daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Formulation Optimization for Compound Inhibitors of WC Oxidation Dissolution by Response Surface Methodology AITranslate

School of Chemistry Engineering, Hebei United University;School of Chemistry Engineering, Hebei United University;School of Chemistry Engineering, Hebei United University;School of Chemistry Engineering, Hebei United University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on the principle of universal central composite rotatable design (CCD),the formulation of compound inhibitors was optimized and the related experiment was designed, by response surface analysis. Effects of compound inhibitors on oxidation dissolution of WC powder were investigated in hydrothermal environment,and compound inhibitors are composed of sodium citrate, borax, nitro-benzoic acid triethano- lamine ester (simplified as aromatic amine ester). The electromotive force changes of different inhibitor so- lution were determined before and after adding WC powder. Response surface and contour line were drawn with AE as the response indicator. The interaction between various factors and leaching degree of WC in different solution were analyzed. The results show that with max response value i. e. minimum WC oxida- tion dissolution,the compound inhibitor formula is as follows:sodium citrate 0. 983 5 g/100 mLH20,borax 2. 507 4 g/100 mLH20,aromatic amine ester with 1 : 1.1 molar ratio 2. 510 3 g/100 mLH20. And the pre- dictive value of the regression model is 0. 059 07 V and the actual measured value is 0. 058 36 V.

KeyWords AITranslate

WC oxidation dissolution compound inhibitor response surface analysis CCD design

1Mason R L,Gunst R F, Hess J J. Statistical design and analysis of experiments with apphcafions to engineeringand science [ M]. Hoboken: John Wiley and Sons lnc, 2003. 116-124.

2Adinarayana K,Ellaiah P, Srinivasulu B, et al. Response surface methodological approach to optimize the nutri- tional parameters for neomycin production by strepto myces marinensis under solid- state fermentation [J].Process Biochemistry,2003,38(11) :1 565-1 572.

3王俊,李安平,黄卫文,刘建军.响应面法优化活性乳酸菌饮料乳化稳定剂配方[J].中国酿造,2009,28(3):121-123. 被引量:16

4Bacaoui A,Dahbi A, Yaacoubi A,et al. Experimental de sign to optimize preparation of activated carbons for use in water treatment[J]. Environmental Science and Tech- nology,2002,3G(17) :3 844-3 849.

5Noordin M Y, Venkatesh V C,Sharf S,et al. Applica tion of response surface methodology in describing the performance of coated carbide tools when turning AISI 1045 steel[J]. Journal of Materials Processing and Tech- nology, 2004,145 (1) : 46-58.

6任露泉.试验设计及其优化(第二版)[M].北京:高等教育出版社,2003.265-278.

7张润楚,刘民千,杨建峰,等.回归分析与实验设计[M].北京:机械工业出版社,2010.171-176.

8汪仁官.实验设计与分析[M].北京:中国统计出版社,1998..

9傅剑锋,武秋立.统计学实验设计分析颗粒状TiO_2光催化AB7染料废水[J].太阳能学报,2008,29(2):152-157. 被引量:5

1胡莉蓉,乐晓兵,陈杰山,陈东旭.响应面分析法优化从钛白废酸中提取钪元素的工艺参数[J].石油化工,2014,43(12):1422-1426. 被引量:1

2轩勤生.硼硅复合抑制剂对焦炭热态性能的实验研究[J].中州煤炭,2014(10):114-116.

3刘书祯.超细晶硬质合金晶粒长大抑制剂的研究[J].稀有金属与硬质合金,2007,35(4):51-56. 被引量:21

4陈金钟,刘江宁,李冰,王瑾,于建国.氧化镁在镁电解质中的溶解度[J].有色金属:冶炼部分,2006(5):20-24. 被引量:2

5金生龙,王雨红,粟海锋,程晨,雷作敏.响应面法优化葡萄糖还原浸出半氧化锰矿的研究[J].广西大学学报:自然科学版,2014,39(6):1403-1408. 被引量:5

6彭博,夏余平,曹叶飞,吴庆定.响应面法优化稀土烧结钢的成分与性能[J].时代农机,2015,42(9):42-44.

7许彩云,娄军峰,程亮.中间包挡墙的设计与优化[J].耐火与石灰,2015,40(6):9-12.

8杨彦松.响应面法优化硝酸浸铅锌矿尾渣回收银工艺研究[J].应用化工,2011,40(8):1401-1404. 被引量:2

9林信平,曹顺华,李炯义.一种新型晶粒长大抑制剂对纳米硬质合金烧结行为的影响[J].稀有金属与硬质合金,2004,32(4):4-9. 被引量:3

10程晨,粟海锋,王雨红,金生龙,雷作敏.混生锰矿的直接酸浸法及其影响因素分析[J].有色金属:冶炼部分,2014(6):9-12. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF111.31[冶金工程—冶金物理化学]

Citation Information:

Based on the principle of universal central composite rotatable design (CCD),the formulation of compound inhibitors was optimized and the related experiment was designed, by response surface analysis. Effects of compound inhibitors on oxidation dissolution of WC powder were investigated in hydrothermal environment,and compound inhibitors are composed of sodium citrate, borax, nitro-benzoic acid triethano- lamine ester (simplified as aromatic amine ester). The electromotive force changes of different inhibitor so- lution were determined before and after adding WC powder. Response surface and contour line were drawn with AE as the response indicator. The interaction between various factors and leaching degree of WC in different solution were analyzed. The results show that with max response value i. e. minimum WC oxida- tion dissolution,the compound inhibitor formula is as follows:sodium citrate 0. 983 5 g/100 mLH20,borax 2. 507 4 g/100 mLH20,aromatic amine ester with 1 : 1.1 molar ratio 2. 510 3 g/100 mLH20. And the pre- dictive value of the regression model is 0. 059 07 V and the actual measured value is 0. 058 36 V.

quote

GB/T 7714-2015 [1] CHEN Xiao-xin, ZHANG Xiu-ling, JIA Xiao-ming, et al. Formulation Optimization for Compound Inhibitors of WC Oxidation Dissolution by Response Surface Methodology[J]. Rare Metals and Cemented Carbides, 2012(5): 57-62.
MLA [1] CHEN Xiao-xin, et al., "Formulation Optimization for Compound Inhibitors of WC Oxidation Dissolution by Response Surface Methodology." Rare Metals and Cemented Carbides, no. 5, 2012, pp. 57-62.
APA [1] CHEN Xiao-xin, ZHANG Xiu-ling, JIA Xiao-ming, & SONG Yue-xing. (2012). Formulation Optimization for Compound Inhibitors of WC Oxidation Dissolution by Response Surface Methodology. Rare Metals and Cemented Carbides(5), 57-62.
IEEE [1] CHEN Xiao-xin, ZHANG Xiu-ling, JIA Xiao-ming, and SONG Yue-xing, "Formulation Optimization for Compound Inhibitors of WC Oxidation Dissolution by Response Surface Methodology," Rare Metals and Cemented Carbides, no. 5, pp. 57-62, 2012. keywords: {WC;oxidation dissolution;compound inhibitor;response surface analysis;CCD design}