Experimental Study on Preparation of Jarosite from Titanium White Waste Water AITranslate
Abstract AITranslate
Jarosite was prepared from titanium white waste water by adding potassium chlorate and potassi- um hydroxide. The effects of reaction temperature,solution pH and reaction time on Fe precipitation rate were investigated. And microstructure and phase composition of the precipitated product were also ana- lyzed. The results show that the precipitation rate of Fe from titanium white waste water is more than 99% under the conditions of temperature of 95 ℃, solution pH of 2.0 and reaction time of 40 min. The precipita- ted product is the acicular crystal of jarosite. In addition to the significant decrease of SO4^2-and Fe2+ concentrations in the filtrate,the contents of the rare metal ions such as Ti,V and Sc are almost unchanged, which is beneficial for the separation and purification of rare metals in the next process step.
KeyWords AITranslate
1王建伟,任秀莲,魏琦峰,杨东,吴成龙.钛白废酸的综合利用研究现状及展望[J].无机盐工业,2009,41(9):4-7. 被引量:26
2张贵清,张启修,周康根,马荣骏.N1923萃取回收钛白水解废酸中的钛——萃取参数的研究[J].矿冶工程,2002,22(3):86-88. 被引量:16
3钟文卓,魏蜀刚,张运德,胡戈,张华.硫酸法钛白粉废酸浓缩及其析出废硫酸亚铁制硫酸[J].硫磷设计与粉体工程,2011(1):6-11. 被引量:9
4熊素玉.硫酸法生产钛白粉的主要环境问题及对策[J].化工设计通讯,2005,31(2):44-46. 被引量:21
5李潜,张启修.萃取法回收钛白水解废酸中硫酸的实验研究[J].稀有金属与硬质合金,2003,31(1):4-7. 被引量:10
6黄珊,李正山.钛白废液的治理、回收及综合利用研究[J].资源开发与市场,2007,23(9):778-781. 被引量:4
7杨涛,王志坚,肖劲,刘吉波,余荣旻,邓志军.赤泥和钛白废液中提钪的浸出工艺研究[J].矿冶,2015,24(5):37-40. 被引量:11
8丁杰,何锡阳,刘晓燕.利用盐酸法钛白废液制备铁黄颜料研究[J].化学研究与应用,2008,20(7):932-934. 被引量:2
9丁杰.盐酸法生产钛白废液制取高纯Fe_2O_3实验研究[J].化工生产与技术,2007,14(4):39-40. 被引量:2
10徐铜文.乳状液膜法提取硫酸法钛白废液中微量钪的研究[J].稀有金属,1994,18(4):245-248. 被引量:8
1陶荣荣,牛泽鹏,朱晓波,李望,张治国.利用钛白废液制备草酸亚铁实验研究[J].稀有金属与硬质合金,2022,50(1):6-9.
1徐勇勇,孙琨,邹增琪,方亮,邢建东.选区激光熔化制备Al_(0.5)CoCrFeNi高熵合金的工艺参数及组织性能[J].西安交通大学学报,2018,52(1):151-157. 被引量:14
2龙眼叶面喷施氯酸钾近季产期调控技术[J].广东农村实用技术,2018,0(1):20-20.
3杨时钧.水火“相生、相依、相克”的设计[J].化学教学,1984,0(4):50-50.
4邓楚燕,罗瑞盈.自愈合基体改性SiC/SiC复合材料的制备与性能研究[J].中国陶瓷工业,2017,24(6):1-4. 被引量:1
5于贺华.含氟废液制备氟钛酸钾工艺研究[J].无机盐工业,2018,50(3):46-48. 被引量:2
6刘卫,何捍卫,尹志芳,杨泱,陈月华.邻碘苯甲酸铵循环去除粗氧化钪中的锆和铪[J].化工进展,2018,37(6):2386-2391.
7巨佳,闫晨,印邵胜,许永祥,杨柳,陈爱华.超声波辅助液相还原铜氨废液制备纳米铜粉[J].中国材料进展,2018,37(3):210-214. 被引量:2
8刘露露,王若兰,吴远,唐开梁.小麦淀粉加工废液制备葡萄糖浆的糖化工艺优化[J].食品工业科技,2018,39(9):131-135. 被引量:2
9杜安睿,姜涛,李骞,徐斌,杨永斌.废铝基/钯催化剂碱性浸出废液制备拟薄水铝石的研究[J].矿产保护与利用,2018,38(1):112-116. 被引量:6
10张金祥,欧阳希,周健,张济山.Cr含量降低对H13钢组织与力学性能的影响[J].材料导报,2018,32(8):1323-1327. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:X788[环境科学与工程—环境工程]
Citation Information:
Jarosite was prepared from titanium white waste water by adding potassium chlorate and potassi- um hydroxide. The effects of reaction temperature,solution pH and reaction time on Fe precipitation rate were investigated. And microstructure and phase composition of the precipitated product were also ana- lyzed. The results show that the precipitation rate of Fe from titanium white waste water is more than 99% under the conditions of temperature of 95 ℃, solution pH of 2.0 and reaction time of 40 min. The precipita- ted product is the acicular crystal of jarosite. In addition to the significant decrease of SO4^2-and Fe2+ concentrations in the filtrate,the contents of the rare metal ions such as Ti,V and Sc are almost unchanged, which is beneficial for the separation and purification of rare metals in the next process step.
quote
| GB/T 7714-2015 | [1] LI Wang℃, ZHAO Heng℃, ZHU Xiao-bo℃. Experimental Study on Preparation of Jarosite from Titanium White Waste Water[J]. Rare Metals and Cemented Carbides, 2018(3): 35-37. |
| MLA | [1] LI Wang℃, et al., "Experimental Study on Preparation of Jarosite from Titanium White Waste Water." Rare Metals and Cemented Carbides, no. 3, 2018, pp. 35-37. |
| APA | [1] LI Wang℃, ZHAO Heng℃, & ZHU Xiao-bo℃. (2018). Experimental Study on Preparation of Jarosite from Titanium White Waste Water. Rare Metals and Cemented Carbides(3), 35-37. |
| IEEE | [1] LI Wang℃, ZHAO Heng℃, and ZHU Xiao-bo℃, "Experimental Study on Preparation of Jarosite from Titanium White Waste Water," Rare Metals and Cemented Carbides, no. 3, pp. 35-37, 2018. keywords: {jarosite;titanium white waste water;potassium chlorate;potassium hydroxide;Fe precipitationrate} |