni-Mo ores is prospected.

quote

GB/T 7714-2015 [1] ZHANG Gang, ZHAO Zhong-wei, HUO Guang-sheng, et al. The Latest Development of the Treatment Technology for Ni-Mo Ores[J]. Rare Metals and Cemented Carbides, 2008(4): 37-41.
MLA [1] ZHANG Gang, et al., "The Latest Development of the Treatment Technology for Ni-Mo Ores." Rare Metals and Cemented Carbides, no. 4, 2008, pp. 37-41.
APA [1] ZHANG Gang, ZHAO Zhong-wei, HUO Guang-sheng, CAO Cai-fang, LI Jiang-tao, CHEN Ai-liang, & LI Hong-gui. (2008). The Latest Development of the Treatment Technology for Ni-Mo Ores. Rare Metals and Cemented Carbides(4), 37-41.
IEEE [1] ZHANG Gang, ZHAO Zhong-wei, HUO Guang-sheng, CAO Cai-fang, LI Jiang-tao, CHEN Ai-liang, and LI Hong-gui, "The Latest Development of the Treatment Technology for Ni-Mo Ores," Rare Metals and Cemented Carbides, no. 4, pp. 37-41, 2008. keywords: {Ni-Mo ore;beneficiation process;hydrometallurgy;pyrometallurgy;the latest development}