daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Experimental Study on Molybdenum Reduction from Ammonium Paratungstate by Washing AITranslate

Luoyang Luanchuan Molybdenum Group Tungsten Co.,Ltd.;Luoyang Luanchuan Molybdenum Group Tungsten Co.,Ltd.;Luoyang Luanchuan Molybdenum Group Tungsten Co.,Ltd.;Luoyang Luanchuan Molybdenum Group Tungsten Co.,Ltd.;Luoyang Luanchuan Molybdenum Group Tungsten Co.,Ltd.;Luoyang Luanchuan Molybdenum Group Tungsten Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The preparation of high purity ammonium paratungstate not only has important economic value,but also has great strategic significance.Reasonable control of molybdenum content in ammonium paratungstate and guarantee of product pass rate are the key to affect the development and economic benefits of enterprises.The effects of washing water pH value,washing temperature,washing time,liquid-solid ratio and washing frequency on the elution rates of molybdenum and tungsten were studied by single factor tests.The results show that the optimal conditions for molybdenum reduction from ammonium paratungstate by washing with pure water are washing water pH value of 7.0,reaction time of 20 min,reaction temperature of 65℃,liquid-solid ratio of 3∶1 and washing frequency of once.At this time,the elution rate of molybdenum reaches 82.01%,and the loss of tungsten is small with an elution rate of 3.97%.This method has the advantages of no other impurities,simple operation,environmentally friendly process and low production cost,and has certain reference value and significance for enterprise development and process improvement of ammonium paratungstate preparation.

KeyWords AITranslate

ammonium paratungstate washing with pure water elution rate molybdenum tungsten
No data

Basic Information:

DOI:

Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]

Citation Information:

The preparation of high purity ammonium paratungstate not only has important economic value,but also has great strategic significance.Reasonable control of molybdenum content in ammonium paratungstate and guarantee of product pass rate are the key to affect the development and economic benefits of enterprises.The effects of washing water pH value,washing temperature,washing time,liquid-solid ratio and washing frequency on the elution rates of molybdenum and tungsten were studied by single factor tests.The results show that the optimal conditions for molybdenum reduction from ammonium paratungstate by washing with pure water are washing water pH value of 7.0,reaction time of 20 min,reaction temperature of 65℃,liquid-solid ratio of 3∶1 and washing frequency of once.At this time,the elution rate of molybdenum reaches 82.01%,and the loss of tungsten is small with an elution rate of 3.97%.This method has the advantages of no other impurities,simple operation,environmentally friendly process and low production cost,and has certain reference value and significance for enterprise development and process improvement of ammonium paratungstate preparation.

quote

GB/T 7714-2015 [1] WANG Jun-jie, WANG Xin-xin, WANG Lu-lu, et al. Experimental Study on Molybdenum Reduction from Ammonium Paratungstate by Washing[J]. Rare Metals and Cemented Carbides, 2024(6): 1-5.
MLA [1] WANG Jun-jie, et al., "Experimental Study on Molybdenum Reduction from Ammonium Paratungstate by Washing." Rare Metals and Cemented Carbides, no. 6, 2024, pp. 1-5.
APA [1] WANG Jun-jie, WANG Xin-xin, WANG Lu-lu, CHEN Li-ge, LIU De-zhi, & LUO Kai. (2024). Experimental Study on Molybdenum Reduction from Ammonium Paratungstate by Washing. Rare Metals and Cemented Carbides(6), 1-5.
IEEE [1] WANG Jun-jie, WANG Xin-xin, WANG Lu-lu, CHEN Li-ge, LIU De-zhi, and LUO Kai, "Experimental Study on Molybdenum Reduction from Ammonium Paratungstate by Washing," Rare Metals and Cemented Carbides, no. 6, pp. 1-5, 2024. keywords: {ammonium paratungstate;washing with pure water;elution rate;molybdenum;tungsten}