Anisotropy of Wetting AITranslate
Abstract AITranslate
Wetting of single-crystal surfaces of metallic solids and oxides by liquid metals and alloys is anisotropic because of the anisotropy of the energies of solid surfaces and of their interfaces with liquids. To provide a basis for a discussion of wetting anisotropy, we review first the literature on surface and interfacial energies in metal-metal and metal-ceramic systems. We then summarize the relevant literature on the anisotropy of the energies of solid surfaces and of solid-liquid interfaces. These energies are then used in conjunction with the Young equation to estimate the expected anisotropy of wetting. Some serious discrepancies are found between these estimates and the experimental anisotropy of wetting. We show that under certain experimental conditions the wetting angles that have been determined are not Young contact angles.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1146/annurev.matsci.38.060407.130210
Chinese Library Classification Number:
Citation Information:
Wetting of single-crystal surfaces of metallic solids and oxides by liquid metals and alloys is anisotropic because of the anisotropy of the energies of solid surfaces and of their interfaces with liquids. To provide a basis for a discussion of wetting anisotropy, we review first the literature on surface and interfacial energies in metal-metal and metal-ceramic systems. We then summarize the relevant literature on the anisotropy of the energies of solid surfaces and of solid-liquid interfaces. These energies are then used in conjunction with the Young equation to estimate the expected anisotropy of wetting. Some serious discrepancies are found between these estimates and the experimental anisotropy of wetting. We show that under certain experimental conditions the wetting angles that have been determined are not Young contact angles.
quote
| GB/T 7714-2015 | [1] Dominique Chatain. Annual Review of Materials Research, 2008(38). DOI:10.1146/annurev.matsci.38.060407.130210. |
| MLA | [1] Dominique Chatain. Annual Review of Materials Research, no. 38, 2008, https://doi.org/10.1146/annurev.matsci.38.060407.130210. |
| APA | [1] Dominique Chatain. (2008). Annual Review of Materials Research(38). https://doi.org/10.1146/annurev.matsci.38.060407.130210 |
| IEEE | [1] Dominique Chatain, Annual Review of Materials Research, no. 38, 2008, doi: 10.1146/annurev.matsci.38.060407.130210. keywords: {liquid metal;metallic solids;oxides;surface;solidliquid interface;equilibrium shape} |