daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Micro/Mesoporous Carbon Nanospheres with Homogeneously N, S, P-Tridoped Skeletons as Electrodes for High-Performance Supercapacitors Micro/Mesoporous Carbon Nanospheres with Homogeneously N, S, P-Tridoped Skeletons as Electrodes for High-Performance Supercapacitors AITranslate

Donghua University; Donghua University; Donghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hierarchical porous heteroatom-doped carbon materials are one of the most promising materials for supercapacitor (SC) electrodes due to their outstanding inherent characteristics. In this study, a micro/mesoporous N, P, S-tridoped carbon material (NPSC-900) is prepared using poly(cyclotriphosphazene-co-4,4′-sulfonyldiphenol) as the only precursor through a one-step synthesis strategy combining direct carbonization and in situ heteroatom doping. The obtained NPSC-900 as a SC electrode exhibits outstanding electrochemical performances, such as a high capacitance of 392 F g–1 at 2 mV s–1, superior rate capacity, and good long-term stability after 10,000 cycles with 98.5% capacitance retention. Moreover, a flexible asymmetric SC is assembled by coupling the NSPC-900/carbon cloth (CC) and NiO/CC electrodes. Its maximum energy and power densities reach 119.5 Wh kg–1 and 23.4 kW kg–1, respectively. The remarkable electrochemical properties of NSPC-900 are benefited from the adequate surface area, ultralarge pore volume, hierarchical micro/mesoporous structure, and heteroatom-doped skeleton, which provide a significant way for designing high-performance electrodes for energy storage systems.

KeyWords AITranslate

heteroatom carbon pore structure supercapacitor electrode
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01056

Chinese Library Classification Number:

Citation Information:

Hierarchical porous heteroatom-doped carbon materials are one of the most promising materials for supercapacitor (SC) electrodes due to their outstanding inherent characteristics. In this study, a micro/mesoporous N, P, S-tridoped carbon material (NPSC-900) is prepared using poly(cyclotriphosphazene-co-4,4′-sulfonyldiphenol) as the only precursor through a one-step synthesis strategy combining direct carbonization and in situ heteroatom doping. The obtained NPSC-900 as a SC electrode exhibits outstanding electrochemical performances, such as a high capacitance of 392 F g–1 at 2 mV s–1, superior rate capacity, and good long-term stability after 10,000 cycles with 98.5% capacitance retention. Moreover, a flexible asymmetric SC is assembled by coupling the NSPC-900/carbon cloth (CC) and NiO/CC electrodes. Its maximum energy and power densities reach 119.5 Wh kg–1 and 23.4 kW kg–1, respectively. The remarkable electrochemical properties of NSPC-900 are benefited from the adequate surface area, ultralarge pore volume, hierarchical micro/mesoporous structure, and heteroatom-doped skeleton, which provide a significant way for designing high-performance electrodes for energy storage systems.

quote

GB/T 7714-2015 [1] LuoJia Feng, JiaYi Yan, ShaoWei Bian. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01056.
MLA [1] LuoJia Feng, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01056.
APA [1] LuoJia Feng, JiaYi Yan, & ShaoWei Bian. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01056
IEEE [1] LuoJia Feng, JiaYi Yan, and ShaoWei Bian, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01056. keywords: {heteroatom carbon pore structure supercapacitor electrode}