Instabilities as the Origin of Large-Area Self-Assembled and Aligned Organic Semiconductor Nanocrystals Instabilities as the Origin of Large-Area Self-Assembled and Aligned Organic Semiconductor Nanocrystals AITranslate
Abstract AITranslate
Aligned nanocrystals of organic semiconductors (OSCs) are highly desirable for electronic devices and biomedical and photonic applications. Solution-based wet processing routes have the potential to produce aligned nanocrystals over large areas in small time frames. Herein, we demonstrate that by optimizing the hydrodynamic evaporative processes, controlled long-range crystalline assemblies of OSCs can be achieved (longest nanocrystal ∼3 mm) purely through physical processes: namely, from fingering instabilities. Self-assembly is achieved here without strong noncovalent interactions such as hydrogen-bonding interactions. Experimentally our approach involves just placing a drop of a solution on an inclined substrate. Nanocrystals with widths of 300–800 nm and lengths of millimeters (length/width aspect ratios >105) are formed in less than 2–8 s. A hydrazine chemiresistive sensor based on the aligned crystalline patterns show unprecedented responsivity (∼10–6), 2 orders greater than those of stick–slip patterns. Finally, experimental parameters that need optimization to achieve nanocrystal patterns are investigated in detail and pointers to fabricate such OSC nanocrystals are provided.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00061
Chinese Library Classification Number:
Citation Information:
Aligned nanocrystals of organic semiconductors (OSCs) are highly desirable for electronic devices and biomedical and photonic applications. Solution-based wet processing routes have the potential to produce aligned nanocrystals over large areas in small time frames. Herein, we demonstrate that by optimizing the hydrodynamic evaporative processes, controlled long-range crystalline assemblies of OSCs can be achieved (longest nanocrystal ∼3 mm) purely through physical processes: namely, from fingering instabilities. Self-assembly is achieved here without strong noncovalent interactions such as hydrogen-bonding interactions. Experimentally our approach involves just placing a drop of a solution on an inclined substrate. Nanocrystals with widths of 300–800 nm and lengths of millimeters (length/width aspect ratios >105) are formed in less than 2–8 s. A hydrazine chemiresistive sensor based on the aligned crystalline patterns show unprecedented responsivity (∼10–6), 2 orders greater than those of stick–slip patterns. Finally, experimental parameters that need optimization to achieve nanocrystal patterns are investigated in detail and pointers to fabricate such OSC nanocrystals are provided.
quote
| GB/T 7714-2015 | [1] Vijay Venugopalan, Bhanprakash Jain, Rajashree Y. Mahale, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00061. |
| MLA | [1] Vijay Venugopalan, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00061. |
| APA | [1] Vijay Venugopalan, Bhanprakash Jain, Rajashree Y. Mahale, Kumar Subramani, & Kothandam Krishnamoorthy. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00061 |
| IEEE | [1] Vijay Venugopalan, Bhanprakash Jain, Rajashree Y. Mahale, Kumar Subramani, and Kothandam Krishnamoorthy, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00061. keywords: {fingering instability aligned fibers nanocrystal arrays organic semiconductors diketopyrrolopyrrole naphthalenediimide} |