Preparation Method and Application of Ti-based Dimensionally Stable Anode AITranslate
Abstract AITranslate
Description is made of the preparation method, applications and future development of Ti - based dimensionally stable anode (DSA)-one kind of new anode.Among all kinds of metal - based DSAa,Ti - based one has widely found its applications in industry because of its long service life, high electro - catalysis properties without secondary pollution. Its application in related industrial operations resulted in less energy consumption, lower cost, less pollution and effective control of industrial waste water, as accords with the requirement of clean production and can bring about tremendous economic and social benefits.
KeyWords AITranslate
1张招贤,王新民.氯化物体系电积钴中活性涂层钛阳极的研制[J].广东有色金属学报,1992,2(2):108-112. 被引量:3
2邹忠,李劼,丁凤其,张文根.梯度功能型金属氧化物涂层阳极(DSA)的制备[J].功能材料,2001,32(4):431-433. 被引量:20
3宋卫锋,吴斌,李义久,倪亚明.形稳阳极电解处理有机废水的机理研究[J].重庆环境科学,2000,22(6):60-63. 被引量:13
4宋卫锋,谢光炎,林美强.DSA类电极催化降解硝基苯及其动力学研究[J].上海环境科学,2002,21(6):353-355. 被引量:20
5宋卫锋,马前,李义久,倪亚明.不同DSA类阳极催化降解苯胺的试验研究[J].环境保护科学,2001,27(2):4-6. 被引量:8
6张招贤.钛电极工学[M].北京:冶金工业出版社,2003..
7冯绍彬,冯丽婷,商士波.三价铬体系电镀铬-镍合金工艺[J].材料保护,2004,37(5):24-25. 被引量:23
8不溶性金属电极DSE[J].钛工业进展,2003(1):39-42. 被引量:1
9尤宏,崔玉虹,冯玉杰,刘峻峰,蔡伟民.钛基Co中间层SnO_2电催化电极的制备及性能研究[J].材料科学与工艺,2004,12(3):230-233. 被引量:27
10Foti G,et al.Characterization of DSA type electrodes prepared by rapid thermal decomposition of the metal precursor[J].Electrochimica Acta,1998,44:813.
1徐浩,张倩,邵丹,延卫.钛基体锑掺杂二氧化锡电极的制备与改性研究进展[J].化工进展,2013,32(S1):145-151. 被引量:7
2延卫,徐浩,汤成莉.水系统的积垢及其物理控制技术[J].净水技术,2008,27(3):9-13. 被引量:15
3王丽艳,王宝辉,吴红军,陈微,刘威,李佳.阳极涂层的研究进展[J].化学工业与工程,2009,26(2):176-182. 被引量:18
4徐浩,延卫,汤成莉.电子水处理技术[J].工业水处理,2009,29(8):5-9. 被引量:16
5张翼,周新新,张玉洁.金属氧化物涂层钛阳极的研究[J].化学进展,2009,21(9):1827-1831. 被引量:12
6贺国旭,张秋霞,杨维春.电浮选方法在废水处理中的应用[J].净水技术,2010,29(5):36-41. 被引量:3
7李晓良,徐浩,延卫,邵丹.钛基SnO_2电极的制备、改性及其应用研究进展[J].电镀与精饰,2016,38(5):16-22. 被引量:5
8赵学天.浅析冶金中二氧化锰阳极研究[J].世界有色金属,2018,43(14):193-193.
9路雨禾,王伟,路殿坤,谢锋.电解沉积用尺寸稳定型钛阳极的研究现状[J].有色金属:冶炼部分,2020(11):18-24. 被引量:2
1徐浩,张倩,邵丹,延卫.钛基体锑掺杂二氧化锡电极的制备与改性研究进展[J].化工进展,2013,32(S1):145-151. 被引量:7
2徐浩,延卫,汤成莉.水垢的电化学去除工艺与机理研究[J].西安交通大学学报,2009,43(5):104-108. 被引量:37
3徐浩,延卫,汤成莉.电子水处理技术[J].工业水处理,2009,29(8):5-9. 被引量:16
4马晓伟,周宁玉,谢朝新,黄俊龙,孙国周,杜建民.高压静电场在反渗透预处理中的试验研究[J].后勤工程学院学报,2010,26(3):62-66.
5卢强,安立超,钟秦,胡悦,夏文文,王志良.Ru0.7Si0.3O2/Ti电极电催化氧化处理硝基苯废水[J].应用化学,2011,28(5):576-582. 被引量:13
6张淳恺,邵艳群,唐电.Ru-Zr-Y氧化物涂层电极的制备及其性能[J].金属热处理,2011,36(5):34-37. 被引量:2
7徐浩,延卫,游莉.不同酸处理对钛基体性能的影响[J].稀有金属材料与工程,2011,40(9):1550-1554. 被引量:15
8罗艳归,隋贤栋,黄肖容.水垢防治技术研究进展[J].工业水处理,2012,32(1):18-20. 被引量:18
9程化,刘军梅,王海林.IrO_2-Ta_2O_5/Ti阳极的研究进展[J].材料保护,2012,45(10):48-52. 被引量:1
10吴方敏,王庆法,王莅.有机添加剂对Ru_(0.5)Ir_(0.5)O_2/Ti电极性能的影响[J].化学工业与工程,2012,29(6):7-10. 被引量:1
1谢素玲.高性能多用途的DSA阳极[J].电镀与涂饰,2004,23(3):30-32. 被引量:7
2朱舸,程志旗,高波.中频电炉应急水系统的改进[J].锻造与冲压,2015,0(19):63-64.
3吴铁丁.小型无缝钢管生产中的延伸工序及其设备[J].山西机械,1999(1):45-46.
4李维毅.焊接烟尘的产生与治理[J].现代焊接,2014(4):55-58.
5图书推荐[J].表面工程资讯,2012,12(2):83-83.
6田志茗.废水中痕量镍的测定[J].哈尔滨师范大学自然科学学报,2005,21(2):74-76. 被引量:3
7《钢丝磷化生产技术资料汇编》[J].金属制品,2016,42(1):29-29.
8C.S.Devaragudi,K.HussainReddy,许菱,许孙曲.分光光度法测定合金钢和工业废水中的铬[J].科教译丛,2000(3):2-6.
9严丽,王强.氧化着色工业废水循环使用的可行性研究[J].黑龙江冶金,2005,25(4):3-5.
10潘继超,周有华,李自立,吴铁成.数控轴承座球面孔镗床的结构设计[J].轴承,2016(7):21-25. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]
Citation Information:
Description is made of the preparation method, applications and future development of Ti - based dimensionally stable anode (DSA)-one kind of new anode.Among all kinds of metal - based DSAa,Ti - based one has widely found its applications in industry because of its long service life, high electro - catalysis properties without secondary pollution. Its application in related industrial operations resulted in less energy consumption, lower cost, less pollution and effective control of industrial waste water, as accords with the requirement of clean production and can bring about tremendous economic and social benefits.
quote
| GB/T 7714-2015 | [1] GONG Zhu-qing, OU Yang-quan-sheng, ZHU Yong-hong, et al. Preparation Method and Application of Ti-based Dimensionally Stable Anode[J]. Rare Metals and Cemented Carbides, 2005(3): 46-50. |
| MLA | [1] GONG Zhu-qing, et al., "Preparation Method and Application of Ti-based Dimensionally Stable Anode." Rare Metals and Cemented Carbides, no. 3, 2005, pp. 46-50. |
| APA | [1] GONG Zhu-qing, OU Yang-quan-sheng, ZHU Yong-hong, & CHENG Dai-song. (2005). Preparation Method and Application of Ti-based Dimensionally Stable Anode. Rare Metals and Cemented Carbides(3), 46-50. |
| IEEE | [1] GONG Zhu-qing, OU Yang-quan-sheng, ZHU Yong-hong, and CHENG Dai-song, "Preparation Method and Application of Ti-based Dimensionally Stable Anode," Rare Metals and Cemented Carbides, no. 3, pp. 46-50, 2005. keywords: {Ti - based anode;DSA;preparation method;coating;application} |